Wood Identification Guide

by Eric Meier

When attempting to identify a wood sample, it’s important to keep in mind the limitations and obstacles that are present in our task. Before starting, please have a look at The Truth Behind Wood Identification to approach the task in a proper mindset; I consider the linked article to be required reading for all those visiting my site with the intent of identifying wood.

1. Confirm it is actually solid wood.

Before proceeding too much farther into the remaining steps, it’s first necessary to confirm that the material in question is actually a solid piece of wood, and not a man-made composite or piece of plastic made to imitate wood.

A solid piece of Cocobolo: note how the grain naturally wraps around the sides and endgrain of the wood.

Can you see the end-grain? 

Manufactured wood such as MDF, OSB, and particleboard all have a distinct look that is—in nearly all cases—easily distinguishable from the endgrain of real wood. Look for growth rings—formed by the yearly growth of a tree—which will be a dead-giveaway that the wood sample in question is a solid, genuine chunk of wood taken from a tree.

Viewing the end of this “board” reveals its true identity: particleboard.

Is it veneered? 

If you see a large panel that has a repeating grain pattern, it may be a veneer. In such cases, a very thin layer of real wood is peeled from a tree and attached to a substrate; sometimes the veneer can be one continuous repeating piece because it is rotary-sliced to shave off the veneer layer as the tree trunk is spun by machines. Assuming it is a real wood veneer with a distinct grain and texture—and not merely a piece of printed plastic—you may still be able to identify the outer veneer wood in question, but you should still realize that is it only a veneer and not a solid piece of wood.

Large repeating patterns suggest a veneer.

Is it painted or printed to look like wood? 

Many times, especially on medium to large-sized flat panels for furniture, a piece of particleboard or MDF is either laminated with a piece of wood-colored plastic, or simply painted to look like wood grain. Many of today’s interior hardwood flooring planks are good examples of these pseudo-wood products: they are essentially a man-made material made of sawdust, glues, resins, and durable plastics.

2. Look at the color.

Some questions to immediately ask yourself:

Is the color of the wood natural, or is it stained?

If there is even a chance that the color isn’t natural, the odds are increased that the entire effort of identifying the wood will be in vain.

The reddish brown stain used on this piece of Jatoba (Hymenaea courbaril) has been planed away on top, exposing the paler color of the raw wood underneath.

Is it weathered or have a patina?

Many woods, when left outside in the elements, tend to turn a bland gray color. Also, even interior wood also takes on a patina as it ages: some woods get darker, or redder, and some even get lighter or lose their color; but for the most part, wood tends to darken with age.

Fresh sanding near the end of this Osage Orange (Maclura pomifera) board has exposed the characteristic yellow coloration of the wood, which has a strong tendency to shift down to a golden brown over time.

Is it possible to sand or plane the board to see the natural raw color of the wood?

The most predictable baseline to use when identifying wood is in a freshly sanded state. This eliminates the chances of a stain or natural aging skewing the color diagnosis of the wood.

3. Observe the wood grain.

If the wood is unfinished, then look at the texture of the grain. Ask yourself these questions:

Does the wood have an open, porous texture?

Most softwoods will be almost perfectly smooth with no grain indentations, while many common hardwoods have an open pore structure, such as oak or mahogany; though there are some hardwoods that are also smooth to the touch, such as maple.

Can you tell if the wood is quartersawn or plainsawn?

By observing the grain patterns, many times you can tell how the board was cut from the tree. Some wood species have dramatically different grain patterns from plainsawn to quartersawn surfaces. For instance, on their quartersawn surfaces, lacewood has large lace patterns, oak has flecks, and maple has the characteristic “butcher block” appearance.

Is there any figure or unusual characteristics, such as sapwood, curly or wild grain, burl/knots, etc.?

Some species of wood have figure that is much more common than in other species: for example, curly figure is fairly common in soft maple, and the curls are usually well-pronounced and close together. Yet when birch or cherry has a curly grain, it is more often much less pronounced, and the curls are spaced farther apart.

Curly Maple (sealed)
The strong, tight curl seen in this wood sample is very characteristic of Maple (Acer spp.).

