Wood Identification Guide

Wood Identification Guide

by Eric Meier

When attempting to identify a wood sample, it’s important to keep in mind the limitations and obstacles that are present in our task. Before starting, please have a look at The Truth Behind Wood Identification to approach the task in a proper mindset; I consider the linked article to be required reading for all those visiting my site with the intent of identifying wood.

1. Confirm it is actually solid wood.

Before proceeding too much farther into the remaining steps, it’s first necessary to confirm that the material in question is actually a solid piece of wood, and not a man-made composite or piece of plastic made to imitate wood.

A solid piece of Cocobolo: note how the grain naturally wraps around the sides and endgrain of the wood.

Can you see the end-grain? 

Manufactured wood such as MDF, OSB, and particleboard all have a distinct look that is—in nearly all cases—easily distinguishable from the endgrain of real wood. Look for growth rings—formed by the yearly growth of a tree—which will be a dead-giveaway that the wood sample in question is a solid, genuine chunk of wood taken from a tree.

Viewing the end of this “board” reveals its true identity: particleboard.

Is it veneered? 

If you see a large panel that has a repeating grain pattern, it may be a veneer. In such cases, a very thin layer of real wood is peeled from a tree and attached to a substrate; sometimes the veneer can be one continuous repeating piece because it is rotary-sliced to shave off the veneer layer as the tree trunk is spun by machines. Assuming it is a real wood veneer with a distinct grain and texture—and not merely a piece of printed plastic—you may still be able to identify the outer veneer wood in question, but you should still realize that is it only a veneer and not a solid piece of wood.

Large repeating patterns suggest a veneer.

Is it painted or printed to look like wood? 

Many times, especially on medium to large-sized flat panels for furniture, a piece of particleboard or MDF is either laminated with a piece of wood-colored plastic, or simply painted to look like wood grain. Many of today’s interior hardwood flooring planks are good examples of these pseudo-wood products: they are essentially a man-made material made of sawdust, glues, resins, and durable plastics.

2. Look at the color.

Some questions to immediately ask yourself:

Is the color of the wood natural, or is it stained?

If there is even a chance that the color isn’t natural, the odds are increased that the entire effort of identifying the wood will be in vain.

The reddish brown stain used on this piece of Jatoba (Hymenaea courbaril) has been planed away on top, exposing the paler color of the raw wood underneath.

Is it weathered or have a patina?

Many woods, when left outside in the elements, tend to turn a bland gray color. Also, even interior wood also takes on a patina as it ages: some woods get darker, or redder, and some even get lighter or lose their color; but for the most part, wood tends to darken with age.

Fresh sanding near the end of this Osage Orange (Maclura pomifera) board has exposed the characteristic yellow coloration of the wood, which has a strong tendency to shift down to a golden brown over time.

Is it possible to sand or plane the board to see the natural raw color of the wood?

The most predictable baseline to use when identifying wood is in a freshly sanded state. This eliminates the chances of a stain or natural aging skewing the color diagnosis of the wood.

3. Observe the wood grain.

If the wood is unfinished, then look at the texture of the grain. Ask yourself these questions:

Does the wood have an open, porous texture?

Most softwoods will be almost perfectly smooth with no grain indentations, while many common hardwoods have an open pore structure, such as oak or mahogany; though there are some hardwoods that are also smooth to the touch, such as maple.

Can you tell if the wood is quartersawn or plainsawn?

By observing the grain patterns, many times you can tell how the board was cut from the tree. Some wood species have dramatically different grain patterns from plainsawn to quartersawn surfaces. For instance, on their quartersawn surfaces, lacewood has large lace patterns, oak has flecks, and maple has the characteristic “butcher block” appearance.

Is there any figure or unusual characteristics, such as sapwood, curly or wild grain, burl/knots, etc.?

Some species of wood have figure that is much more common than in other species: for example, curly figure is fairly common in soft maple, and the curls are usually well-pronounced and close together. Yet when birch or cherry has a curly grain, it is more often much less pronounced, and the curls are spaced farther apart.

