Wood Identification Guide

by Eric Meier

When attempting to identify a wood sample, it’s important to keep in mind the limitations and obstacles that are present in our task. Before starting, please have a look at The Truth Behind Wood Identification to approach the task in a proper mindset; I consider the linked article to be required reading for all those visiting my site with the intent of identifying wood.

1. Confirm it is actually solid wood.

Before proceeding too much farther into the remaining steps, it’s first necessary to confirm that the material in question is actually a solid piece of wood, and not a man-made composite or piece of plastic made to imitate wood.

A solid piece of Cocobolo: note how the grain naturally wraps around the sides and endgrain of the wood.

Can you see the end-grain? 

Manufactured wood such as MDF, OSB, and particleboard all have a distinct look that is—in nearly all cases—easily distinguishable from the endgrain of real wood. Look for growth rings—formed by the yearly growth of a tree—which will be a dead-giveaway that the wood sample in question is a solid, genuine chunk of wood taken from a tree.

Viewing the end of this “board” reveals its true identity: particleboard.

Is it veneered? 

If you see a large panel that has a repeating grain pattern, it may be a veneer. In such cases, a very thin layer of real wood is peeled from a tree and attached to a substrate; sometimes the veneer can be one continuous repeating piece because it is rotary-sliced to shave off the veneer layer as the tree trunk is spun by machines. Assuming it is a real wood veneer with a distinct grain and texture—and not merely a piece of printed plastic—you may still be able to identify the outer veneer wood in question, but you should still realize that is it only a veneer and not a solid piece of wood.

Large repeating patterns suggest a veneer.

Is it painted or printed to look like wood? 

Many times, especially on medium to large-sized flat panels for furniture, a piece of particleboard or MDF is either laminated with a piece of wood-colored plastic, or simply painted to look like wood grain. Many of today’s interior hardwood flooring planks are good examples of these pseudo-wood products: they are essentially a man-made material made of sawdust, glues, resins, and durable plastics.

2. Look at the color.

Some questions to immediately ask yourself:

Is the color of the wood natural, or is it stained?

If there is even a chance that the color isn’t natural, the odds are increased that the entire effort of identifying the wood will be in vain.

The reddish brown stain used on this piece of Jatoba (Hymenaea courbaril) has been planed away on top, exposing the paler color of the raw wood underneath.

Is it weathered or have a patina?

Many woods, when left outside in the elements, tend to turn a bland gray color. Also, even interior wood also takes on a patina as it ages: some woods get darker, or redder, and some even get lighter or lose their color; but for the most part, wood tends to darken with age.

Fresh sanding near the end of this Osage Orange (Maclura pomifera) board has exposed the characteristic yellow coloration of the wood, which has a strong tendency to shift down to a golden brown over time.

Is it possible to sand or plane the board to see the natural raw color of the wood?

The most predictable baseline to use when identifying wood is in a freshly sanded state. This eliminates the chances of a stain or natural aging skewing the color diagnosis of the wood.

3. Observe the wood grain.

If the wood is unfinished, then look at the texture of the grain. Ask yourself these questions:

Does the wood have an open, porous texture?

Most softwoods will be almost perfectly smooth with no grain indentations, while many common hardwoods have an open pore structure, such as oak or mahogany; though there are some hardwoods that are also smooth to the touch, such as maple.

Can you tell if the wood is quartersawn or plainsawn?

By observing the grain patterns, many times you can tell how the board was cut from the tree. Some wood species have dramatically different grain patterns from plainsawn to quartersawn surfaces. For instance, on their quartersawn surfaces, lacewood has large lace patterns, oak has flecks, and maple has the characteristic “butcher block” appearance.

Is there any figure or unusual characteristics, such as sapwood, curly or wild grain, burl/knots, etc.?

Some species of wood have figure that is much more common than in other species: for example, curly figure is fairly common in soft maple, and the curls are usually well-pronounced and close together. Yet when birch or cherry has a curly grain, it is more often much less pronounced, and the curls are spaced farther apart.

Curly Maple (sealed)
The strong, tight curl seen in this wood sample is very characteristic of Maple (Acer spp.).