4. Consider the weight and hardness of the wood.

If it’s possible, pick the piece of wood up and get a sense of its weight, and compare it to other known wood species. Try gouging the edge with your fingernail to get a sense of its hardness. If you have a scale, you can take measurements of the length, width, and thickness of the wood, and combine them to find the density of the wood. This can be helpful to compare to other density readings found in the database. When examining the wood in question, compare it to other known wood species, and ask yourself these questions:

Is the wood dry?

Wood from freshly felled trees, or wood that has been stored in an extremely humid environment will have very high moisture contents. In some freshly sawn pieces, moisture could account for over half of the wood’s total weight! Likewise, wood that has been stored in extremely dry conditions of less than 25% relative humidity will most likely feel lighter than average.

How does the wood’s weight compare to other species?

Taking into account the size of the board, how does its weight compare to other benchmark woods? Is it heavier than oak? Is it lighter than pine? Look at the weight numbers for a few wood species that are close to yours, and get a ballpark estimate of its weight.

A piece of Lignum Vitae is weighed on a small digital scale.

How hard is the wood? 

Obviously softwoods will tend to be softer than hardwoods, but try to get a sense of how it compares to other known woods. Density and hardness are closely related, so if the wood is heavy, it will most likely be hard too. If the wood is a part of a finished item that you can’t adequately weigh, you might be able to test the hardness by gouging it in an inconspicuous area. Also, if it is used in a piece of furniture, such as a tabletop, a general idea of its hardness can be assessed by the number and depth of the gouges/dings in the piece given its age and use. A tabletop made of pine will have much deeper dents than a tabletop made of Oak. Additionally, you can always try the “fingernail test” as a rough hardness indicator:  find a crisp edge of the wood, and with your fingernail try to push in as hard as you can and see if you’re able to make a dent in the wood.

5. Consider its history.

Many times we forget common sense and logic when attempting to identify wood. If you’ve got a piece of Amish furniture from Pennsylvania, chances are more likely that the wood  will be made of something like black walnut or cherry, and not African wenge or jatoba. You might call it “wood profiling,” but sometimes it can pay to be a little prejudiced when it comes to wood identification. Some common-sense questions to ask yourself when trying to identify a piece of wood:

Where did it come from?

Knowing as much as you can about the source of the wood—even the smallest details—can be helpful. If the wood came from a wood pile or a lumber mill where all the pieces were from trees processed locally, then the potential species are immediately limited. If the wood came from a builder of antique furniture, or a boat-builder, or a trim carpenter: each of these occupations will tend to use certain species of woods much more often than others, making a logical guess much simpler.

Despite its discoloration and wear, it’s very likely that this rolling pin is made of hard maple.

How old is it?

As with the wood’s source, its age will also help in identification purposes. Not only will it help to determine if the wood should have developed a natural patina, but it will also suggest certain species which were more prevalent at different times in history. For instance, many acoustic guitars made before the 1990s have featured Brazilian rosewood backs/sides, yet due to CITES restrictions placed upon that species, East Indian rosewood became a much more common species on newer guitars. (And this is a continuing shift as newer replacements are sought for rosewoods altogether.)

How large is the piece of wood?

Some species of trees are typically very small—some are even considered shrubs—while others get quite large. For instance, if you see a large panel or section of wood that’s entirely black, chances are it’s either painted, dyed, or stained: Gaboon ebony and related species are typically very small and very expensive.

What is the wood’s intended use?

Simply knowing what the wood was intended for—when considered in conjunction with where it came from and how old it is—can give you many clues to help identify it. In some applications, certain wood species are used much more frequently than others, so that you can make an educated guess as to the species of the wood based upon the application where it was used. For instance, in the United States: many older houses with solid hardwood floors have commonly used either red oak or hard maple; many antique furniture pieces have featured quartersawn white oak; many violins have spruce tops; many closet items used aromatic red cedar, and so forth. While it’s not a 100% guarantee, “profiling” the wood in question will help reduce the number of possible suspects, and aid in deducing the correct species.