Curly Maple (sealed)
The strong, tight curl seen in this wood sample is very characteristic of Maple (Acer spp.).

4. Consider the weight and hardness of the wood.

If it’s possible, pick the piece of wood up and get a sense of its weight, and compare it to other known wood species. Try gouging the edge with your fingernail to get a sense of its hardness. If you have a scale, you can take measurements of the length, width, and thickness of the wood, and combine them to find the density of the wood. This can be helpful to compare to other density readings found in the database. When examining the wood in question, compare it to other known wood species, and ask yourself these questions:

Is the wood dry?

Wood from freshly felled trees, or wood that has been stored in an extremely humid environment will have very high moisture contents. In some freshly sawn pieces, moisture could account for over half of the wood’s total weight! Likewise, wood that has been stored in extremely dry conditions of less than 25% relative humidity will most likely feel lighter than average.

How does the wood’s weight compare to other species?

Taking into account the size of the board, how does its weight compare to other benchmark woods? Is it heavier than oak? Is it lighter than pine? Look at the weight numbers for a few wood species that are close to yours, and get a ballpark estimate of its weight.

A piece of Lignum Vitae is weighed on a small digital scale.

How hard is the wood? 

Obviously softwoods will tend to be softer than hardwoods, but try to get a sense of how it compares to other known woods. Density and hardness are closely related, so if the wood is heavy, it will most likely be hard too. If the wood is a part of a finished item that you can’t adequately weigh, you might be able to test the hardness by gouging it in an inconspicuous area. Also, if it is used in a piece of furniture, such as a tabletop, a general idea of its hardness can be assessed by the number and depth of the gouges/dings in the piece given its age and use. A tabletop made of pine will have much deeper dents than a tabletop made of Oak. Additionally, you can always try the “fingernail test” as a rough hardness indicator:  find a crisp edge of the wood, and with your fingernail try to push in as hard as you can and see if you’re able to make a dent in the wood.

5. Consider its history.

Many times we forget common sense and logic when attempting to identify wood. If you’ve got a piece of Amish furniture from Pennsylvania, chances are more likely that the wood  will be made of something like black walnut or cherry, and not African wenge or jatoba. You might call it “wood profiling,” but sometimes it can pay to be a little prejudiced when it comes to wood identification. Some common-sense questions to ask yourself when trying to identify a piece of wood:

Where did it come from?

Knowing as much as you can about the source of the wood—even the smallest details—can be helpful. If the wood came from a wood pile or a lumber mill where all the pieces were from trees processed locally, then the potential species are immediately limited. If the wood came from a builder of antique furniture, or a boat-builder, or a trim carpenter: each of these occupations will tend to use certain species of woods much more often than others, making a logical guess much simpler.

Despite its discoloration and wear, it’s very likely that this rolling pin is made of hard maple.

How old is it?

As with the wood’s source, its age will also help in identification purposes. Not only will it help to determine if the wood should have developed a natural patina, but it will also suggest certain species which were more prevalent at different times in history. For instance, many acoustic guitars made before the 1990s have featured Brazilian rosewood backs/sides, yet due to CITES restrictions placed upon that species, East Indian rosewood became a much more common species on newer guitars. (And this is a continuing shift as newer replacements are sought for rosewoods altogether.)

How large is the piece of wood?

Some species of trees are typically very small—some are even considered shrubs—while others get quite large. For instance, if you see a large panel or section of wood that’s entirely black, chances are it’s either painted, dyed, or stained: Gaboon ebony and related species are typically very small and very expensive.

What is the wood’s intended use?

Simply knowing what the wood was intended for—when considered in conjunction with where it came from and how old it is—can give you many clues to help identify it. In some applications, certain wood species are used much more frequently than others, so that you can make an educated guess as to the species of the wood based upon the application where it was used. For instance, in the United States: many older houses with solid hardwood floors have commonly used either red oak or hard maple; many antique furniture pieces have featured quartersawn white oak; many violins have spruce tops; many closet items used aromatic red cedar, and so forth. While it’s not a 100% guarantee, “profiling” the wood in question will help reduce the number of possible suspects, and aid in deducing the correct species.

