Kingwood

> Hardwoods > Fabaceae > Dalbergia > cearensis
DATA SOURCE(S): 10,15,20,34,36,63
Kingwood (Dalbergia cearensis)

Average Dried Weight:AVERAGE DRIED WEIGHT
Density is the measurement of a wood’s weight per unit volume. Here, "dried weight" specifically refers to wood at 12% moisture content, and values are given in pounds per cubic foot and kilograms per cubic meter. Also keep in mind that density commonly varies by +/- 10% from the average.

Click on the link "Average Dried Weight" for more details.
65.1 lbs/ft3 (1,045 kg/m3) High WEIGHT TIERS
Extremely Low:     0+ kg/m3
Very Low:   420+ kg/m3
Low:   520+ kg/m3
Medium-Low:   620+ kg/m3
Medium:   730+ kg/m3
Medium-High:   840+ kg/m3
High:   960+ kg/m3
Very High: 1,080+ kg/m3
Extremely High: 1,200+ kg/m3
Tiers are based on CSIRO provisional strength groupings (SD1-SD8) based on density.

Janka Hardness:JANKA HARDNESS
This test measures a wood’s resistance to indentation, and is the pounds of force (or Newtons) required to embed a .444" (11.28 mm) diameter steel ball halfway into the wood. Values are for side grain, measured at 12% MC.

Click on the link "Janka Hardness" for more details.
2,660 lbf (11,850 N) High JANKA HARDNESS TIERS
Extremely Low:      0+ N
Very Low:  2,050+ N
Low:  3,150+ N
Medium-Low:  4,480+ N
Medium:  6,280+ N
Medium-High:  8,380+ N
High: 11,080+ N
Very High: 14,000+ N
Extremely High: 17,450+ N
Tiers are derived from CSIRO provisional strength classifications (SD1-SD8) in conjunction with the USDA's estimated hardness based on density.

Modulus of Rupture:MODULUS OF RUPTURE
Sometimes called bending strength, this test measures a wood’s strength before breaking (i.e., rupturing). Values are given in pounds of force per square inch and megapascals, measured at 12% MC.

Click on the link "Modulus of Rupture" for more details.
18,980 lbf/in2 (130.9 MPa) Very High MOR TIERS
Extremely Low:   0+ MPa
Very Low:  45+ MPa
Low:  55+ MPa
Medium-Low:  65+ MPa
Medium:  78+ MPa
Medium-High:  94+ MPa
High: 110+ MPa
Very High: 130+ MPa
Extremely High: 150+ MPa
Tiers are based on CSIRO strength classifications (SD1-SD8).

Crushing Strength:CRUSHING STRENGTH
Also called compression strength, this test measures the maximum stress sustained before failure. Force is applied parallel to the grain (producing stress akin to chair legs). Values are given in pounds of force per square inch and megapascals, measured at 12% MC.

Click on the link "Crushing Strength" for more details.
10,150 lbf/in2 (70.0 MPa) Very High CRUSHING STRENGTH TIERS
Extremely Low:  0+ MPa
Very Low: 30+ MPa
Low: 36+ MPa
Medium-Low: 41+ MPa
Medium: 47+ MPa
Medium-High: 54+ MPa
High: 61+ MPa
Very High: 70+ MPa
Extremely High: 80+ MPa
Tiers are based on CSIRO strength classifications (SD1-SD8).

Shrinkage:SHRINKAGE
These values represent the percentage change in radial and tangential faces of the wood—as well as the total (volumetric) shrinkage—as the moisture content goes from green (maximum) down to oven-dry (minimum), approximating the wood's stability with changes in humidity. T/R ratio helps to estimate the uniformity of the shrinkage across different wood faces.

Click on the link "Shrinkage" for more details.
Radial: 6.9%, Tangential: 9.3% Very High SHRINKAGE TIERS
Very Low:   0%+   
Low: 3.6%+   
Medium: 5.1%+   
High: 6.6%+   
Very High: 8.1%+   
Tiers are based on tangential shrinkage (green to oven-dry) from CSIRO shrinkage classifications (1-5).