4. Consider the weight and hardness of the wood.

If it’s possible, pick the piece of wood up and get a sense of its weight, and compare it to other known wood species. Try gouging the edge with your fingernail to get a sense of its hardness. If you have a scale, you can take measurements of the length, width, and thickness of the wood, and combine them to find the density of the wood. This can be helpful to compare to other density readings found in the database. When examining the wood in question, compare it to other known wood species, and ask yourself these questions:

Is the wood dry?

Wood from freshly felled trees, or wood that has been stored in an extremely humid environment will have very high moisture contents. In some freshly sawn pieces, moisture could account for over half of the wood’s total weight! Likewise, wood that has been stored in extremely dry conditions of less than 25% relative humidity will most likely feel lighter than average.

How does the wood’s weight compare to other species?

Taking into account the size of the board, how does its weight compare to other benchmark woods? Is it heavier than oak? Is it lighter than pine? Look at the weight numbers for a few wood species that are close to yours, and get a ballpark estimate of its weight.

A piece of Lignum Vitae is weighed on a small digital scale.

How hard is the wood? 

Obviously softwoods will tend to be softer than hardwoods, but try to get a sense of how it compares to other known woods. Density and hardness are closely related, so if the wood is heavy, it will most likely be hard too. If the wood is a part of a finished item that you can’t adequately weigh, you might be able to test the hardness by gouging it in an inconspicuous area. Also, if it is used in a piece of furniture, such as a tabletop, a general idea of its hardness can be assessed by the number and depth of the gouges/dings in the piece given its age and use. A tabletop made of pine will have much deeper dents than a tabletop made of Oak. Additionally, you can always try the “fingernail test” as a rough hardness indicator:  find a crisp edge of the wood, and with your fingernail try to push in as hard as you can and see if you’re able to make a dent in the wood.

5. Consider its history.

Many times we forget common sense and logic when attempting to identify wood. If you’ve got a piece of Amish furniture from Pennsylvania, chances are more likely that the wood  will be made of something like black walnut or cherry, and not African wenge or jatoba. You might call it “wood profiling,” but sometimes it can pay to be a little prejudiced when it comes to wood identification. Some common-sense questions to ask yourself when trying to identify a piece of wood:

Where did it come from?

Knowing as much as you can about the source of the wood—even the smallest details—can be helpful. If the wood came from a wood pile or a lumber mill where all the pieces were from trees processed locally, then the potential species are immediately limited. If the wood came from a builder of antique furniture, or a boat-builder, or a trim carpenter: each of these occupations will tend to use certain species of woods much more often than others, making a logical guess much simpler.

Despite its discoloration and wear, it’s very likely that this rolling pin is made of hard maple.

How old is it?

As with the wood’s source, its age will also help in identification purposes. Not only will it help to determine if the wood should have developed a natural patina, but it will also suggest certain species which were more prevalent at different times in history. For instance, many acoustic guitars made before the 1990s have featured Brazilian rosewood backs/sides, yet due to CITES restrictions placed upon that species, East Indian rosewood became a much more common species on newer guitars. (And this is a continuing shift as newer replacements are sought for rosewoods altogether.)

How large is the piece of wood?

Some species of trees are typically very small—some are even considered shrubs—while others get quite large. For instance, if you see a large panel or section of wood that’s entirely black, chances are it’s either painted, dyed, or stained: Gaboon ebony and related species are typically very small and very expensive.

What is the wood’s intended use?

Simply knowing what the wood was intended for—when considered in conjunction with where it came from and how old it is—can give you many clues to help identify it. In some applications, certain wood species are used much more frequently than others, so that you can make an educated guess as to the species of the wood based upon the application where it was used. For instance, in the United States: many older houses with solid hardwood floors have commonly used either red oak or hard maple; many antique furniture pieces have featured quartersawn white oak; many violins have spruce tops; many closet items used aromatic red cedar, and so forth. While it’s not a 100% guarantee, “profiling” the wood in question will help reduce the number of possible suspects, and aid in deducing the correct species.

6. Find the X-Factor.

Sometimes, after all the normal characteristics of a sample have been considered, the identity of the wood in question is still not apparent. In these instances—particularly in situations where a sample has been narrowed down to only a few possible remaining choices—it’s sometimes helpful to bring in specialized tests and other narrower means of identification.