6. Find the X-Factor.

Sometimes, after all the normal characteristics of a sample have been considered, the identity of the wood in question is still not apparent. In these instances—particularly in situations where a sample has been narrowed down to only a few possible remaining choices—it’s sometimes helpful to bring in specialized tests and other narrower means of identification.

The following techniques and recommendations don’t necessarily have a wide application in initially sorting out wood species and eliminating large swaths of wood species, but will most likely be of use only as a final step in special identification circumstances.

Odor

Believe it or not, freshly machined wood can have a very identifiable scent. When your eyes and hands can’t quite get a definitive answer, sometimes your nose can. Assuming there is no stain, finish, or preservative on or in the wood, quickly sand, saw, or otherwise machine a section of the wood in question, and take a whiff of the aroma.

Although new scents can be very difficult to express in words, many times the scent of an unknown wood may be similar to other known scents. For instance, rosewoods (Dalbergia spp.) are so named for their characteristic odor that is reminiscent of roses. Although difficult to directly communicate, with enough firsthand experience scents can become a memorable and powerful means of wood identification.

Fluorescence

While certain woods can appear basically identical to one another under normal lighting conditions, when exposed to certain wavelengths—such as those found in blacklights—the wood will absorb and emit light in a different (visible) wavelength. This phenomenon is known as fluorescence, and certain woods can be distinguished by the presence or absence of their fluorescent qualities. See the article Fluorescence: A Secret Weapon in Wood Identification for more information.

Black Locust: fluorescence (under blacklight)
Black Locust (Robinia pseudoacacia) glows a bright yellow-green when placed under a blacklight.

Chemical Testing

There are only a small number of chemical tests regularly used on wood, most of which are very specialized and were developed to help distinguish easily confused species with one another. They work by detecting differences in the composition of heartwood extractives. A chemical substance (called a reagent) is usually dissolved in water and applied to the wood surface: the surface is then observed for any type of chemical reaction (and accompanying color change) that may occur. Two of the most useful are the tests that are meant to separate Red and White Oak, and Red and Hard Maple.

Heartwood Extractives Leachability

Sometimes a wood species will have heartwood extractives that will be readily leachable in water and capable of conspicuously tinting a solution of water a specific color. For instance, the heartwood extractives contained in osage orange (Maclura pomifera) contain a yellowish-brown dye that is soluble in water. (This can sometimes be observed anecdotally when the wood is glued with a water-based adhesive: the glue’s squeeze-out is an unusually vibrant yellow.)

In a simple water extract color test, wood shavings are mixed with water in a vial, test tube, or other suitably small container, and the color of the water is observed after a few minutes. If the heartwood extractives are leachable by water, then a corresponding color change should quickly occur.

In addition to osage orange (Maclura pomifera)merbau (Intsia spp.), and rengas (Gluta spp. and Melanorrhoea spp.) are also noted for their readily leachable heartwood extractives. Because this property is quite uncommon, it can serve to quickly differentiate these woods from other lookalikes.

7. Look at the endgrain.

Perhaps no other technique for accurate identification of wood is as helpful and conclusive as the magnified examination of the endgrain. Frequently, it brings the identification process from a mostly intuitive, unscientific process into a predictable, repeatable, and reliable procedure.

Looking at the endgrain with a magnifier shouldn’t be a mystifying or esoteric art. In many cases, it’s nearly as simple as examining small newsprint under a magnifying glass. There are three components necessary to reap the full benefits contained in the endgrain:

I. A prepared surface.

When working with wood in most capacities, it becomes quickly apparent that endgrain surfaces are not nearly as cooperative or as easily worked as face grain surfaces. However, in this case, it is absolutely critical that a clear and refined endgrain surface is obtained.

