Wood Identification Guide

by Eric Meier

When attempting to identify a wood sample, it’s important to keep in mind the limitations and obstacles that are present in our task. Before starting, please have a look at The Truth Behind Wood Identification to approach the task in a proper mindset; I consider the linked article to be required reading for all those visiting my site with the intent of identifying wood.

1. Confirm it is actually solid wood.

Before proceeding too much farther into the remaining steps, it’s first necessary to confirm that the material in question is actually a solid piece of wood, and not a man-made composite or piece of plastic made to imitate wood.

A solid piece of Cocobolo: note how the grain naturally wraps around the sides and endgrain of the wood.

Can you see the end-grain? 

Manufactured wood such as MDF, OSB, and particleboard all have a distinct look that is—in nearly all cases—easily distinguishable from the endgrain of real wood. Look for growth rings—formed by the yearly growth of a tree—which will be a dead-giveaway that the wood sample in question is a solid, genuine chunk of wood taken from a tree.

Viewing the end of this “board” reveals its true identity: particleboard.

Is it veneered? 

If you see a large panel that has a repeating grain pattern, it may be a veneer. In such cases, a very thin layer of real wood is peeled from a tree and attached to a substrate; sometimes the veneer can be one continuous repeating piece because it is rotary-sliced to shave off the veneer layer as the tree trunk is spun by machines. Assuming it is a real wood veneer with a distinct grain and texture—and not merely a piece of printed plastic—you may still be able to identify the outer veneer wood in question, but you should still realize that is it only a veneer and not a solid piece of wood.

Large repeating patterns suggest a veneer.

Is it painted or printed to look like wood? 

Many times, especially on medium to large-sized flat panels for furniture, a piece of particleboard or MDF is either laminated with a piece of wood-colored plastic, or simply painted to look like wood grain. Many of today’s interior hardwood flooring planks are good examples of these pseudo-wood products: they are essentially a man-made material made of sawdust, glues, resins, and durable plastics.

2. Look at the color.

Some questions to immediately ask yourself:

Is the color of the wood natural, or is it stained?

If there is even a chance that the color isn’t natural, the odds are increased that the entire effort of identifying the wood will be in vain.

The reddish brown stain used on this piece of Jatoba (Hymenaea courbaril) has been planed away on top, exposing the paler color of the raw wood underneath.

Is it weathered or have a patina?

Many woods, when left outside in the elements, tend to turn a bland gray color. Also, even interior wood also takes on a patina as it ages: some woods get darker, or redder, and some even get lighter or lose their color; but for the most part, wood tends to darken with age.

Fresh sanding near the end of this Osage Orange (Maclura pomifera) board has exposed the characteristic yellow coloration of the wood, which has a strong tendency to shift down to a golden brown over time.

Is it possible to sand or plane the board to see the natural raw color of the wood?

The most predictable baseline to use when identifying wood is in a freshly sanded state. This eliminates the chances of a stain or natural aging skewing the color diagnosis of the wood.

3. Observe the wood grain.

If the wood is unfinished, then look at the texture of the grain. Ask yourself these questions:

Does the wood have an open, porous texture?

Most softwoods will be almost perfectly smooth with no grain indentations, while many common hardwoods have an open pore structure, such as oak or mahogany; though there are some hardwoods that are also smooth to the touch, such as maple.

Can you tell if the wood is quartersawn or plainsawn?

By observing the grain patterns, many times you can tell how the board was cut from the tree. Some wood species have dramatically different grain patterns from plainsawn to quartersawn surfaces. For instance, on their quartersawn surfaces, lacewood has large lace patterns, oak has flecks, and maple has the characteristic “butcher block” appearance.

Is there any figure or unusual characteristics, such as sapwood, curly or wild grain, burl/knots, etc.?

Some species of wood have figure that is much more common than in other species: for example, curly figure is fairly common in soft maple, and the curls are usually well-pronounced and close together. Yet when birch or cherry has a curly grain, it is more often much less pronounced, and the curls are spaced farther apart.

Curly Maple (sealed)
The strong, tight curl seen in this wood sample is very characteristic of Maple (Acer spp.).