The following techniques and recommendations don’t necessarily have a wide application in initially sorting out wood species and eliminating large swaths of wood species, but will most likely be of use only as a final step in special identification circumstances.

Odor

Believe it or not, freshly machined wood can have a very identifiable scent. When your eyes and hands can’t quite get a definitive answer, sometimes your nose can. Assuming there is no stain, finish, or preservative on or in the wood, quickly sand, saw, or otherwise machine a section of the wood in question, and take a whiff of the aroma.

Although new scents can be very difficult to express in words, many times the scent of an unknown wood may be similar to other known scents. For instance, rosewoods (Dalbergia spp.) are so named for their characteristic odor that is reminiscent of roses. Although difficult to directly communicate, with enough firsthand experience scents can become a memorable and powerful means of wood identification.

Fluorescence

While certain woods can appear basically identical to one another under normal lighting conditions, when exposed to certain wavelengths—such as those found in blacklights—the wood will absorb and emit light in a different (visible) wavelength. This phenomenon is known as fluorescence, and certain woods can be distinguished by the presence or absence of their fluorescent qualities. See the article Fluorescence: A Secret Weapon in Wood Identification for more information.

Black Locust: fluorescence (under blacklight)
Black Locust (Robinia pseudoacacia) glows a bright yellow-green when placed under a blacklight.

Chemical Testing

There are only a small number of chemical tests regularly used on wood, most of which are very specialized and were developed to help distinguish easily confused species with one another. They work by detecting differences in the composition of heartwood extractives. A chemical substance (called a reagent) is usually dissolved in water and applied to the wood surface: the surface is then observed for any type of chemical reaction (and accompanying color change) that may occur. Two of the most useful are the tests that are meant to separate Red and White Oak, and Red and Hard Maple.

Heartwood Extractives Leachability

Sometimes a wood species will have heartwood extractives that will be readily leachable in water and capable of conspicuously tinting a solution of water a specific color. For instance, the heartwood extractives contained in osage orange (Maclura pomifera) contain a yellowish-brown dye that is soluble in water. (This can sometimes be observed anecdotally when the wood is glued with a water-based adhesive: the glue’s squeeze-out is an unusually vibrant yellow.)

In a simple water extract color test, wood shavings are mixed with water in a vial, test tube, or other suitably small container, and the color of the water is observed after a few minutes. If the heartwood extractives are leachable by water, then a corresponding color change should quickly occur.

In addition to osage orange (Maclura pomifera)merbau (Intsia spp.), and rengas (Gluta spp. and Melanorrhoea spp.) are also noted for their readily leachable heartwood extractives. Because this property is quite uncommon, it can serve to quickly differentiate these woods from other lookalikes.

7. Look at the endgrain.

Perhaps no other technique for accurate identification of wood is as helpful and conclusive as the magnified examination of the endgrain. Frequently, it brings the identification process from a mostly intuitive, unscientific process into a predictable, repeatable, and reliable procedure.

Looking at the endgrain with a magnifier shouldn’t be a mystifying or esoteric art. In many cases, it’s nearly as simple as examining small newsprint under a magnifying glass. There are three components necessary to reap the full benefits contained in the endgrain:

I. A prepared surface.

When working with wood in most capacities, it becomes quickly apparent that endgrain surfaces are not nearly as cooperative or as easily worked as face grain surfaces. However, in this case, it is absolutely critical that a clear and refined endgrain surface is obtained.

For a quick glance of a softwood sample, a very sharp knife or razor blade can be used to take a fresh slice from the endgrain. However, in many denser species, especially in tropical hardwoods, one of the best ways to obtain a clear endgrain view is through diligent sanding. It’s usually best to begin with a relatively smooth saw cut (as from a fine-toothed miter saw blade) and proceed through the grits, starting at around 100, and working up to at least 220 or 320 grit, preferably higher for the cleanest view.

II. The right magnifier.

It need not be expensive, but whatever tool is used to view the endgrain should have adequate magnifying power. In most instances, 10x magnification is ideal, however, anything within the range of 8 to 15x magnification should be suitable for endgrain viewing. (Standard magnifying glasses are typically in the range of 2 to 4x magnification.)