For a quick glance of a softwood sample, a very sharp knife or razor blade can be used to take a fresh slice from the endgrain. However, in many denser species, especially in tropical hardwoods, one of the best ways to obtain a clear endgrain view is through diligent sanding. It’s usually best to begin with a relatively smooth saw cut (as from a fine-toothed miter saw blade) and proceed through the grits, starting at around 100, and working up to at least 220 or 320 grit, preferably higher for the cleanest view.

II. The right magnifier.

It need not be expensive, but whatever tool is used to view the endgrain should have adequate magnifying power. In most instances, 10x magnification is ideal, however, anything within the range of 8 to 15x magnification should be suitable for endgrain viewing. (Standard magnifying glasses are typically in the range of 2 to 4x magnification.)

These stronger magnifiers, sometimes called loupes, usually have a smaller viewing area than standard magnifying glasses. Fancier models—with built in lights, or larger viewing surfaces—are available at a premium; but the most basic models are usually only a few dollars.

amazon-button
amazon-button

III. A trained eye.

The third element that constitutes a proper endgrain examination is simply knowing what to look for. In analyzing the patterns, colors, shapes, and spacing of the various anatomical features, there is a veritable storehouse of information within the endgrain—all waiting to be unlocked. Yet, if these elements have not been pointed out and learned, the array of features will simply seem like an unintelligible jumble. The discipline of recognizing anatomical endgrain features is not easily summed up in a few sentences or even a few paragraphs, but it is nonetheless critical to the identification process. To this end, an in-depth look should be given to the various categories, divisions, and elements that constitute endgrain wood identification on the macroscopic level. (In this regard, macroscopic denotes what can be seen with a low-powered, 10x hand lens—without the aid of a microscope—rather than simply what can be seen with the naked eye.) Because the anatomy between softwoods and hardwoods is so divergent, each will be considered and examined separately:

Still stumped?

If you have a mysterious piece of wood that you’d like identified, you’ve got a few options for next steps:

USDA’s Forest Products Laboratory

You can mail your physical wood samples to the Center for Wood Anatomy Research

Pros:

  • Free
  • Professional wood identification

Cons:

  • Only available to US citizens
  • Slow turnaround times (up to a month or more)
  • Limited to three IDs per year

See their Wood ID Factsheet for more info.

Alden Identification Service

You can mail your physical wood samples (even small sections taken from antiques) to Alden Identification Service.

Pros:

  • Professional wood identification
  • Faster turnaround times (ranging from a few days to a week or two)

Cons:

  • Paid service

See their ordering page for more info. (Note that Harry Alden has written several books while at USDA, including both Hardwoods and Softwoods of North America.)

Ask for help online

If the wood ID is merely a curiosity, or non-critical, you can post pictures of the wood in question.

Pros:

  • Free
  • No need to send physical samples

Cons:

  • Greatly limited by the quality of the pictures provided
  • Extra work usually required to get adequate clarity in photos

See article of Common US Hardwoods to help find the most commonly used woods.

Get the hard copy

wood-book-standupIf you’re interested in getting all that makes The Wood Database unique distilled into a single, real-world resource, there’s the book that’s based on the website—the Amazon.com best-seller, WOOD! Identifying and Using Hundreds of Woods Worldwide. It contains many of the most popular articles found on this website, as well as hundreds of wood profiles—laid out with the same clarity and convenience of the website—packaged in a shop-friendly hardcover book.
Subscribe
Notify of
guest
4.2K Comments
Inline Feedbacks
View all comments
Paul Glanville

Hello. I have a burl that I got from a store 10+ years ago. There was no identification with it. It does have “MA 8.5” written on one face. I am pretty sure it is NOT MAple. I will try attaching some images. It is quite hard and heavy. Some of the pictures are raw wood, sanded, and some have light coat of semi-gloss Deft lacquer. I see only 3 pics are allowed. I have more if needed. Thanks.

IMG_1184.jpg
IMG_1190.jpg
IMG_1195.jpg
Brad

Hi Eric,

Can you tell what type of wood this table is. Bought at thrift store on west coast and is very heavy.