6. Find the X-Factor.

Sometimes, after all the normal characteristics of a sample have been considered, the identity of the wood in question is still not apparent. In these instances—particularly in situations where a sample has been narrowed down to only a few possible remaining choices—it’s sometimes helpful to bring in specialized tests and other narrower means of identification.

The following techniques and recommendations don’t necessarily have a wide application in initially sorting out wood species and eliminating large swaths of wood species, but will most likely be of use only as a final step in special identification circumstances.

Odor

Believe it or not, freshly machined wood can have a very identifiable scent. When your eyes and hands can’t quite get a definitive answer, sometimes your nose can. Assuming there is no stain, finish, or preservative on or in the wood, quickly sand, saw, or otherwise machine a section of the wood in question, and take a whiff of the aroma.

Although new scents can be very difficult to express in words, many times the scent of an unknown wood may be similar to other known scents. For instance, rosewoods (Dalbergia spp.) are so named for their characteristic odor that is reminiscent of roses. Although difficult to directly communicate, with enough firsthand experience scents can become a memorable and powerful means of wood identification.

Fluorescence

While certain woods can appear basically identical to one another under normal lighting conditions, when exposed to certain wavelengths—such as those found in blacklights—the wood will absorb and emit light in a different (visible) wavelength. This phenomenon is known as fluorescence, and certain woods can be distinguished by the presence or absence of their fluorescent qualities. See the article Fluorescence: A Secret Weapon in Wood Identification for more information.

Black Locust: fluorescence (under blacklight)
Black Locust (Robinia pseudoacacia) glows a bright yellow-green when placed under a blacklight.

Chemical Testing

There are only a small number of chemical tests regularly used on wood, most of which are very specialized and were developed to help distinguish easily confused species with one another. They work by detecting differences in the composition of heartwood extractives. A chemical substance (called a reagent) is usually dissolved in water and applied to the wood surface: the surface is then observed for any type of chemical reaction (and accompanying color change) that may occur. Two of the most useful are the tests that are meant to separate Red and White Oak, and Red and Hard Maple.

Heartwood Extractives Leachability

Sometimes a wood species will have heartwood extractives that will be readily leachable in water and capable of conspicuously tinting a solution of water a specific color. For instance, the heartwood extractives contained in osage orange (Maclura pomifera) contain a yellowish-brown dye that is soluble in water. (This can sometimes be observed anecdotally when the wood is glued with a water-based adhesive: the glue’s squeeze-out is an unusually vibrant yellow.)

In a simple water extract color test, wood shavings are mixed with water in a vial, test tube, or other suitably small container, and the color of the water is observed after a few minutes. If the heartwood extractives are leachable by water, then a corresponding color change should quickly occur.

In addition to osage orange (Maclura pomifera)merbau (Intsia spp.), and rengas (Gluta spp. and Melanorrhoea spp.) are also noted for their readily leachable heartwood extractives. Because this property is quite uncommon, it can serve to quickly differentiate these woods from other lookalikes.

7. Look at the endgrain.

Perhaps no other technique for accurate identification of wood is as helpful and conclusive as the magnified examination of the endgrain. Frequently, it brings the identification process from a mostly intuitive, unscientific process into a predictable, repeatable, and reliable procedure.

Looking at the endgrain with a magnifier shouldn’t be a mystifying or esoteric art. In many cases, it’s nearly as simple as examining small newsprint under a magnifying glass. There are three components necessary to reap the full benefits contained in the endgrain:

I. A prepared surface.

When working with wood in most capacities, it becomes quickly apparent that endgrain surfaces are not nearly as cooperative or as easily worked as face grain surfaces. However, in this case, it is absolutely critical that a clear and refined endgrain surface is obtained.

For a quick glance of a softwood sample, a very sharp knife or razor blade can be used to take a fresh slice from the endgrain. However, in many denser species, especially in tropical hardwoods, one of the best ways to obtain a clear endgrain view is through diligent sanding. It’s usually best to begin with a relatively smooth saw cut (as from a fine-toothed miter saw blade) and proceed through the grits, starting at around 100, and working up to at least 220 or 320 grit, preferably higher for the cleanest view.