4. Consider the weight and hardness of the wood.

If it’s possible, pick the piece of wood up and get a sense of its weight, and compare it to other known wood species. Try gouging the edge with your fingernail to get a sense of its hardness. If you have a scale, you can take measurements of the length, width, and thickness of the wood, and combine them to find the density of the wood. This can be helpful to compare to other density readings found in the database. When examining the wood in question, compare it to other known wood species, and ask yourself these questions:

Is the wood dry?

Wood from freshly felled trees, or wood that has been stored in an extremely humid environment will have very high moisture contents. In some freshly sawn pieces, moisture could account for over half of the wood’s total weight! Likewise, wood that has been stored in extremely dry conditions of less than 25% relative humidity will most likely feel lighter than average.

How does the wood’s weight compare to other species?

Taking into account the size of the board, how does its weight compare to other benchmark woods? Is it heavier than oak? Is it lighter than pine? Look at the weight numbers for a few wood species that are close to yours, and get a ballpark estimate of its weight.

A piece of Lignum Vitae is weighed on a small digital scale.

How hard is the wood? 

Obviously softwoods will tend to be softer than hardwoods, but try to get a sense of how it compares to other known woods. Density and hardness are closely related, so if the wood is heavy, it will most likely be hard too. If the wood is a part of a finished item that you can’t adequately weigh, you might be able to test the hardness by gouging it in an inconspicuous area. Also, if it is used in a piece of furniture, such as a tabletop, a general idea of its hardness can be assessed by the number and depth of the gouges/dings in the piece given its age and use. A tabletop made of pine will have much deeper dents than a tabletop made of Oak. Additionally, you can always try the “fingernail test” as a rough hardness indicator:  find a crisp edge of the wood, and with your fingernail try to push in as hard as you can and see if you’re able to make a dent in the wood.

5. Consider its history.

Many times we forget common sense and logic when attempting to identify wood. If you’ve got a piece of Amish furniture from Pennsylvania, chances are more likely that the wood  will be made of something like black walnut or cherry, and not African wenge or jatoba. You might call it “wood profiling,” but sometimes it can pay to be a little prejudiced when it comes to wood identification. Some common-sense questions to ask yourself when trying to identify a piece of wood:

Where did it come from?

Knowing as much as you can about the source of the wood—even the smallest details—can be helpful. If the wood came from a wood pile or a lumber mill where all the pieces were from trees processed locally, then the potential species are immediately limited. If the wood came from a builder of antique furniture, or a boat-builder, or a trim carpenter: each of these occupations will tend to use certain species of woods much more often than others, making a logical guess much simpler.

Despite its discoloration and wear, it’s very likely that this rolling pin is made of hard maple.

How old is it?

As with the wood’s source, its age will also help in identification purposes. Not only will it help to determine if the wood should have developed a natural patina, but it will also suggest certain species which were more prevalent at different times in history. For instance, many acoustic guitars made before the 1990s have featured Brazilian rosewood backs/sides, yet due to CITES restrictions placed upon that species, East Indian rosewood became a much more common species on newer guitars. (And this is a continuing shift as newer replacements are sought for rosewoods altogether.)

How large is the piece of wood?

Some species of trees are typically very small—some are even considered shrubs—while others get quite large. For instance, if you see a large panel or section of wood that’s entirely black, chances are it’s either painted, dyed, or stained: Gaboon ebony and related species are typically very small and very expensive.

What is the wood’s intended use?

Simply knowing what the wood was intended for—when considered in conjunction with where it came from and how old it is—can give you many clues to help identify it. In some applications, certain wood species are used much more frequently than others, so that you can make an educated guess as to the species of the wood based upon the application where it was used. For instance, in the United States: many older houses with solid hardwood floors have commonly used either red oak or hard maple; many antique furniture pieces have featured quartersawn white oak; many violins have spruce tops; many closet items used aromatic red cedar, and so forth. While it’s not a 100% guarantee, “profiling” the wood in question will help reduce the number of possible suspects, and aid in deducing the correct species.

6. Find the X-Factor.

Sometimes, after all the normal characteristics of a sample have been considered, the identity of the wood in question is still not apparent. In these instances—particularly in situations where a sample has been narrowed down to only a few possible remaining choices—it’s sometimes helpful to bring in specialized tests and other narrower means of identification.

The following techniques and recommendations don’t necessarily have a wide application in initially sorting out wood species and eliminating large swaths of wood species, but will most likely be of use only as a final step in special identification circumstances.