ED5B2500-C7AE-40E3-9E82-F66A4360EFDD.jpeg
5ABE75D9-6160-4075-94A9-52047550B07F.jpeg
Brad

Ok thank you! It is very hard also ..can’t get finger nail into it at all.

A73E9CBB-F601-4390-82C8-A8BD915E047E.jpeg
Suzanne

Hi Eric, I am refinishing an antique side table and trying to identify the wood. Seems like walnut or cherry but perhaps mahogany. Table is heavy; it had a dark stain on it which I am still working to remove on the top. Wood seems to have a red hue to it on drawers. Attached is top and a drawer. Thanks for any insights.

IMG_1860.jpg
IMG_1863.jpg
Don Johnson

Hello Eric,
Got the Crown molding from grandfather after years of him saving in the garage.
Wanted to know what type of wood material it is, looks like pine but If you could confirm it would be greatly appreciated. Some crown in 10ft 121″ pieces, 41/4″ wide, some Knotts in the wood. Your knowledge is greatly appreciated.
Thank you for your time, Take care.

1601078864296141361098.jpg
Dean Douglas

I am looking for help in identifying this wood.

20200923_111336.jpg
Dean

Some background, this is in a century old house in Pasadena, Ca. The wood is used in this cabinet as well as extensively as moldings and wainscoting in the dining room, its has an orange-y tone to it. I will get a closer image of the grain.

Dean

Here is a sanded sample. When “wet” orange color is predominant.
Unfortunately, I didn’t get the chance to smell this when it was being sanded.

Last edited 5 years ago by Dean
Dean

technical trouble!

20201001_121112.jpg
Dean

Could this be plain sawn KOA?

Dean Douglas

We determined that this piece was actually American Red Gum a species of liquidamber from the Southern states.

Megan

Removing a mismatched stain and thought I’d better identify the wood before staining again. I would love your help! Thanks!

27FF9833-DE93-4EA9-B2B4-EB6B588B0504.jpeg
5393DCC4-113E-4CC2-B3D8-A2E98CEB4D90.jpeg
1784B5C9-509C-45DC-A898-306CFBA80865.jpeg
Emily

Hi Eric, I sanded down the wood on a 65+ year old dresser that I got in Southern California. Before it was sanded, you said it may have been ash wood. Is that still what you think it is? Sorry about the shade.

1-1.jpg
Jeffrey Sloe

Hi Eric,

Im renovating an old home (built in 1925). I’m trying to determine what type of wood is being used for wrapping the arch opening. I added a second arch opening and would like to use the same type of wood.
Thanks.
Jeff

image.jpg
image.jpg
Jeffrey L Sloe

Hi Eric,
you are correct about the finish. Most of the trim has the same issue. I’m planning on sanding and refinishing the trim. Is there a better way to identify the wood type? Would a better pic work?
thank you
Jeff

Ralph

Hi Eric. Sorry to bother you again. Last time I promise. Could you please identify these 3 peices of wood please? Many thanks.

20200924_105540.jpg
20200924_105558.jpg
20200924_105735.jpg
Ralph

Hi Eric. As requested

20200924_132434.jpg
Ralph

Darker peice.

16010334374208068487281790680784.jpg
Ralph

Thanks Eric. When I get round to turning something with it, I’ll get some better grain photos.

Kelly Schoenhofen

I am trying to salvage this very old door; I have citrus-stripped it twice, cleaned it once with mineral spirits, any idea what kind of wood this is?

PXL_20200923_164018472.jpg
Kelly Schoenhofen

I’m in Minnesota but this door came from a series of salvage/reclamation places, so I have no idea of the origin. The hardware on the door was a lock & solid bronze knobs made in 1900 in a foundry in New Britain Connecticut.
I’ll get a shot of the end grain, I’m thinking I need to sand it down a bit on the ends (because they are pretty destroyed) and that may help tell me if it’s a veneer over another piece of wood or what.

