Yellow Buckeye (Aesculus octandra)
Yellow Buckeye (Aesculus octandra)

View More Images Below

Common Name(s): Buckeye, Ohio Buckeye, Yellow Buckeye

Scientific Name: Aesculus spp. (A. flava and A. glabra)

Distribution: Eastern United States

Tree Size: 50-75 ft (15-23 m) tall, 1.5-2 ft (.5-.6 m) trunk diameter

Average Dried Weight: 25 lbs/ft3 (400 kg/m3)

Specific Gravity (Basic, 12% MC): .33, .40

Janka Hardness: 350 lbf (1,560 N)

Modulus of Rupture: 7,500 lbf/in2 (51.7 MPa)

Elastic Modulus: 1,170,000 lbf/in2 (8.07 GPa)

Crushing Strength: 4,170 lbf/in2 (28.8 MPa)

Shrinkage: Radial: 3.6%, Tangential: 8.1%, Volumetric: 12.5%, T/R Ratio: 2.3

Color/Appearance: Heartwood is creamy white or light yellow, not clearly demarcated from the white sapwood. Can have grayish streaks. Buckeye burl can feature reddish brown knots, with light to dark gray swirls of discoloring (see pictures below).

Grain/Texture: Buckeye has a fine, even texture. Grain tends to be straight or slightly interlocked.

Endgrain: Diffuse-porous; very small pores in no specific arrangement; solitary and radial multiples of 2-3; growth rings faintly distinct due to marginal parenchyma; rays barely visible even with 10x lens; parenchyma banded.

Rot Resistance: Buckeye has poor decay resistance, and is rated as non-durable to perishable.

Workability: Buckeye is generally easy to work, but its unusually low density can lead to fuzzy surfaces, similar to Aspen or Cottonwood. Responds poorly to steam bending. Glues and finishes well.

Odor: Buckeye can have an unpleasant smell when green, which greatly subsides upon drying.

Allergies/Toxicity: Besides the standard health risks associated with any type of wood dust, no further health reactions have been associated with Buckeye. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Pricing/Availability: Not typically used for lumber due to its low density and strength, Buckeye can sometimes be found in board form, and should be comparable to Aspen or Basswood. Burls are more valuable and are sold for smaller specialty purposes.

Sustainability: This wood species is not listed in the CITES Appendices or on the IUCN Red List of Threatened Species.

Common Uses: Furniture, utility wood, boxes/crates, pulpwood; while the burl sections are used for electric guitar tops, pen blanks, and other small, specialty turned objects.

Comments: Buckeye is one of the softest and lightest hardwoods native to the United States. It’s low strength and bland appearance limit it to basic utility purposes.

The burl sections of Buckeye are much more prized, and their light-on-dark knot clusters, and unique, almost black discolorations make them sought after for a variety of specialty and hobbyist applications.

Related Species:

Related Articles:

Scans/Pictures:

Yellow Buckeye (Aesculus octandra)
Yellow Buckeye (sanded)

Yellow Buckeye (sealed)
Yellow Buckeye (sealed)

Yellow Buckeye (endgrain)
Yellow Buckeye (endgrain)

Yellow Buckeye (endgrain 10x)
Yellow Buckeye (endgrain 10x)

Buckeye Burl (sanded)
Buckeye Burl (sanded)

Buckeye Burl (sealed)
Buckeye Burl (sealed)

3
Share your experience

avatar
Photo and Image Files
 
 
 
3 Comment threads
0 Thread replies
0 Followers
 
Most reacted comment
Hottest comment thread
3 Comment authors
Michael LombardMoriacarolyn alexander Recent comment authors
  Subscribe  
Notify of
Michael Lombard
Michael Lombard

Buckeye seals very nicely with Cactus Juice, available from https://www.turntex.com and a number of other suppliers.

Moria
Moria

I get it from Cook Woods in Oregon. They ship. (I’m not affiliated at all, just was looking up buckeye as I just ordered a large burl piece and wanted to read info about its working properties.)

carolyn alexander
carolyn alexander

What should be used to seal buckeye wood. I have a dough tray made from buckeye which has not be sealed and I would like to preserve it. It will never be used to making dough.

thanks