Odor

Believe it or not, freshly machined wood can have a very identifiable scent. When your eyes and hands can’t quite get a definitive answer, sometimes your nose can. Assuming there is no stain, finish, or preservative on or in the wood, quickly sand, saw, or otherwise machine a section of the wood in question, and take a whiff of the aroma.

Although new scents can be very difficult to express in words, many times the scent of an unknown wood may be similar to other known scents. For instance, rosewoods (Dalbergia spp.) are so named for their characteristic odor that is reminiscent of roses. Although difficult to directly communicate, with enough firsthand experience scents can become a memorable and powerful means of wood identification.

Fluorescence

While certain woods can appear basically identical to one another under normal lighting conditions, when exposed to certain wavelengths—such as those found in blacklights—the wood will absorb and emit light in a different (visible) wavelength. This phenomenon is known as fluorescence, and certain woods can be distinguished by the presence or absence of their fluorescent qualities. See the article Fluorescence: A Secret Weapon in Wood Identification for more information.

Black Locust: fluorescence (under blacklight)
Black Locust (Robinia pseudoacacia) glows a bright yellow-green when placed under a blacklight.

Chemical Testing

There are only a small number of chemical tests regularly used on wood, most of which are very specialized and were developed to help distinguish easily confused species with one another. They work by detecting differences in the composition of heartwood extractives. A chemical substance (called a reagent) is usually dissolved in water and applied to the wood surface: the surface is then observed for any type of chemical reaction (and accompanying color change) that may occur. Two of the most useful are the tests that are meant to separate Red and White Oak, and Red and Hard Maple.

Heartwood Extractives Leachability

Sometimes a wood species will have heartwood extractives that will be readily leachable in water and capable of conspicuously tinting a solution of water a specific color. For instance, the heartwood extractives contained in osage orange (Maclura pomifera) contain a yellowish-brown dye that is soluble in water. (This can sometimes be observed anecdotally when the wood is glued with a water-based adhesive: the glue’s squeeze-out is an unusually vibrant yellow.)

In a simple water extract color test, wood shavings are mixed with water in a vial, test tube, or other suitably small container, and the color of the water is observed after a few minutes. If the heartwood extractives are leachable by water, then a corresponding color change should quickly occur.

In addition to osage orange (Maclura pomifera)merbau (Intsia spp.), and rengas (Gluta spp. and Melanorrhoea spp.) are also noted for their readily leachable heartwood extractives. Because this property is quite uncommon, it can serve to quickly differentiate these woods from other lookalikes.

7. Look at the endgrain.

Perhaps no other technique for accurate identification of wood is as helpful and conclusive as the magnified examination of the endgrain. Frequently, it brings the identification process from a mostly intuitive, unscientific process into a predictable, repeatable, and reliable procedure.

Looking at the endgrain with a magnifier shouldn’t be a mystifying or esoteric art. In many cases, it’s nearly as simple as examining small newsprint under a magnifying glass. There are three components necessary to reap the full benefits contained in the endgrain:

I. A prepared surface.

When working with wood in most capacities, it becomes quickly apparent that endgrain surfaces are not nearly as cooperative or as easily worked as face grain surfaces. However, in this case, it is absolutely critical that a clear and refined endgrain surface is obtained.

For a quick glance of a softwood sample, a very sharp knife or razor blade can be used to take a fresh slice from the endgrain. However, in many denser species, especially in tropical hardwoods, one of the best ways to obtain a clear endgrain view is through diligent sanding. It’s usually best to begin with a relatively smooth saw cut (as from a fine-toothed miter saw blade) and proceed through the grits, starting at around 100, and working up to at least 220 or 320 grit, preferably higher for the cleanest view.

II. The right magnifier.

It need not be expensive, but whatever tool is used to view the endgrain should have adequate magnifying power. In most instances, 10x magnification is ideal, however, anything within the range of 8 to 15x magnification should be suitable for endgrain viewing. (Standard magnifying glasses are typically in the range of 2 to 4x magnification.)