II. The right magnifier.

It need not be expensive, but whatever tool is used to view the endgrain should have adequate magnifying power. In most instances, 10x magnification is ideal, however, anything within the range of 8 to 15x magnification should be suitable for endgrain viewing. (Standard magnifying glasses are typically in the range of 2 to 4x magnification.)

These stronger magnifiers, sometimes called loupes, usually have a smaller viewing area than standard magnifying glasses. Fancier models—with built in lights, or larger viewing surfaces—are available at a premium; but the most basic models are usually only a few dollars.

amazon-button
amazon-button

III. A trained eye.

The third element that constitutes a proper endgrain examination is simply knowing what to look for. In analyzing the patterns, colors, shapes, and spacing of the various anatomical features, there is a veritable storehouse of information within the endgrain—all waiting to be unlocked. Yet, if these elements have not been pointed out and learned, the array of features will simply seem like an unintelligible jumble. The discipline of recognizing anatomical endgrain features is not easily summed up in a few sentences or even a few paragraphs, but it is nonetheless critical to the identification process. To this end, an in-depth look should be given to the various categories, divisions, and elements that constitute endgrain wood identification on the macroscopic level. (In this regard, macroscopic denotes what can be seen with a low-powered, 10x hand lens—without the aid of a microscope—rather than simply what can be seen with the naked eye.) Because the anatomy between softwoods and hardwoods is so divergent, each will be considered and examined separately:

Still stumped?

If you have a mysterious piece of wood that you’d like identified, you’ve got a few options for next steps:

USDA’s Forest Products Laboratory

You can mail your physical wood samples to the Center for Wood Anatomy Research

Pros:

  • Free
  • Professional wood identification

Cons:

  • Only available to US citizens
  • Slow turnaround times (up to a month or more)
  • Limited to three IDs per year

See their Wood ID Factsheet for more info.

Alden Identification Service

You can mail your physical wood samples (even small sections taken from antiques) to Alden Identification Service.

Pros:

  • Professional wood identification
  • Faster turnaround times (ranging from a few days to a week or two)

Cons:

  • Paid service

See their ordering page for more info. (Note that Harry Alden has written several books while at USDA, including both Hardwoods and Softwoods of North America.)

Ask for help online

If the wood ID is merely a curiosity, or non-critical, you can post pictures of the wood in question.

Pros:

  • Free
  • No need to send physical samples

Cons:

  • Greatly limited by the quality of the pictures provided
  • Extra work usually required to get adequate clarity in photos

See article of Common US Hardwoods to help find the most commonly used woods.

Get the hard copy

wood-book-standupIf you’re interested in getting all that makes The Wood Database unique distilled into a single, real-world resource, there’s the book that’s based on the website—the Amazon.com best-seller, WOOD! Identifying and Using Hundreds of Woods Worldwide. It contains many of the most popular articles found on this website, as well as hundreds of wood profiles—laid out with the same clarity and convenience of the website—packaged in a shop-friendly hardcover book.
Subscribe
Notify of
guest
4.2K Comments
Sean Galliher

I got these samples from some pallets at work. I believe this is all the same species. It is some kind of very hardwood with beautiful grain patterns. Anyone know what it is?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
I'm not sure
IMG_20220315_091946531_HDR.jpg
IMG_20220315_091900246_HDR.jpg
16473507511181223147503831288392.jpg
16473509001428923719999215543013.jpg
Sean Galliher

I looked around alot on the web after I sent the question to you and I had settled on lati. I believe that’s what it is but I’m still not 100% certain. Either way, this is some very pretty wood. I did part of a wall in my bedroom with it. Turned out well. A little Danish oil to really bring out the grain patterns

IMG_20220227_214307987.jpg
Chris

I bought this piece at an architectural salvage place in St. Louis. So it’s probably of Midwest origin. Came out of a barn. 12″x6/4×17′. Ran it through the planer and this is the result. Help!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
Midwest
20220314_174304.jpg
20220314_174252.jpg
Chris

That was my first thought given that it was pulled from a barn and most likely a floor joist or roof truss being 17′ long. The grain isn’t like anything I’ve seen before. Parts look like the grain you see in pine and some places look like maple to me, but it’s too soft for maple. On a side note, not sure how it’s related, If it’s a character of the wood or a product of whatever was done in the barn. Carrying it, I rubbed my bare arm against the unplaned board and the wood fibers imbedded in my… Read more »

Helen

Any chance of identifying our dining room table please?