These stronger magnifiers, sometimes called loupes, usually have a smaller viewing area than standard magnifying glasses. Fancier models—with built in lights, or larger viewing surfaces—are available at a premium; but the most basic models are usually only a few dollars.

amazon-button
amazon-button

III. A trained eye.

The third element that constitutes a proper endgrain examination is simply knowing what to look for. In analyzing the patterns, colors, shapes, and spacing of the various anatomical features, there is a veritable storehouse of information within the endgrain—all waiting to be unlocked. Yet, if these elements have not been pointed out and learned, the array of features will simply seem like an unintelligible jumble. The discipline of recognizing anatomical endgrain features is not easily summed up in a few sentences or even a few paragraphs, but it is nonetheless critical to the identification process. To this end, an in-depth look should be given to the various categories, divisions, and elements that constitute endgrain wood identification on the macroscopic level. (In this regard, macroscopic denotes what can be seen with a low-powered, 10x hand lens—without the aid of a microscope—rather than simply what can be seen with the naked eye.) Because the anatomy between softwoods and hardwoods is so divergent, each will be considered and examined separately:

Still stumped?

If you have a mysterious piece of wood that you’d like identified, you’ve got a few options for next steps:

USDA’s Forest Products Laboratory

You can mail your physical wood samples to the Center for Wood Anatomy Research

Pros:

  • Free
  • Professional wood identification

Cons:

  • Only available to US citizens
  • Slow turnaround times (up to a month or more)
  • Limited to three IDs per year

See their Wood ID Factsheet for more info.

Alden Identification Service

You can mail your physical wood samples (even small sections taken from antiques) to Alden Identification Service.

Pros:

  • Professional wood identification
  • Faster turnaround times (ranging from a few days to a week or two)

Cons:

  • Paid service

See their ordering page for more info. (Note that Harry Alden has written several books while at USDA, including both Hardwoods and Softwoods of North America.)

Ask for help online

If the wood ID is merely a curiosity, or non-critical, you can post pictures of the wood in question.

Pros:

  • Free
  • No need to send physical samples

Cons:

  • Greatly limited by the quality of the pictures provided
  • Extra work usually required to get adequate clarity in photos

See article of Common US Hardwoods to help find the most commonly used woods.

Get the hard copy

wood-book-standupIf you’re interested in getting all that makes The Wood Database unique distilled into a single, real-world resource, there’s the book that’s based on the website—the Amazon.com best-seller, WOOD! Identifying and Using Hundreds of Woods Worldwide. It contains many of the most popular articles found on this website, as well as hundreds of wood profiles—laid out with the same clarity and convenience of the website—packaged in a shop-friendly hardcover book.
Subscribe
Notify of
guest
4.2K Comments
Inline Feedbacks
View all comments
Marie Graham

Hi! I found this frame at an estate sale. It is quite heavy. Any idea about type of wood? Thank you so much and advance

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Georgia
08780A03-4A39-465E-9F37-7744DAB004CB.jpeg
Marie Graham

Thank you so much!

Elizabeth

Recently purchased a home, and not sure what kind of wood floors we have. The home is 111 years old.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Midwest
20210903_110910.jpg
April

Any idea what type of wood this furniture is? It is quite heavy. I’m trying to determine what stain colors will look like on it without buying every sample available.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Southeast
IMG_9987.jpeg
IMG_9991.jpeg
IMG_9990.jpeg
IMG_9986.jpeg
April

I was thinking it’s somewhere in the oak family. Thank you so very much!

Constance Lai

I have wood windows from 1942 that were built as WWII federal worker housing. We always assumed they were long leaf pine, but it seems a lot denser through my 10x loupe.

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
dc
FF45EF4E-4691-4575-A16A-74778BCAF16B.jpeg
Therese

Trying to figure out what type of wood each of these are. First 2 are from the same bedroom set. Are any of them Elm?
Also would you have any idea if someone was allergic to elm tree, if having elm wood in the house could cause a reaction?
Thanks so much

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
OH - unsure about the woods origin
20210830_180120.jpg
20210830_180200.jpg
20210830_180451.jpg
20210830_180503.jpg
Cindy Paulick

Hello. I am looking to match my current hardwood floor, but have no idea what kind of wood it is. The house was built in 2003 in Colorado as a model home. The first picture is not bleached by the sun and second picture is. Thank you!