These stronger magnifiers, sometimes called loupes, usually have a smaller viewing area than standard magnifying glasses. Fancier models—with built in lights, or larger viewing surfaces—are available at a premium; but the most basic models are usually only a few dollars.

amazon-button
amazon-button

III. A trained eye.

The third element that constitutes a proper endgrain examination is simply knowing what to look for. In analyzing the patterns, colors, shapes, and spacing of the various anatomical features, there is a veritable storehouse of information within the endgrain—all waiting to be unlocked. Yet, if these elements have not been pointed out and learned, the array of features will simply seem like an unintelligible jumble. The discipline of recognizing anatomical endgrain features is not easily summed up in a few sentences or even a few paragraphs, but it is nonetheless critical to the identification process. To this end, an in-depth look should be given to the various categories, divisions, and elements that constitute endgrain wood identification on the macroscopic level. (In this regard, macroscopic denotes what can be seen with a low-powered, 10x hand lens—without the aid of a microscope—rather than simply what can be seen with the naked eye.) Because the anatomy between softwoods and hardwoods is so divergent, each will be considered and examined separately:

Still stumped?

If you have a mysterious piece of wood that you’d like identified, you’ve got a few options for next steps:

USDA’s Forest Products Laboratory

You can mail your physical wood samples to the Center for Wood Anatomy Research

Pros:

  • Free
  • Professional wood identification

Cons:

  • Only available to US citizens
  • Slow turnaround times (up to a month or more)
  • Limited to three IDs per year

See their Wood ID Factsheet for more info.

Alden Identification Service

You can mail your physical wood samples (even small sections taken from antiques) to Alden Identification Service.

Pros:

  • Professional wood identification
  • Faster turnaround times (ranging from a few days to a week or two)

Cons:

  • Paid service

See their ordering page for more info. (Note that Harry Alden has written several books while at USDA, including both Hardwoods and Softwoods of North America.)

Ask for help online

If the wood ID is merely a curiosity, or non-critical, you can post pictures of the wood in question.

Pros:

  • Free
  • No need to send physical samples

Cons:

  • Greatly limited by the quality of the pictures provided
  • Extra work usually required to get adequate clarity in photos

See article of Common US Hardwoods to help find the most commonly used woods.

Get the hard copy

wood-book-standupIf you’re interested in getting all that makes The Wood Database unique distilled into a single, real-world resource, there’s the book that’s based on the website—the Amazon.com best-seller, WOOD! Identifying and Using Hundreds of Woods Worldwide. It contains many of the most popular articles found on this website, as well as hundreds of wood profiles—laid out with the same clarity and convenience of the website—packaged in a shop-friendly hardcover book.
Subscribe
Notify of
guest
4.2K Comments
Inline Feedbacks
View all comments
George

Hi we make knives in Australia, our overseas supplier from China has given us some handles that they say are from USA and called it Destert Iron wood, can you look at the pictures and give us your recomendations on what you think it is? I know this may be difficult but any help is appriciated
Thanks

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
USA??
handle33333.JPG
Palma

Hello, We just purchased a house with solid wood cabinets in the kitchen and dining room that have most people stumped. Two cabinet makers have said they are spalted hickory while another cypress. I love the cabinets and want to keep them and don’t want to paint them, just cleaned up and sealed. I have provided a photo of a cabinet face, a close up of the cabinet and a set in the dining room…with my pup. They are not super heavy…rather medium in weight. Would love to know what we have and if I’m correct in keeping the cabinets…many… Read more »

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
United States, Texas
Cabinets 2.jpg
Cabinets 1.jpg
Pepper on cabinets.jpg
Alfredo

Just wondering what kind of wood this is in my apartment. Hoping to get furniture to match or at least complement.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Illinois
20220907_230113.jpg
20220907_230128.jpg
20220907_230157.jpg
20220907_230406.jpg
Marisa

Hi I have this table that is real wood but each joined piece looks like they are from different wood species. The wood is easily dented. Also the table top is a natural wood colour but the sides of the table have been stained or dyed making it look like a red cherry wood. Can you please help advise what type of wood this table is made of. also when I wiped where the grooves were (you can see how red the flat panels on the side of the table are vs the table top ) with disinfectant, a bright… Read more »

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Australia
image.jpg
image.jpg
image.jpg
image.jpg
Marisa

Thanks Eric. Would you know why a bright red stain is coming off when I wipe the side panels with disinfectant. This occurred on all sides of the table. the red stain was easily wiped off from the entire first wooden groove (the section below after the red stripey panel) and the stain could be easily wiped off around on four sides of the table. The rest of the panels on each side do not having this red stain rub off. The wood still remains a dark red though after I wiped this off, as some stain has successfully soaked… Read more »

image.jpg
image.jpg
Crystal

I bought this stool and have always wondered what types of wood were used. Please see pictures