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
I don't know
Geographic region
United Kingdom
20220314_124030.jpg
20220314_124034.jpg
Maureen Hinds

I believe we were told this was from Bali. It was all hand made. It’s very, very, very heavy lol. I would guess it sinks. Thank you!

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
Yes
Geographic region
CA
PXL_20220313_232123989.jpg
PXL_20220313_232131662.jpg
joanna

Please help to identify this table – it was handmade very expensive they made it in walnut or mahogany – trying to find out which one i have thanks

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
california
4B3744F9-050F-4557-BCC6-B12B60485920.png
Joanna

Thank you Eric

Amy

This is a vintage waffle cone roller. It is either Northern European or American. If American, I believe it to be maple. If European, perhaps it is beech? It is of medium weight—heavier than pine, but lighter than oak—and hardness. Any help is appreciated!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Europe or America
Amy

Photos attached.

07586FB7-573B-4553-8FD9-C4621A3E8334.jpeg
9914FCF0-CC73-4B67-BFD4-D55A34404022.jpeg
444B653B-6E67-4810-8E75-DCFFEEBA5E5A.jpeg
8309424A-A27C-40B7-BE9A-819AC7B1A6DC.jpeg
Amy

Thank you!

Tuna

2 weeks of sanding and I’m very curious about the wood type. I’d be remiss to think I know. Thanks in advance for any help.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
South Florida
20220311_164146.jpg
20220311_164137.jpg
20220311_164151.jpg
Steph

Hi, I have sanded back this tallboy and would love to know what type of wood it is, it’s lovely! Can you help? Thank you!

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
Yes
Geographic region
Uk
20220309_222224.jpg
20220309_222142.jpg
Bill

Eric, picked up this solid wood table. Trying to ID the wood type. Table was made by Hastings Table Co in Hastings MI and sold by a furniture company in Buffalo NY that closed in the 1950s. Thx for the help.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Northeast
6ACAE2D8-A637-4756-A536-D5B396594EB1.jpeg
CB1748E3-0425-49B3-BC37-3E04DECE6E8C.jpeg
884E59E6-6F2A-4F81-BB43-A609A8A43D56.jpeg
Jennifer

Hello! My hardwood floors… trying to find a match after some had to be torn up for a water leak. We were told they are Miami Dade pine, but have no real idea if that is correct. House built in the Florida Keys in 1984.

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
Florida
Landon

Oven hood I am told is solid wood.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
North Idaho
IMG_3627.jpg
IMG_3626.jpg
Landon

Local hardwood store said it could be cherry like you said, but that it is probably alder. What do you think from these pictures? Thank you.

Dany

Vintage door that was stained a dark brown (see at the bottom), now sanded raw. Range of hues from almost blond to green to brown. (Don’t mind the casing)

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
MA
CCDAB97A-CA3E-4FEF-9913-1AFC33BE0266.jpeg
5B05F534-6FD0-4E05-9ADD-0360C7995724.jpeg
Dany
  1. Thanks very much, Eric. Here’s where I see green: 1. Dark brown sticking with green; 2. Faint green in the top rail; 3. Another piece of sticking, this one paler, but note the contrast with the reddish tinged stile
E121E8A7-93F7-465B-A104-83E2E04640AE.jpeg
08808F47-C033-4783-B746-F99DE9227C9B.jpeg
04130084-E09B-4B22-9FCA-4AC75A2B907B.jpeg
Landon

Eric,

This is an oven hood. I could check inside the hood and on the sides, and maybe disassemble a piece of it to see if its composite, veneer, or solid wood.

