Birdseye maple

Hardwoods > Sapindaceae > Acer > saccharum

Birdseye maple (Acer saccharum)

Common Name(s): Birdseye maple, bird’s eye maple

Botanical Designation: Not a distinct species of maple; considered a growth/grain anomaly. Although rare exceptions exist, birdseye maple is almost exclusively harvested from hard maple (Acer saccharum).

Distribution: Northeastern North America

Average Dried Weight: 44.0 lbs/ft3 (705 kg/m3)

Janka Hardness: 1,450 lbf (6,450 N)

Comments: Called birdseye maple (sometimes written out as bird’s eye) because the tiny knots in the grain resemble small bird’s eyes. The figure is reportedly caused by unfavorable growing conditions for the tree. The tree attempts to start numerous new buds to get more sunlight, but with poor growing conditions the new shoots are aborted, and afterward a number of tiny knots remain.

Birdseye maple is frequently sold in veneer form, but solid lumber is available as well. Being tiny knots, the birdseye figure is most noticeable and pronounced on flatsawn pieces of lumber. For more information on strength and working characteristics, see the full article on hard maple (Acer saccharum).

Images: Drag the slider up/down to toggle between raw and finished wood. The video linked below shows birdseye figure in maple as well as a handful of other woods to illustrate that birdseye is not always a growth form that belongs exclusively to maple. A special thanks to Ben Vaterlaus for providing the picture of the turned pen.

 

Birdseye Maple (bookmatched veneer)
Birdseye maple (bookmatched veneer)
Birdseye maple (turned pen)

Identification: Since birdseye maple is not a distinct species, the written information below is for hard maple (Acer saccharum), though the endgrain images show a sample with birdseye figure for reference. See the article on Hardwood Anatomy for definitions of endgrain features.

Birdseye maple (endgrain 10x)
Birdseye maple (endgrain 1x)
Porosity: diffuse porous Arrangement: solitary and radial multiples Vessels: small to medium; moderately numerous to numerous Parenchyma: banded (marginal) Rays: both narrow and wide; normal spacing Lookalikes/Substitutes: Sometimes confused with species of soft maple, hard maple can sometimes be differentiated on the basis of weight, where hard maple is markedly heavier than some lighter species such as silver maple (Acer saccharinum). Also, hard maple has a greater diversity of ray widths when looking at the endgrain (ranging from narrow to wide rays), while most other maples native to North America have more uniform medium-width rays. See the article on telling hard and soft maple apart for more information, including chemical testing. Notes: None.

Related Content:

Subscribe
Notify of
guest
23 Comments
Inline Feedbacks
View all comments
Mike Stafford

A box in birdseye maple

Birdseye-Maple-1.875T-X-2.75D
Robert

Has anyone ever heard of bird’s eye with curly figure within

20250710_214901
20250710_214849
sara

Is this birds eye maple? it is from a soft maple.

MJStone

Birdseye Maple is acer saccharum aka Hard Maple.

Kimberly Cox

Is this a veneer?

Steve Ondich

Because birdseye is so sought after, the logs with birdseye figure are often made into veneer. However, some logs are processed into lumber, as well. Generally speaking, the highest quality birdseye logs end up as veneers. Sometimes this presents a problem when woodworkers need lumber figure to match a veneer figure.

Rik

Is there such a thing as a law against cutting down a Birdseye maple tree?? And, what might used Birdseye maple flooring (in, say, good shape) be worth?

MJStone

As long as it’s on your property or you have permission to cut it down, there are no restrictions on logging Birdseye Maple aka Hard Maple. If you have Birdseye floorboards in good shape then you should be able price similar to lumberyard prices, or maybe even higher. The more birds eyes the better and pricier, usually. Luthiers (guitar builders) love the stuff.

Rik

Is there such a thing as a law against cutting down a Birdseye maple tree? And, what might used Birdseye maple flooring be worth (in, say, “good” shape)?

Jake

What type of maple are basketball courts made of

Monty McNeill

We’ve compleated birds eye maple paneling job less than a year ago but now all the walls exposed to sunlight are turning green. Has any one else had this happen? The panels not exposed to sunlight are fine. We are replacing the green ones. Is this a problem with finish or veneer or what?

Kate Johnson

My fiance is interested in getting his wedding band with grey birdseye maple. Does anyone know the durability of this type of wood?

Thomas L Brooks

Do any of the maple species that grow in the Pacific Northwest develop birdseyes?

suzanne

my birdseye maple is dull. it does not have a glossy finish like my birdseye armoires. can I put a furniture oil on it?

Bill Bagley

If it’s your floor you trying to shine, please don’t use oil. That will cause a contamination with any future floor finish. Your birdseye floor can be buffed & coated with a glossier sheen. A good cleaner like Bona floor care may help too.

nic payne

Would this also be birdseye maple? It looks very similar except it has dark spots throughout, which I have not noticed in Birdseye maple.

Kelley pedigo

I acquired a large slab of maple, it has sharp knobby protrusions all around the bark side, it’s punky in the middle, rotting. I think it’s a Maple Burl wood, the grain is beautiful, maybe a tiger maple ?

Bob Card

Hi Kelly – that sounds to me like it might be Big Leaf Maple. It will have more reddish color than Hard Maple or Soft Maple, and a lot of character in the grain. Big Leaf Maple grows in the Pacific Northwest, unlike the other varieties, which are more commonly found in the Eastern US and Canada. Here’s a picture of a table I made with Big Leaf Maple.

Mike

I agree birdseye maple.

Nicole Ongo

Hi, wondering if you can help me identify this wood? I’m thinking it’s birds eye maple, but I’m not 100% sure. The table is at least 65 years old. I recently inherited this table from my late grandmother, it had about 10 layers of paint/varnish on it. I used Circa1850 paint remover today and (after lots if elbow grease) this lovely grain was revealed!