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Ontario, Canada
D36A5317-722C-479C-B9A9-2B33D29717D4.jpeg
FF949953-7253-4AC9-9544-C7BAB1ADC2EF.jpeg
DF99305F-23DC-4DB0-86CC-B89F13B87C6A.jpeg
Jennifer

Found this treasure of a lamp at a thrift store. After stripping the stain, here’s what I’m left with. The red coloring is quite prevalent. Would love to know the species. Thanks

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Midwest
90D40536-061D-4F47-BA22-1FDBD5A5648D.jpeg
Jennifer

Oh interesting – thanks for your time and feedback.

Seth Koket

I’m trying to identify the wood used in our arbor. I’m not sure why it has all the lines in it, The wood was stained so it’s dark, it was supposed to be cedar.
Thanks

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
Dallas ft worth
0D2F99B2-1961-4731-A56D-91A0BD8270F6.jpeg
F84E1E27-8FCC-446A-A8A8-CF05ACB43DA3.jpeg
Luis Mateo

Can anyone tell what specie of wood are this cabinets?

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
CA
IMG_20220825_113438084_HDR.jpg
IMG_20220825_113449782.jpg
Luis

Thank you so much!

Kyley Metcalf

Wondering what kind of wood my floor is.
my house was built in the 40’s. It has a weird smell as I am sanding it down.
please help me identify

Wood weight
Fairly light (like pine)
Distinct wood odor?
Yes
Geographic region
Missouri
E35B901F-2CD1-4F44-B29B-3555FA904289.jpeg
Tammie

I bought this China cabinet to paint the exterior black and I wanted to strip and stain the shelves a light stain. I have stripped and sanded but now I’m worried about staining because I have read certain woods will only darken such as mahogany. Any ideas what I have hear before I try and satin and get disappointed if it turns red again.

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
Unsure
44834767-47C3-49DD-B198-D867D3EF2F48.jpeg
6001F374-751C-436C-BE35-DD7DFB5FBA3E.jpeg
7F7C1A3E-210C-4CC4-8E3A-D5385223EE22.jpeg
B0B9AF5A-6C30-4118-9100-4B22897C0D21.jpeg
Wendy

Hello, I bought an old coffee table set that had marble slabs on-top, I am refinishing the wood bases and would be curious to know what kind of wood I am working on. Thank you

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
Unsure
307826D7-0F4C-4DE6-8637-FE4DBBF25E0A.jpeg
Wendy Coome

Here’s a better photo

image.jpg
James

Wondering what kind of wood this is. It came from overseas as a pallet. It is very heavy. When 5 pieces are joined together It takes 2 people to pick it up. Material on it was from Thailand.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Maybe thailand
20220816_071625.jpg
Stacey

Hello, could anyone help me identify what wood this is please? We recently purchased the property and not sure what it is, house was built in 2004 in UK. Any help would be much appreciated.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Wiltshire
Floor 1.jpg
Floor 2.jpg
Stacey

Here’s another photo

image.jpg
Michelle Rohm

Thrift store find. This is the back of a mirror. The front is stain that has been painted over. Will strip and refinish. Seems like a hardwood. Seems like a tight grain with no knots. Have you any idea based on the picture as to wood type ?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Pittsburgh Pa
image.jpg
Chris

Hello,
Looking for help identifying the wood on my dining set. It is quite old and has been in the family for many years. I have attached pictures of the finished top side and also of the unfinished bottom. Thank you!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
New York
D456C048-9E58-4AE8-98D4-5F26D34263D1.jpeg
C3D5DC42-AF4B-4F7E-8C5A-7B0BE7608E6F.jpeg
Gregor

Hi, I would greatly appreciate any help identifying this wood. It was sold among a shipment of Leadwood but it just looks very different from all the other pieces I received. It has a very warm red brown, much redder and lighter than the other pieces of leadwood with a courser looking texture of larger black pores/ spots. (The second picture shows it next to a piece of Leadwood). It is equally hard and heavy though. The density of this specific piece is 1.26 g/cm3 or 78.66 lbs/ft3 The closest matches from your fantastic database seem to be Camelthorn or… Read more »

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
No
Geographic region
Africa
WoodSample_01.jpg
WoodSample_02.jpg
WoodSample_03.jpg
WoodSample_04.jpg
Gregor

You’re right, it could be easily from another lot/ differently aged since I bought it from a shop and not directly from a sawmill.
I was just very surprised by the difference in colour texture. And it’s also the first time for me to work with Leadwood or any other heavy African wood species, so I don’t have any personal frame of reference or idea what else it could have been.
Thanks a lot for your opinion and the great database, Eric!