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Home built in Colorado
PXL_20210828_192823730.jpg
PXL_20210828_193632797.jpg
Tina C.

Can anyone identify this type of wood? It has a fragrant smell and the dresser is altogether quite heavy and hard. Is it oak? pine?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
not sure
20210826_141834.jpg
20210826_141825.jpg
Marcus Bumgardner

Pictures didn’t come through. Used wenge, purple heart and unknown hardwood. Dad used to make ink pens and gave me various hardwoods. All labeled except one. White one on ends. Would like to know what type of wood it is.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
Sc. But wood origin unknown
20210826_015251.jpg
16299598645387198582094012075269.jpg
20210826_023918.jpg
Jessica

I bought an old dining table recently. The top had a piece of laminate on it so I removed the laminate. We know that the laminate was not the original top. The laminate was added to it later. Under the laminate was veneer. I removed the veneer and this is what was underneath. Can anyone tell me what type of wood this is? And would anyone know about how old this table is?

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Mississippi
DB988073-117E-4E68-803B-BFEA55781585.jpeg
F7FC7C89-8F31-4F2D-AD3F-B7614AB96CB1.jpeg
1DDDCF9C-45F9-4F3C-8B0C-2DA9B2F2F16E.jpeg
5B23D970-6C55-4F28-BC01-82E804CF787F.jpeg
Jessica

I bought an old dining table recently. The top had a piece of laminate on it so I removed the laminate. Under the laminate was veneer. I removed the veneer and this is what was underneath it. Can anyone tell me what kind of wood this is? I don’t think it is letting me add a photo but it looks like different strips of wood put together most of the strips are a light color and then several throughout the table top are green.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Mississippi
Last edited 4 years ago by Jessica
Wendy

Can anyone identify what type of wood this is? I’m guessing pine as it was near our cabin and there were many pine and aspen trees. I’m guessing pine but curious as to what type specifically. Thank you!

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
Colorado rocky mtn national forest
8C726731-454D-46E2-B44F-DB437CDB1A3E.jpeg
Joanne Le Mura

It looks like crepe myrtle which I have growing in my yard. It is meant to be good for furniture construction as far as I know

Cindy Butor

Would anyone be able to tell me what kind of wood this is? It’s the wood trim on our closet door, and I’m trying to figure out what it is so I can replace the missing back trim. The darkest piece is when we first uncovered it; it was obviously stained. The other pictures are after we finished paint stripping and sanding it a couple times. Is it just extremely old pine? (I know it’s at least 50 years old.)

Wood weight
Fairly light (like pine)
Distinct wood odor?
Yes
Geographic region
Kentucky
20210814_192522.jpg
20210815_204045.jpg
20210819_222237.jpg
Megan

I just bought a house that was built in 1941 and took up the carpet to find this wood can anyone identify what kind

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
ID
20210816_081052.jpg
Doc

What type of wood is this? Thanks in advance. Brent

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Not sure where it came from.
PXL_20210809_215624671.jpg
Tim

Just sanded the top of this coffee table down and I’m trying to figure out what type of wood it is, any helpis appreciated!

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
Central
20210809_161944.jpg
Kellie Snow

My house was built 1850 these are the original wood floors. Planks are 10″. House is in Ohio. I want to care for them appropriately, can anyone help identify the type?

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
OH
20210807_092827.jpg
20210807_093108.jpg
Emily

Also curious about this desk I have … Unfortunately I did not get photos of the wood while it was raw, its does have ‘honey’ stain on it and I don’t remember if it had a distinct smell while sanding..