Alejandra Martins

Hi Eric-

Looking to stain the wood in my kitchen darker. Thought I was doing it correctly but now am thinking I maybe be wrong. Any help? The house was built in 1920.

image.jpg
image.jpg
Egle

This is the wood in the house I am staying in. I was told it’s oak.

92A17609-3B52-437A-B610-4735219C08F2.jpeg
A4E2B30F-E5DC-487F-8CDA-12C81CACC346.jpeg
Egle

Thank you!

Maxine Cassidy

We have a very dark stained mantel, I’ve been sanding it back so I can restain it much lighter but need to know what it is to make sure I use the right products

16008761299697323425673183556810.jpg
Ellen

Hi. I was given this matched pair of mid century chairs. They have been outside for over a year here in Calgary. One seems to be raw now and I think a type of teak and the other though structurally, exactly the same, is light and have some kind of finish on part of it. When I sand, the light one stays light and in places a bit rosy colored. The dark one is rich and dark and when wet even darker. Two cuts or types of teak like wood. They are not exceptionally heavy and with the fingernail test… Read more »

20200921_200444.jpg
20200922_172025.jpg
20200922_172056.jpg
Ellen

Hi Eric and thank you so much. Attached are some more clear close up photos. As I mentioned, the chairs are identical in every way. It just seems they are different woods but they may not be. I’ll value your opinion. The first 3 are of the more blonde chair and the last two are close ups of the darker chair that has no finish left on it except a

Ellen

The photos didn’t post. Here are 3 of the lighter chair.

20200923_083551.jpg
20200923_083603.jpg
20200923_083608.jpg
Ellen

Thank you Eric. Yes, the chair is getting weathered and has some dark streaks in the grain that look like mold or mildew.

Ellen

And three of the darker chair that seems to have no finish left on it. You can see in the first photos that it looks darker where the cushion sat when the chair was left outside. My neighbours had these sitting behind their garage and I asked for them.

20200922_172025.jpg
20200923_083654.jpg
20200923_083701.jpg
Ellen

Thank you so much Eric for all you do. I agree and wondered upon closer inspection if it was a type of mahogany. How odd that two identical chairs should be such different woods.

Alex

I have engineered flooring with a very dark finish on what looks like much lighter wood. Do you know what the wood could actually be? Would like to try and get it refinished

Floor.jpg
Laurie

This is a butcher block type table bought in Germany in early 2000’s. I’d love to refinish it.

E8628DAD-E62D-4FF7-A42A-174A04AB8392.jpeg
Laurie

Thanks so much!

Marybeth

I got this piece of wood at a craft store I want to make a Cutting board out of it but I’m not sure if it’s hard enough to do that or what type of wood it is can anyone please help?

1519F7DB-18BF-45C6-AE82-276B7CFF1F20.jpeg
Velma

Can you help identify this wood so I can have more cabinets made

20200916_110154.jpg
20200916_110235.jpg
John

Hi, I picked up some bits of this wood from a local timber yard, in North Queensland, Australia. I haven’t been able to identify what it is, as I’m new to woodworking, and the yard owner wasn’t sure, as he had just bought the yard and was still figuring out what was there. I’ve done some work on a bit, and it has an almost shimmering effect in the right light (couldn’t get it on camera), it’s quite hard and has a distinct scent, especially when I plane it. The bits I got still had a much lighter sapwood still… Read more »

Screenshot_20200916-182412_Gallery.jpg
Screenshot_20200916-182339_Gallery.jpg
Screenshot_20200916-182315_Gallery.jpg
Davy Boy

Looks like laburnum. This is a small tree though, so the planks you have would have to have come from a large specimen. If it is laburnum, take great care maching and handling it as all parts of the tree are poisonous.

John

Having looked at a few pictures on google, I think you may be right. Good thing I hadn’t gotten around to working it too heavily yet. The only thing that sounds off is that I saw it described as having no characteristic odour, when the bits I’ve been working with definitely have a very specific, pleasant scent when worked. Either way, I’ll take more care with it from now on. Thanks.