Ariane

hey! clearing out a storage unit – this table top is heavy but one person can lift it when upright (as shown in photo) The wood is sanded down/no varnish on bottom edge corners where table legs were attached. Don’t notice a distinct odor but that’s probably because it’s varnished. Really appreciate any help! Thanks :)

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
N/A
IMG_20220727_152055.jpg
IMG_20220727_152223.jpg
IMG_20220727_152238.jpg
IMG_20220727_152712.jpg
Marc

Hi Ariane, I am not an expert in recognising woods, but one thing you can see it is not a solid piece of wood, but veneered particleboard or plywood. In the third picture you see from three sides it has no endgrain. Beautiful table! I love this kind of veneered material, mostly used in vintage / mid century furniture.

Kira

Built in 2001

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Toronto Canada
5D590644-8124-43DA-AFD7-52D2EF261DF7.jpeg
272CD667-CD20-4FF8-AC09-67BB6C24A981.jpeg
2CB83980-D85B-457F-8511-7E9645EA21EA.jpeg
Regina

Did a knife class, and the instructor thinks this is canary wood, but is it?

Wood weight
Very light (like balsa)
Distinct wood odor?
I don't know
Geographic region
New York
Screenshot_20220731-202640~3.png
Regina

This is the only other photos I have unfortunately

Screenshot_20220802-132905.png
Screenshot_20220802-132855.png
Screenshot_20220802-133037.png
Screenshot_20220802-133024.png
Regina

It looks like it, thank you so much for your input!!

Armando

I purchased a home that looks to be built around 1900-1920’s. I’ve just sanded the floors and it appears I have two different type of wood here. Can you help me identify the two? I believe the bigger planks maybe pine. Not sure about the other.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
dont know
image.jpg
image.jpg
image.jpg
image.jpg
Armando

Thank you!! Much appreciated!!

Francesca Austin

We bought a table from someone who was moving who acquired it with his house. Very heavy – mover estimated 200 lbs for 5’ round table – and dense, no odor with a rippled top. Ignore the glue – that was to repair a non matching chair! What is it?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Old - Purchased used from someone who didn’t know what it was
4E38E5C0-B6FD-4BE3-A2E1-898943F92F21.jpeg
A416BE07-D3AB-490B-98CE-072610C80739.jpeg
CD7F27D8-F763-4364-9512-55573C02E97A.jpeg
Clinton Edmiston

Extending these solid wood interior doors. Not 100% on the type of wood.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
California
1B0DA3C9-D169-4D1B-917C-5EECCED61944.jpeg
C760E2FE-2D55-4502-B491-FF32B992CDF7.jpeg
Dale Lindsay

Old cuttingboard I found in relatives house. I’m stumped on this wood. I was thinking it was White Ash but not sure.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Tennessee
Screenshot_20220725-154949_Gallery.jpg
Leslie A Clement

It looks just like some of the yellow poplar. There distinct color difference between the sapwood and heartwood is a clue as well.

Sender

Dear Wood-Database.com,

Could you please tell me what type of wood this is? Thanks!

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
USA
Wooden_floor_1.jpeg
Wooden_floor_2.jpeg
Dale Lindsay

Looks kinda like white oak but that’s just a guess. I’m not an expert by any means. But the wide grain pattern is similar to white oak.

Helene Holl

Vintage or Antique Wooden Bowl. Heavy for its size. Can anyone help me identify the type of wood. Many thanks.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
United States, California
DFA5F25F-3AA6-494B-8848-E014485E6196.jpeg
F5B8B833-2006-4DA0-80F3-265B0EF07005.jpeg
A97068FD-84DD-40E8-AC36-664D6E488C58.jpeg
1E4AF1D1-0D3E-448E-9C95-ED789F090BE5_1_201_a.jpeg
Sander

Can anyone tell me what type of slab this is?