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Not sure, I'm in NV
PSX_20210607_225346.jpg
PSX_20210616_010255.jpg
20210806_050919.jpg
20210806_050547.jpg
Emily

I’ve acquired this wardrobe and I’m trying to learn as much about it as possible, including what type of wood it’s made out of..
Kind of smells like coffee when sanded..
Front and end grain photos are taken from the drawer after being sanded

TIA :)

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
Not sure, I'm in NV
20210411_213313.jpg
20210411_213348.jpg
20210806_044145.jpg
20210806_044402.jpg
Steve

This is my back door freshly sanded. Home was built in 1912. Design and original hardware markings indicate it is the original door. Home is in northwest Illinois.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
Northwest Illinois
9FEAF606-F1F5-4EC0-B753-63485672CB65.jpeg
A0284598-7A06-4E73-A56C-EBBF62A49CE3.jpeg
Steve

Thanks for your help!

Karen

100+ year old dining table, had 3 extension leaves that were in horrible non-restorative shape. Has been in the family for years. Grandparents from Niagara, NY area as well as Canada. Table had very dark, maybe black, stain with several layers of urethane and furniture polish. Was easier to sand than use stripper. Stripper took forever and I still ended up sanding. Labeled photos.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Lower Peninsula of Michigan, Niagara, NY; Niagara, Ontario, Canada or Thunder Bay, Ontario, Canada
B188697C-82ED-40AD-83E3-31DC6347E43C.jpeg
2123B1A7-51D0-4943-9751-31F241AC1F92.jpeg
7C543692-E986-49C6-B7B9-FBDC87128E78.jpeg
66701D6B-E21A-4F50-854B-EF991ECF2437.jpeg
Cameron

Looking for some help identifying this wood that is in the living room of the house I just bought. I live in the upper peninsula of Michigan if that helps. Is it cedar? When I took a board off it smelled like cedar but it’s hard to tell as the room on the other side is done in a similar way but the boards look different.

photos were too big here is a link to a Google drive folder with the pictures.

https://drive.google.com/drive/folders/1-GIdBYcBs9s8xUWSRHumUqOBjXcLQWGU

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
Upper Peninsula of Michigan
Susan Daniero

Sorry, it took me 3 tries to upload a photo. :-(
Hi! I’m trying to figure out what wood my ceiling is made of. I’d like to add an accent wall to my home using the same wood and stain. Please take a look and help.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
United States
IMG_3313.jpg
Susan Daniero

Thanks Eric! Any chance it could be cedar? Here is a closer image.

ceiling_wood_image.jpg
Chris

Could someone please identify this wood? When I was cleaning out my father’s house after he passed a couple of years ago, I found several pieces just like this, all of equal size (4″x6″), finished with beveled corners. It very well may be stained, I just don’t know. He was an amateur woodworker, so that would explain why he had them, but I only took one block as a curiosity. Please don’t tell me if it is rare or valuable as the rest of the pieces are now gone forever (j/k).

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
USA
Wood1.jpg
Wood2.jpg
Elle

I’ve been trying to sand (using random orbital sa der) the painted finish off of our wooden fireplace mantle and it is taking forever. What’s mostly left now are some white paint spots and black spots I can’t identify. Can you tell from these pics what type of wood this might be? Also, any idea about the black areas?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
Chicago
20210725_105233.jpg
20210725_103913.jpg
Linda

Thanks Eric!

Steve

Sorry just one more comment. By clear grain, in my comment below I mean distinctive grain. I’ve looked around at some samples and I was wondering if this was oak?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Western Australia
Steve

Hi all. This is a very interesting article. This chair has a clear grain I think. Located and probably made in Australia. Does anyone have any idea of what it might be made of? Thanks if you can help.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Western Australia
Dining chair top of back splat.jpg
Dining chair sideview.jpg
Dining chair.jpg
Emily

Here are four of the pics from my comment—upload didn’t work the first time.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Chicago
91B16706-4BFB-4872-AA26-969F85ABE2C8.jpeg
26CCBE3B-AA51-4215-9DBA-2722554924BB.jpeg
8E13713C-D32B-483B-ADD4-A20141E62BA6.jpeg
97D0BEDE-5EB3-47C2-A1CE-76AF6A9D35EF.jpeg
Emily

This is a cross section I cut off the base of a chair leg from a very weathered outdoor chair. The dust from sawing/sanding is a brownish color. I sanded it and wiped it off with water, so the pictures I’m attaching include the wood when it’s wet, and also as it’s drying. (I can specify which is which if needed). There’s another picture of one of the legs after sawing, as well. Given how weathered the wood is, I can’t know if it originally had an odor. It just doesn’t now, though. Same goes for sinking in water—I don’t… Read more »

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Chicago
Caitlin

Bought this table from someone who picked it up at an estate sale and then refinished it. The seller says they were told it was from the 1960s – but then again everyone wants MCM furniture, so who knows. The table is stamped “MADE IN JAPAN” and is quite heavy – took more than a bit of effort for my partner and I to move it, though I can’t say I actually tested if it would sink in water!