                          Volumetric: 16.5%, T/R Ratio: 1.4

Color/Appearance: Heartwood is a dark purplish or reddish brown with darker black streaks. Sapwood is pale yellow and sharply demarcated from the heartwood.

Grain/Texture: Grain is usually straight or occasionally interlocked. Fine, uniform texture and a high natural luster.

Rot Resistance: Reported as being very durable in decay resistance, and is also resistant to termites.

Workability: Tends to be difficult to work due to its high density. Kingwood has a moderate blunting effect on cutters, and tearout can occur during planing if interlocked grain is present. Can be difficult to glue due to natural oils and high density. Turns very well and takes a high polish.

Odor: Distinct, rosewood-like odor when being worked.

Allergies/Toxicity: Although severe reactions are quite uncommon, kingwood has been reported as a sensitizer. Can cause eye and skin irritation, as well as pink eye. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Pricing/Availability: Likely to be very expensive, and seldom available as lumber due to the small size of the tree itself. Kingwood is most often seen as smaller turning stock, with its cost being on par with other scarce rosewoods in the Dalbergia genus

Sustainability: Kingwood is listed on CITES appendix II under the genus-wide restriction on all Dalbergia species—which also includes finished products made of the wood (though finished items under 10 kilograms are exempted). Additionally, kingwood is rated as being near threatened by the IUCN, remarking that prior to the CITES restrictions, there was ongoing harvesting of wild trees and exporting of timber, which  “potentially resulted in local extinction in Ceará.”[1]2021. Dalbergia cearensisThe IUCN Red List of Threatened Species Accessed on 04 July 2025 . (Note that Ceara is the name of the Brazilian state where kingwood is commonly harvested from and is actually the source of its Latin species name, cearensis.)

Common Uses: Inlays, veneers, tool handles, and other small turned and/or specialty items.

Comments: So named from several French kings (Louis XIV and Louis XV) in the 17th and 18th centuries that preferred the wood in the use of fine furniture. Kingwood is considered a
true rosewood in the Dalbergia genus, and if going by the original Portuguese name for rosewood, jacaranda, then kingwood was actually regarded as one of the very earliest sources of true rosewood, being sold as jacarandá-violeta (along with Brazilian rosewood, known then as jacarandá-da-Bahia).

Another closely related species found in Mexico, Dalbergia congestiflora, bears a very close resemblance to kingwood and is sometimes called camatillo or Mexican kingwood.  Information on how to distinguish between these two species can be found in the identification section below.

Note: This profile page had formerly listed no mechanical data for kingwood, and a dried weight of 75 lbs/ft3 (1,200 kg/m3). However, this commonly-cited density value comes from the wide-ranging 1943 volume, Timbers of the New World by Record and Hess, where they simply commented that the wood’s air dry specific gravity was “about 1.20.”[2]Record, S. J., & Hess, R. W. (1943). Timbers of the New World, p. 254. Yale University Press. However, I have since come across several more data sources (including an important one in Portuguese)[3]Lima, J. L. S. de, Serpa, F. da G., Sá, I. B. de, Mendonça, A. L., & Duarte, E. S. (1996). Características físico-mecânicas e energéticas de madeiras do trópico semi-árido do nordeste do … Continue reading which all paint a much more moderate picture of kingwood’s density and strength properties. Values from all sources have been averaged and are represented at the beginning of this profile page.

Images: Drag the slider up/down to toggle between raw and finished wood.

A special thanks to Steve Earis for providing a wood sample of this wood species.

Kingwood with flat sawn grain
Quartersawn kingwood with sapwood
Kingwood full board (46″ / 118 cm) long
Kingwood chess piece by Matthew Byrne
Kingwood (turned)

Do you have images of projects made from this wood species? You can submit them to me here.

Identification: See the article on Hardwood Anatomy for definitions of end grain features.

Kingwood (end grain 10x)
Kingwood (end grain 1x)
Kingwood with sapwood (end grain 10x)
Kingwood with sapwood (end grain 1x)

Porosity:POROSITY
Specifies the overall pore structure (ring-porous, semi-ring-porous, or diffuse porous), and notes if annual growth rings may still be seen even for diffuse porous hardwoods.