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
europe
9DCAEACA-74D1-4445-8DA6-7FB96EE720EC.jpeg
7003C237-206E-4D41-B9E6-9BF6A1C8704E.jpeg
Armando Lopez

What type of wood is this? I think it’s cherry wood.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Not sure
EEE8DB6C-B6B2-4B5F-A4AA-6EFFDF7E20DC.jpeg
Fabian

Great site here! I’m stumped with what type of wood this is (bad pun). First it’s from a Pier 1 TV tray table top, likely circa 1990’s. First thought it was bamboo but it has knots. I sanded finish down, it laughed at my 100 grit paper on power sander, though the paper was a bit worn…. It’s somewhat light but has a very, very hard surface. Yet it did absorb some teak oil stain, and teak oil sealer reasonably quickly. I also tested with Cetol as a finish. I’m repurposing as a cockpit table for my boat since it’s… Read more »

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
United States
7FCB066A-6FAE-457E-8A73-E4BDEF7D55AF.jpeg
6F6B81FE-D3BD-4D9C-AA31-536DE1B970E7.jpeg
47621527-2E17-4B93-A664-0615B7AFBB8E.jpeg
Fabian

Thank you

Raymond G Florant

Hi there!
I just moved into my first house, and pulled up the carpet to reveal hardwood! I’m not sure what kind of wood it is, could anyone take a look? In the picture, I believe there’s two finishes, and in the middle the threshold might be the raw wood.
Thank you!

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Massachusetts
IMG_6565.JPG
Last edited 3 years ago by Raymond G Florant
Raymond

Thanks!

Dale Lindsay

Not sure why someone had carpet over that. A little TLC and you’ve got a beautiful floor that will last forever.

Raymond

yeah, we were happy to see it was in good shape! We’re going to sand it all down, and then do a natural finish more like the light color under the carpet.

bozena boboryk

Hi
Does anyone know what type of wood is my furniture please?
Thank you for your help

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
London
2F55D850-8DD5-4A2C-BA77-D1292488E241.jpeg
6949718B-37D0-4F79-8D0C-ACF6C6428067.jpeg
Joos

Planning to refinish this outdoor chair and would like to identify wood so I understand how to sand, stain, and seal it. The chair and ottoman are very light weight for size.

Wood weight
Very light (like balsa)
Distinct wood odor?
No
Geographic region
New York
image.jpg
image.jpg
image.jpg
Kim

Anyone know what this is? Found this slab and I am making a bench but would like to know what type of wood it is.

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
I don't know
Geographic region
Maine
image.jpg
Kim

Thank you for the information, I had already stained the slab and have since begun stripping it off. I didn’t like the color, so was hoping to find out what type of wood so that I could better anticipate what the stain would look like.

Jeremy

Hand rail found in basement. Freshly sanded. Maple maybe

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
TN
0717221604.jpg
D. Vaughn

I purchased a home and have no idea what type of flooring this is. I need to replace some spots. Any idea? It’s textured and feels like real wood, home built in around 1975. I’m not sure if it’s a laminate floor or small pieces of wood laid in this pattern.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Midwest
7E7925D1-EB1C-4D0B-84FA-29E9A1DE7BEA.jpeg
27D8CFA2-5873-4010-B545-546D9D2AC5A6.jpeg
Joe

Purchased this lovely chair with the view of restoring it to reveal its full glory, any ideas of age and style would be helpful, thank you

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
unkown
chair.jpg
Joe

Thank you for the info Eric
Most appreciated
Joe

Dale Lindsay

Completely agree. Sand it down and start fresh and stain it however you want. Has lots of potential.

Nat

I’m trying to identify the type of wood that this sample is made out of.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Not sure
wood.jpg
Dale Lindsay

Kinda looks like Padauk also. Can you tell us what the original color was? Somewhere on the sample piece, take some 80 grit sandpaper and sand it down to the raw material and then post a picture of what that looks like. I think it’s Padauk but can’t be sure.

T.Brown

Moving the kitchen island around and found that the previous owner didn’t have hardwood under it installed, but we are having a real hard time finding a match. Any thoughts???