What do you think it is based on the visible grain pattern? Thank you

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
North Idaho
20220304_160726.jpg
Nathan

Old style tv stand – similar to a dresser in size

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
South Dakota
7D86EEEA-3873-4D6B-8D46-618EA9CF7C6A.jpeg
Joe

Quarter-sawn floorboard made of what?
comment image

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
NY, US
Lan

Hi Eric,
Can you please tell me what type of wood this is?
Thank you.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
California
4FBFFB93-2250-4BC1-8393-23E7578F7BE4.jpeg
37109DAB-FB78-4DCC-BFA7-5AB6D2D52A0E.jpeg
Robert

Is this pecky cypress?

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
NC
Screenshot_20220228-221716_Chrome.jpg
Robert

If it’s not cypress, what do you think it is?

Robert

I’m sure sure it’s not cypress, but still dont know what it is. Here is a shot of the left drawer.

Robert

Hickory, maybe?

IMG_20220302_183348818.jpg
Robert

End grain

IMG_20220302_212903716.jpg
Robert

Thank you for your time.

Deedra

What is this?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Kansas
0516EB85-9F14-4258-AE06-D1C5D301EEA8.jpeg
Beth

Hi – Would you be able to tell me what the trim is here? This is in my living room. It’s a 1920 bungalow in the NE that I bought a few months ago. I haven’t begun to do anything with the trim yet, but thankfully most of the rooms are unpainted! Thanks!

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
MA
living_rm_trim.jpg
Beth

oh, I found Douglas fir in the kitchen under 70’s sheet vinyl so maybe that does make sense. It just didn’t look quite the same as that so I wasn’t sure. A lot of the floors were redone at some point with oak, but it’s obvious the trim was already there (not the best job in some areas). Thank you!

Amy

I bought these salad servers in Costa Rica about 10 years ago and have always wondered what kind of wood it is. It’s very dense and heavy. Don’t know if this is the natural color or if it’s stained. It doesn’t *look* stained to me, but I’m no expert. I wish I had a better picture but they were a gift for my dad, so not in my possession any more. I’d love to find a set for myself but don’t know what to search for!

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
I don't know
Geographic region
Costa Rica
IMG_5754.JPG
Amy

Thank you so much!

Bev

can someone help me identify the wood on my table. It was sold as cherry wood but I’m not so sure that’s correct. thank you.

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
canada
wood.jpg
wood2.jpg
Darrin Skinner

Hi Eric, how about this wood? It’s on the walls in a house we just bought. Don’t have access to it yet. Probably there since 1961. This is in Northern California

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
CA
IMG_0673.JPG
IMG_0675.JPG
IMG_0674.JPG
Darrin Skinner

Thanks for the quick look. It’s very possible/likely it’s cedar given the area and age. In a woodworkers group, the vote was pretty split between cedar and pecky cypress. Obviously, I’ve love it to be the cypress given the value of that wood. How do I find out for sure? More/different photos after we move in and I take it all down? I can then cut and sand a board to see what it’s natural look is. There is about 500bf of this in the house.

Darrin Skinner

roger that. I’ll be taking it down in 3-4 weeks, will post back then when I know.

Chris

It may be heavier than “fairly heavy”, but it’s a pretty large piece so it’s hard for me to define the weight. I’m hoping this is a softball for you.
Thanks for any help!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Minnesota
20220129_092404.jpg
20220129_092417.jpg
20220129_092451.jpg
Sarah Jean Jones

Hi Eric I am so pleased I found this site. I have a rental property that I am restoring the floors in. They were stained and we have spent two days sanding them. It is a HUGE undertaking. I think they floors are pine or perhaps fir. I think they were done by the previous owner at least 20 years ago. They were stained, we are a good way along at removing the stain.

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
Alberta
IMG_6544.jpg
IMG_7510.jpg
IMG_7509.jpg
Robert

I have a solid ,strange wooden skull shaped hinged box Very knotty Heavy strange grain. Possibly a knot from a larger tree. Please tell the species of it.