Click on the link “Porosity” for more details.
diffuse porous (occasionally appearing semi-ring-porous due to a subtle variation in pore size from earlywood to latewood)

Arrangement:ARRANGEMENT
Describes the more individual pore arrangements found throughout the end grain surface, such as solitary, multiples, chains, clusters, etc.

Click on the link “Arrangement” for more details.
solitary and radial multiples

Vessels:VESSELS
Describes the relative size and frequency of the pores (vessels), as well as any contents found in the pores, such as tyloses, colored mineral deposits, etc.

Click on the link “Vessels” for more details.
medium to large, few to moderately numerous; reddish-brown deposits occasionally present

Parenchyma:PARENCHYMA
Describes the pattern(s) of the parenchyma cells seen on the endgrain, such as vasicentric, aliform (winged or lozenge), confluent, and banded.

Click on the link “Parenchyma” for more details.
vasicentric, aliform, diffuse-in-aggregates, and banded (marginal)

Rays:RAYS
Describes the relative width and frequency of the rays (appearing as thin vertical lines on the endgrain), as well as a note on if these rays are visible with/without magnification.

Click on the link “Rays” for more details.
narrow width, normal spacing; rays not visible without magnification

Lookalikes/Substitutes: Another very similar species, Dalbergia congestiflora, is sometimes sold interchangeably as kingwood—though it’s more commonly called camatillo. The two woods have a very similar appearance and density, though they can usually be separated based on the parenchyma. True kingwood usually has more sparse and thin parenchyma bands (usually at the annual growth margins), while camatillo tends to have wider parenchyma bands that can be several cells wide.

Notes: Because of the very dark color of the heartwood, it can be helpful to use the lighter sapwood (if present) to look at the wood anatomy. A second alternate end grain image set with sapwood is also pictured.

Related Content:

References

References
1 2021. Dalbergia cearensisThe IUCN Red List of Threatened Species Accessed on 04 July 2025 .
2 Record, S. J., & Hess, R. W. (1943). Timbers of the New World, p. 254. Yale University Press.
3 Lima, J. L. S. de, Serpa, F. da G., Sá, I. B. de, Mendonça, A. L., & Duarte, E. S. (1996). Características físico-mecânicas e energéticas de madeiras do trópico semi-árido do nordeste do Brasil (Comunicado Técnico Nº 63). EMBRAPA-Centro de Pesquisa Agropecuária do Tropico Semi-Árido (CPATSA).
Subscribe
Notify of
guest
35 Comments
Inline Feedbacks
View all comments
Hammy Hamilton

Hello, I work restoring antique flutes, and have been doing a lot of research recently into the wood that they were made from, which are very often misattributed in sales catalogues and museum listings. One timber that is seen almost exclusively used in French flutes in the last half of the 19th century has often attracted comment from flute makers and collectors, but no one seems to really know what it is. One unusual aspect of it is the way it maintains the lighter colours, where most other woods used in flute making darken very quickly with exposure to light… Read more »

IMG_0328.JPG
IMG_0598.jpeg
IMG_0599.jpeg
IMG_0328 2.JPG
Graham

I’m no wood expert, but am wondering about cocus wood. Daniel Pailthorpe plays on this in the BBC SO, having sourced one of the last pieces in Britain. Many 19th century flutes were made of cocus, I believe. You might ask or compare.

Bates woodworking

Kingwood used on the outer edge of this cutting board. Great dark heartwood and light yellow sapwood with this stuff. Great to work and really hard.

Screenshot 2022-02-14 043917.jpg
Felipe

Real Kingwood for the enthusiasts.

95EA1D63-531B-425C-8925-D014171F125E.jpeg
99B17742-44DC-43DD-AE18-1B2432A5C1A8.jpeg
56556827-AD29-4CC2-BAAE-AA03A73F7027.jpeg
EC0DAAD8-D75B-455D-AD6E-44576C9CB677.jpeg
Valleyedgecanada

I Made a Mk2 frag keychain and the spoon is of Kingwood:

B52F6C98-F748-4C3D-95A3-41E4908C1E15.jpeg
0ACCB77A-C677-4838-9D3B-3B311716A4AF.jpeg
Mark

All I know is my Father purchased it as “Kingwood” in the 1980’s. Thanks again.