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Midwest, US
C91E9E99-D219-42D9-BF4C-F9AAD6372D1D.jpeg
8A16C8C7-2546-4829-8503-C56B27983CC1.jpeg
Dale Lindsay

I’m pretty sure that is Hickory. If not maybe Teak. Either way you have some fantastic flooring. Both are really great species. May get expensive finishing under the old island.
Google Hickory hardwood flooring and you’ll see what I mean. They look so similar.

Paula

I’m trying to identify the wood species on this antique desk or dining table.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Pennsylvania
4CF37A34-51CE-43E7-992B-69BBD342101E.jpeg
CD0FD9F8-3DB7-4C51-8EE8-B2E5C51A8FBB.jpeg
Paula

Thank you so much!

Donna Gum

I purchased 2 candlestick holders both made in Thailand. Upon closer inspection, they’re made from different wood. Ant idea?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Thailand
1657392570146850807387027114823.jpg
1657392626817462245186170419896.jpg
16573926535726426852884597455.jpg
16573926707124380456967782781052.jpg
Lukas

Hi, what does this wood grain look like? Trying to find a way to match it to repair the hole. Thank you!!

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
USA
Screen Shot 2022-07-07 at 4.30.41 PM.png
Lukas

Thank you!!!

Mrs. Aho

I’m trying to identify the type of wood that this plaque is made out of. The country of origin is China. The age of the wood is between 80-110 years old (so it has likely darkened a bit). It has been stored, so identifying a distinctive odor was difficult (it smells like a box LOL). I would likely have to have been a wood native to China, but I suppose it could have been imported (likely between 1900-1920 or thereabouts).

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
Minnesota, USA
Screenshot_20220701_135301.jpg
Mrs. Aho

A bigger picture might have helped. I asked someone else and they said maybe elm or cypress?

20220701_132542.jpg
Mrs. Aho

This one shows the back of the plaque. The small “dots” aren’t flaws in the wood, but rather small pegs where the craftsperson fastened the inlaid stone by pounding them through the back of the plaque. I apologize for not including these two photos with the original post.

Screenshot_20220701_135400.jpg
Lance Fromme

Restoring an old Excelsior dome top trunk. Thought these were all oak but I need to splice in a break that I can’t identify, or duplicate, so far. Leftmost slat, next to the black iron. Any ideas?

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Massachusetts
IMG_1054.jpg
Otto

Massive ceiling lamp. Probably some kind of fruit wood

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Idk
IMG20220701152411.jpg
Dennis

Does anyone know what type of wood this door is

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Pa
image.jpg
Dan Vibar

Can you recommend a laboratory in U.S. where a wood sample can be sent and analyzed? Can you give off hand based on the attached photo a ball park estimate which specie it is? I was told it is a very hardwood, the chainsaw’s chain used in slicing the tree toppled by a storm had to be replaced twice. The story behind it was the experienced chainsaw operator said he never came across any tree this hard in his decades of cutting trees

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
Yes
Geographic region
Asia -
inbound2261307055894355025.jpg
Gloria

Can you tell what wood this is? It was bought in mid 1980’s

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Florida
image.jpg
image.jpg
image.jpg
Michael Cavallaro

This is the top of a sanded vintage ming style low table, origen unknown. I’ve tried as best I can to identify the wood, and am hovering around sheesham, but I thought I’d turn to those wiser and more knowledgeable than I.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Southern Oregon
20220626_103234.jpg
Suzanne

Sheesh! I might be spoiled for life now. Love this! Never heard of it before but I google-lensed your picture and found more sheesham that looked very much like this, but I know nothing about it. And so far, there doesn’t appear to be anyone wiser and more knowledgeable than you. But how fun would it would be to use sheesham in a sheshed. :D Sheesham sheshed down by the seashore. Sheshore?

Paula Spano

This is a very heavy piece. Any ideas on what type of wood this is?

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
No
Geographic region
California
IMG_8722.jpg
Josh

Hello! I need to identify the wood in this executive desk! Thanks in advance! Definitely heavy enough that it normally takes 3 people to move it (or 2 really strong people) :)

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
Indiana
wood1.jpg
wood3.jpg
woos2.jpg
Rik Simpson

Hi any idea what this wood is likely to be?

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
United Kingdom
F859D9D5-95D7-4EC7-9E58-C68EA59135C4.jpeg
339EF80B-ECB9-49E8-B536-C9F15EED4DB2.jpeg
Chuck Kubin

Hem fir

1 35 36 37 38 39 41