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
No
Geographic region
Unknown
image.jpg
image.jpg
image.jpg
Chris

I am refinishing a table and have stripped down to bare wood. I’m trying to determine the type of wood this is as I have never seen a grain like this. The leaf of the table is very heavy. Any insight would be appreciated. 2 pics attached.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Connecticut
DF42FB05-A1C6-4479-8C98-4C2DE493F358.jpeg
E2428001-29EF-464E-8A82-DB1D88ED2BC7.jpeg
Ashlinn

Hi Eric! I was wondering if you could help me figure out what type of wood this is

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
California
B7B2AA10-AE62-4B57-9DB4-155A931A8F1B.jpeg
263390A5-4488-461C-B7EF-05737DD29A41.jpeg
Jeanne

Hello, I have an old armchair I’m restoring, built in Wisconsin, it had a dark stain and some sort of varnish finish. I stripped the finish off of the arms and found an interesting piece of reddish spotted wood on one of them. I’m wondering what it is and if the two arms are the same wood or just cut from different sections. Thanks!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Milwaukee
IMG_6711[1].jpg
IMG_6712[1].jpg
IMG_6713[1].jpg
Jeanne

Hi Eric, any thoughts on this wood?

Sara

Hi! This article is incredibly informative. I am so glad I found it! I was wondering if you could help me identify the wood that this bench is made out of. It dates back to at least as early as the 1970s, but I’m not sure of its origin before that, if any. It is a bench that we plan on restoring, and is heavy like oak. I really appreciate your time! Thank you!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
NY
D33862A1-F5D6-4828-86BF-231481C492B0.jpeg
3F8749AF-F439-4518-9C7F-A823745E711A.jpeg
D6B632A8-8B33-4728-A547-34FA9C3F32AC.jpeg
Sara

That was my guess. Thank you so very much!

Joseph McAnally

This tree was cut down in our park just a few days ago. It has a distinct yellow color.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
TX
1.jpg
2.jpg
Mitch Gillilan

Looks like honey locust for sure.

Maureen Merrifield

Hello! Would you be able to identify the type of wood my floors are made of? Below are some pics. Thanks for any help you can offer!

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
Northeastern Ontario, Canada
1C82328D-CC63-43DE-93D1-39E06C478854.jpeg
BCFF577A-DEF8-4F8F-AA13-2100F05A21C4.jpeg
Maureen Merrifield

Thank you! They definitely need some TLC! Lol. I don’t think they’ve ever been refinished. I’m looking into whether to refinish or just replace. Anyway, thanks again!

Anna

These are my floors. Any idea on the type of wood?

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
NJ
1DE48BB2-9FE7-4CCC-927C-E86311437EB2.jpeg
Andrew Toh

Hey Eric great post here, but I’m still trying to figure out what wood this is though I don’t have a magnifying glass to zoom into the grains, appreciate any input here.

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
No
Geographic region
Singapore
D857AECA-DB20-4704-AEE0-02B7E45B4563.jpeg
7FBCC1EF-A93C-4D3A-8638-2D3D34AC57B2.jpeg
Charisse Tasset

So happy I found your site! What type of wood is this? Kitchen Cabinets from a house in France. Thank you!

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Dallas, TX, United States
kit wood grain - Copy.PNG
Charisse Tasset

Another couple of images.

kitchen cabinets.jpg
The-Mill-House-Transformation-by-Marie-Laure-Helmkampf-4.jpg
Jack

Love the blog and saw you’re answering questions right now! Any chance identifying the wood of this hand railing? It’s the original railing from a ~100 year old home that we are currently paint stripping. The original floors were pine, would that give you any hint?