Mark

I have sent a sample to a lab for analysis and will let you know the outcome!

Mark

Hi Eric:
FYI you were correct, the wood is Pau Ferro. Thanks again.
Mark

Mark

Thank you Eric. Attached are more photos.

Kingwood 03.jpg
Kingwood 05.jpg
Mark

Can someone help me to confirm the planks in the attached photo are Kingwood?
Thanks,
Mark

IMG_1740 (2).jpg
Joseph Melton

I would bet the turned object (Kingwood) above is Cocobolo. It doesn’t resemble Kingwood at all. At least, in your photo.

steve

They are close relatives. There is cocobolo, kingwood, and para kingwood. The above photo is closest to kingwood.

Adam

As someone that works with kingwood daily as a turned object, I can attest that the wood in the photo is certainly kingwood (Dalbergia Cearensis). The grain in that particular piece exhibits grain patterns indicating long wet seasons and low levels of tannins. While most kingwood pieces are nearly a dark violet in color (hence the nickname violetwood), many are almost orange in color when subjected to long wet seasons.

Felipe

These pictures don’t resemble Kingwood at all. Kingwood has knots and are very pinkish like. The picture resembles Pau Ferro or some other species. Here a set of a beautiful MG Kingwood back and sides.

C6391B4F-D8C0-4F32-AF1F-BEA1764945DE.jpeg
Julia Xia

do you know high frequency vacuum wood dryer?Please check our websites https://www.sagamachinery.com

Marv Hamels

just informed this wood is now on the cites 2 appendix as well as most true central american rosewoods. anybody have more insight into this.

Jennifer C

We have worked with other types of Rosewood a lot, but this was a first for Kingwood. I think it is really pretty and like the mauve tones this particular piece has. These have a couple coats of CA and then a Carnauba wax top coat. Pretty!

Elaine

I have an old furniture which looks very like Kingwood. Is this kind of furniture expensive?

Peter

Camatillo , ( Mexican Kingwood ) to me smells like pipe tobacco when being worked

Peter

I’ve been doing a bit more work with the Camatillo and it smells more like coconut surfboard wax

Trevor

Well Eric I think you’re right about rosewood, but I’m not stopping because of the dust I’m quiting because its really hard to glue.

Jennifer C

Cyanoacylate (super glue) will glue it just fine. That is what you have to use and can even finish with it.

Ganymede

You could rub it down with acetone prior to gluing, and maybe try using titebond 2 or 3?

Trevor

Until I flare like a balloon Eric I don’t think I will quit turning this wood but I will be careful not to let the sandpaper fly out of my hands again.
Thanks for the advice.
~Trevor

Trevor

During a recent turning experience with Kingwood, when I was sanding with a piece of 400 sandpaper well it was turning to fast and it slipped out from under my hand and so the dust flew into my face I experienced a serious burning sensation in my nose and throat. Hope this helps.
~Trevor

Dave Langille

Recently I was turning a piece of Kingswood on the lathe and developed a severe rash on my turning hand and arm neck . I am not sentive to any other type of wood. Has any one else experienced a reaction such as this?

Lee Donald

Hey great site, lots of good info!
One question tho.. We have a sealed piece of wood (labeled “Eb”-I assumed Ebony) but after quartering it for turning projects it looks like either Kingwood or Cocobolo.
Both woods seem to have that “spice like scent” when worked and fairly close look.
Is it possible to post a picture or 2 for an answer?
-Lee D.

Bridgette Smith

dang I was really hoping to see an answer to your post Lee. I also had a sealed piece which I thought was Gaboon till I started turning. it is a very purple red with black streaking, has a good weight to it. I think smells like dill pickle when turning. Going through information on internet I am leaning towards Kingswood but would like to get a second opinion.