Elijah

I’m trying to identify some veneer from a mid-century looking piece. Photos include one with finish on, one of the inner side which does not look finished and one with finish scraped off.

IMG_8340.jpg
IMG_8335.jpg
IMG_8339.jpg
ann

Hello! I think this is Douglas Fir but am not 100% certain – would love an expert’s confirmation! Thank you!

teredo.jpg
Amn

Thank you Eric!

Lisa

Help please, looking to buy a house that has this wood EVERYWHERE, doors, baseboards, door jams etc, love the wood not the color. Can you tell what wood it is and can i restain it a different color?

1.jpg
2.jpg
3.jpg
Stefan

was used for a humidor, was told it was spanish red cedar but I’m questioning the authenticity of that. Picture is all i have to go off of.

20200914_070811.jpg
Last edited 5 years ago by Stefan
Trevor Allen

I was wondering if you can confirm what type of wood this is. I used it as a test piece for my home built CNC but I have no idea what the wood is. I thought it might be ambrosia maple. I received the wood from a local pipe supplier as scrap lumber from their shipments. I am in Canada (Saskatchewan).

7BD9AA21-7085-49FA-A5A7-AA9B2197A416.jpeg
Trevor Allen

Hi. I live in Canada (Saskatchewan). However I got some dunage hardwood from a company the brings in pipes. So I don’t know where this wood would have come from. Most of the wood has been maple and white oak however I just milled some of the boards and this wood seems different. The reddish hue is throwing me off on what it might be. I though maybe cherry. Hopefully you can assist.

FB4F9459-AFEF-4CCB-B32E-57E4B88FBBBB.jpeg
29A12BDE-6DCC-4BE7-A4D8-1846BA474383.jpeg
1B48A454-3224-49EB-9D14-CE74517395D0.jpeg
Trevor Allen

Hopefully these ones are better.

312E02AD-B8C6-444E-9E6E-18CCD3023D69.jpeg
6E7999E9-AEE5-4E90-A3D7-54D576A6BDB6.jpeg
Liz Rivera

You’re a good egg, Eric Meier! You have provided more than 2,000 people with answers to their most challenging wood-related questions!! To me, that’s an amazing feat. Hoping you can help me as well. Riverside, CA. Home built in 1956. Part of the “Sungold” series of tract homes. Many of which are right here in Riverside where just last week, the thermometer hit a staggering 117°! Miserable as Hell! Toss in a Global Pandemic, the biggest and most catastrophic and costly fire season on record. Just glad to be here. This is a drawer from the kitchen. From stripping via… Read more »

DSC_0051.JPG
DSC_0042.JPG
DSC_0040.JPG
James

Hi, an 1870’s American clock case I’m guessing walnut? Heavily stained unfortunately. I cleaned the spot of shellac for a cleare grain view. Not positive of the crown mounding though.

09C7FE90-C668-494E-9FB7-E86A32866A09.jpeg
D65C5BA8-6493-404C-842B-19BD232546E4.jpeg
24A0EFDE-C209-413C-950D-7ED1C8F411EF.jpeg
Ray

Great article! I’m a newbie and am trying to educate myself a bit more on wood in general. What do you think this is? It’s the top of a piece I’m in the process of refinishing.

08206750-3BEA-4C82-AD93-7250D5AB55D4.jpeg
OLIVIA

Any idea what type of wood this is? Looking to make some fixes to a water stain!

IMG_6365.jpg
Senja

hi
could you please identify this. I have four pieces and each is around 59.2 lbs/ cubic foot

unknown end.JPG
unknown face.JPG
Senja

im in North Vietnam

Ed B

Hi Eric and thank you for all this information. I am trying to identify the wood type of my wainscoting from my home in Pennsylvania. Any ideas? It is an older house built in 1860s, though I can’t be sure how old the wood is.

Ralph

Hi.

Found this wood in my late fathers workshop. The white wood is very hard and heavy. Looks like sycamore and maple. Its just too hard to be either of those I think. The two peices are the same wood. Just one half is turned. No distinct smell to the wood. Really bad end grain tear out on the bowl.