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
DC
59D9E279-7CFC-4944-92DD-D2D959E81AB9.JPG
Jack

Thanks Eric!

lilly

what type of wood? this is a 1949 bendix 95B3 radio Console that is freshly sanded! Some of the trims seems to have a greenish discoloration. Wood is very soft.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
texas
pre stain 2.jpg
lilly

What type of wood?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
texas
unnamed.jpg
Michelle

We love this midcentury wood paneling from our 1953 rancher, we would love to know what type of wood it is, if I had to guess I was thinking it was European Walnut in Crown Cut but I am not sure! Looking to an expert.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Seattle
thumbnail_IMG_6414.jpg
Michael

Please help me identify type of wood. Thank you

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
NC
D93AED16-8D99-42B2-94D7-FA70AEB29CED.jpeg
D5A0C699-6612-4283-B426-F8FDA6ADE529.jpeg
F63AA1A9-A720-445A-BF4A-0C849585935B.jpeg
77CD7288-2AE3-4928-9647-B851496900DD.jpeg
Michael

Thank you for your response. I’m on the way out to pressure wash and saw the end off one of the beams to help you help me. Will post pics shortly. Thanks again

Michael

Here are some better pics for you and anyone else that could help me identify type of wood. Sorry pics yesterday were shorty…..they’ve been dry stored for over fifty years though. Thank you very much

BF6842D4-6095-453A-AA6D-5DF7F14E9AF2.jpeg
F14CE689-42F4-46F6-9CFC-7587667FDF9D.jpeg
F5074677-18AB-4B02-8E35-4E9E0880750D.jpeg
051FA9EF-DD47-44BB-9804-5FED2ED9EB21.jpeg
Lahoma

Anyone know what this is? It’s an old vanity and bench

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
Virginia
0468C31E-10E6-4BB2-987F-112E57EB2FA2.jpeg
190BA878-BE11-4880-94AB-7731118CB75A.jpeg
Amber

I received a box of wood yesterday and this piece has me stumped. It is very gorgeous and I would love to know so I can definitely find more.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
North East Indiana
20220209_052424.jpg
Fanny

I am looking at all kinds of wood doors, can you please tell me what kind of wood they are?

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
I don't know
Geographic region
Florida
E1B6F281-D33C-4DF3-B762-5E55812D4757.jpeg
Ivan

Hi Eric.

Thanks for providing a great civic service. I am wondering if you can tell me what wood my stairs are? Thank you very much.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Toronto
79ABFA66-CC1D-49DC-8253-9662A6D503FE.jpeg
Ivan

Thank you very much.

Christine Murray

Hi,

I have some large scale, likely industrial door handles, solid wood with brass tips and brackets.They’re super heavy. If you run you nail across the wood, you can feel the grain as its slightly indented.
Any ideas as to what wood it is?
Pic attached, they need a good clean!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
UK
A883F20A-5644-4CDE-8482-2F4E2F29FCCA_1_201_a.jpeg
Ryan Totten

Possibly teak

Regina

I have a shipping crate i need to figure out what kind of wood it is.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
I’m in Texas not sure where it originated
87C2D86B-0420-4232-BC68-413807439458.jpeg
Candy Oreb

Trying to find out what type of wood my great grandmas highboy is

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
California
20220206_100205.jpg
Wendy Hickman

I am curious as the what type of wood this is. I am wanting to get matching dressers however I dont know what type of wood this is. I inherited from a family member that recently past.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
US
20220202_135927.jpg
Wendy Hickman

Here are more pics. I tried to get some without so much glare.

20220206_174925.jpg
20220206_175034.jpg
Wendy Hickman

I am curious as to what kind of of sleigh bed this is. I was thinking cherry but not 100%. Thanks

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
IN
20220205_202521.jpg
Matt Kennedy

Hi, I was wondering what type of wood this might be. Pictures are from the door of an old bureau. Sorry, pictures didn’t upload in my last comment!
Thanks!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
UK
5AD95E36-7B6B-48F1-8FD0-E3C6A7A2F185.jpeg
6AA255E9-59E4-4189-991A-38E8D7E4FB0C.jpeg
Rob Dearing

Rob Dearing
correction, it does float.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
Wyoming
A72EBF4F-EA2A-4226-B792-79C50D1745A6.jpeg
7F3D6323-AF97-4C0E-B690-3C462F05E2D4.jpeg
D170EBD1-30A1-4643-A6C7-F7B3A36AB3F9.jpeg
Rob Dearing

Thank you, would you like me to send you a sample for your collection?

Rob Dearing

You’re sample of Kempas is a great match! Thank you!

1 33 34 35 36 37 41