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
No
Geographic region
Seattle, WA
IMG_2445.jpg
IMG_2446.jpg
IMG_2447.jpg
Efstathios Sideris

Hi everyone, just trying to identify what sort of wood that is! Thanx

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Berlin
IMG_20210720_132805.jpg
Corinna Staub

Hello, any idea what kind of wood this might be? The next to last pic is the underside of the table. Thank you

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
Virginia
IMG_0288.jpg
IMG_0355.jpg
IMG_0423.jpg
IMG_0424.jpg
Corinna Staub

Thank you for your reply, Eric!

Karl Gustav

Hi there,

Any help with identifying this type of wood ? It’s not light-weight, it’s rather solid and the legs of this table have a spot-like, line-like pattern. When sanded and unvarnished it is very light in color. It also had no significant or noticeable smell when it was sanded.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Namibia
tb.jpg
tb0.jpg
Lisa Marie Simmons

Anyone know what kind of wood this is?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Houston,Texas
image.jpg
image.jpg
image.jpg
Melanie

Hello, I hope someone can help me identify the type (or types) of wood used to make this vanity. There’s a Schuster’s Milwaukee sticker inside and it had bakelite handles so I believe it would have been made sometime between 1930 – 1961 and is handmade. The wood weight varies. The drawers and doors are much heavier than the actual frame. I didn’t refinish the inside so I took photos from there. The first one is the inside of the back panel and appears to be unfinished. The rest have the original finish. The second one is the inside of… Read more »

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
Purchased at a store in Milwaukee Wisconsin
Back Panel Inside - Unfinished.jpg
Door Inside - Original Finish.jpg
Drawer Inside- Original Finish.jpg
Inside Cabinet Section - Original Finish.jpg
Melanie

Thanks Eric,
I appreciate your response.

Gwen

Hello, any idea what wood this would be ?

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
I don't know
Geographic region
Montreal, Canada
Daniel

I just moved into a new home and want to figure out what type of wood was used on the doors, which appear to be relatively new. I’d like to use the same type of wood to build a floating beach inside. Any idea what this might be?

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
Colorado
029059E5-5B9A-4966-AF22-A7E3F1B9550E.jpeg
1B47653B-CC66-4811-9F69-FC4A092F5227.jpeg
Juian Spooner

Any idea what this is it is quite heavy and v.hard, was part of a pallet for something heavy but don’t know what or where ftom

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Unsure
16262460069243409286147436606661.jpg
Juian Spooner

Do you know what wood this is, it’s hard but quite light

Wood weight
Fairly light (like pine)
Distinct wood odor?
No
Geographic region
UK?
16262454550731798840388952175689.jpg
CLAIRE

Hi …my belief is that this is carved ironwood…am I correct?

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
Yes
Geographic region
West Midlands
20210712_151527.jpg
20210712_151705.jpg
20210712_151459.jpg
20210712_151432.jpg
LSM

Can someone ID this please? Australian made. Fairly heavy. Durable. I think it’s a hardwood.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
I don't know
Geographic region
Australia
1R4pnqv.jpeg
r4PfzuD.jpeg
unAIkTS.jpeg
Janet

Uncovered this hardwood flooring in a 150 plus year old structure … cannot identify . Any help is appreciated ! Thanks so much

Wood weight
I don't know
Distinct wood odor?
Yes
Geographic region
Ohio
Janet

Attaching pics again ?

3153C4C2-4458-4C2C-835F-235C44D6A9D6.jpeg
94030181-8DBA-4C6E-A4F2-5AFFA55BF8C6.jpeg
D97C00BE-F3FE-4C58-8333-A659CBE3C6E2.jpeg
Rick

Hello all, I need to know what kind of wood this is. Very tight grain, pretty heavy and definitely a hardwood. I apologize if the pictures don’t show enough, I can try to get a closer pic but I’ve already stained it. Any help would be appreciated, generally speaking most hardwood guitars are ash or alder, I’m just not sure what this is.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Not sure
IMG_0622.JPG
IMG_0657.JPG
Rick

Well thanks Eric, I appreciate the input lol

Goran

2 buildings – roof beams.

Wood weight
I don't know
Distinct wood odor?
I don't know
Geographic region
Michigan
IMG_0824.JPG
IMG_0827.JPG
Goran

Meant to add that I am trying to identify the type of wood. The buildings are from 1900s, but the roofs seem to have been updated recently.

Last edited 4 years ago by Goran
Cassie

I’m trying to figure out what type of wood this bench is. It was originally a bench in a Nashville train station and has been in the family for 40+ years. It’s heavy and I can’t make a mark with my fingernail. I’d like to remove the finish but would like to know what it’ll look like underneath first.

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
I don't know
Geographic region
Nashville TN
5ED9085E-43E3-4C6D-8F0C-3F7979626275.jpeg
B720BCB8-AD22-421C-9029-701BA7DA5E95.jpeg
Will

Can you help me with what type of flooring this is? House was built in 1967. I believe this is original flooring that has never been refinished and was under carpet for decades. It is solid wood tongue and groove 2.25” planks

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
Virginia
45F33DB8-391E-43C1-B0F4-E03AFFFA7271.jpeg
77F1B23F-C407-4ADA-8A7C-D63F9D5E52AA.jpeg
Skylar

Got a few pieces of this from a friend who took it out of his attic when he was redoing his 1910 house. Would love to know what kind of wood this is so I can figure out the best projects for it.

Wood weight
Fairly light (like pine)
Distinct wood odor?
I don't know
Geographic region
Florida
Last edited 4 years ago by Skylar
Mia

Hello, this salad bowl is very heavy – 3.5 pounds, however I don’t know if it sinks in water but I believe it would. It’s 5″ high, 13.75″ in diameter. Dark (stain?) outside, light (stain?) inside. No clue where it’s from or what the wood is; I’m inquiring! Thank you in advance for information.

Wood weight
Extremely heavy (sinks in water)
Distinct wood odor?
No
Geographic region
absolutely no idea
Salad bowl (2).JPG
Salad bowl (1).JPG
Salad bowl (3).JPG
Salad bowl (4).JPG
Lisa

Pictures didn’t post on the original thread. Would like to identify. I would love to restore this beauty. I plan on placing in my kitchen and trying to figure out the best way to refinish. The door came from Louisiana the hardware dates to 1930’s. The door is heavy.

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Louisiana
AC6C6A67-EF6C-49DB-AF08-14CE28DB2BD4.jpeg
8B2B46AA-9EAE-4E31-AA0D-09ED4601144E.jpeg
Lisa

Hello. Can you tell me what type of wood this is. We purchased these today for our kitchen. The place where we purchased it does a lot with reclaimed wood. The original length was 10ft and at least 2” high. The owner of the reclaimed wood place gets a lot his wood from barns in upper mid west.

01FB7C74-7399-4649-A5B2-073A452D3BA2.jpeg
3B529A7F-7B62-4471-A5B8-57EC0554A4B2.jpeg
Jess

I am refinishing a dresser and sanded off all the (horrible) paint as finish from the drawer fronts, I am wondering what type of wood the veneer is.
The darker portions have an almost grey undertone and the middle, lighter portions have a bit of a yellow undertone, both are still a bit dusty from my sanding though.

Wood weight
I don't know
Distinct wood odor?
No
Geographic region
Ontario, Canada
received_239883470998736.jpeg
received_515282713019177.jpeg
Jess

Thanks! I’ve sanded off the paint and finish that was on this piece, the lighter wood is very dry, the darker wood is beautifully smooth though.

16255826571135115627075131114348.jpg
Kim

Would like to identify this wood

Wood weight
Fairly heavy (like oak)
Distinct wood odor?
No
Geographic region
Canada
image.jpg
1 30 31 32 33 34 41