I presume Eric will reply so thank you very much Eric.

15996665953446612414647517358780.jpg
15996671225331539591329507364795.jpg
15996671644854620483869206115157.jpg
Ralph

Hi Eric.
Apologies for the European measurement, but the density is 853kg/m3. Which isn’t sycamore or hard maple.

Ralph

Hi Eric.
I found it at the back of my fathers workshop in West Wales, so its probably been in there for about 30 years. He was a cabinet maker so he has lots of peices of hardwood scattered around and could be anything. Its very dry.
Could it be satinwood or yellowheart? Were they readily available decades ago?
Your doing a very good job here Eric. Well done.

Ralph

Thank you very much Eric. Your time is much appreciated.

Lenea Green

Hi! Just purchased this old trestle table and was told (not with much confidence though) that it’s from the 1940s. I’m thinking maybe alder but would love to know your opinion. Photos are once the finish was stripped.

2993F097-6B87-439D-AF8F-5B6CC81BD33A.jpeg
C6F07552-AF48-4F9C-A0DB-1AB793EDAAD2.jpeg
B121E300-88AA-43A3-BAC9-82282D6D45D6.jpeg
Laura

Hi Eric,

My boss bought some property and it had huge beams of this wood. It’s very hard and dense and it kind of stinks. Any ideas?

IMG_20200908_151829836.jpg
IMG_20200908_151758362.jpg
IMG_20200908_151811201.jpg
Cathy

Hi Eric! I can’t find anyone who can tell me what kind of wood this antique bed is made of. Can you help? And, no, the grain is not painted on. Thanks!

70FD5A7C-0D1E-4EEA-A036-89FDD3AF763D.jpeg
B7DFC8ED-F7B0-438E-8520-B1425C01B980.jpeg
Jon

Hello,
what kind of wood is this?

teak.jpg
John Morphis

Hi Eric, I have a home in Buffalo NY built in 1911. The sheathing and framing were done in a rough cut lumber that I assume is a type of spf but want to know if it has any treatment to it, since it has a red tint to it and I cannot seem to match it to anything. There is scrap wood around and if it has any type of treatment I won’t use it, if it’s fine I’d love to use it. It seems like a soft wood but has more toughness and “meat” than any softs I… Read more »

John Morphis

The last pic is the best shot of the end grain I could get.

A1729AAB-4F65-4BDA-A2F9-AC02CF4A42F1.jpeg
8384E807-C3F6-4AC4-9F28-9E7BAA3DC4FC.jpeg
53330751-910B-4B46-B73C-EC2C427C22DC.jpeg
Lianne Hanson

what wood would you say this is? I thought Acacia but someone else said Dalbergia Sissoo?

20200905_160252.jpg
20200907_161606.jpg
Cora Skylark

Hello Eric, could you please help identify these two types of veneer. The lighter one has very ‘orange-y’ tint to it which I’d like to sand down and make it look more natural. The middle is a darker one which I think I will need to replace as the knots (the dot like looking at the bottom) are peeling off. I’m in the UK and I’ve seen lots of older furniture of this type so must have been a trend at some point. I’d greatly appreciate your help. Cora

IMG_20200907_130700.jpg
Larry Zarra

Hi Eric, I hope you can help ID this wood I got from a local tree trimmer. Location is Spring, Texas, just north of Houston. Bark is about 1/8 inch thick. Sapwood is 1/2 inch thick, and is essentially white. Heartwood is light brown to olive green hued with hints of dark mustard color. I am uploading a photomicrograph of the endgrain (not sure if image actually uploaded). Thank you, Larry

Norman Lucia

please help me identify this piece of wood ,it is stumping me ,i live and acquired this wood in florida it was already milled ,i dont remember where i got it, it was in with my other woods from years ago when i was working with wood alot. it is hard and dense ,i cant make out the odor i think it might be in the hickory family , thanks in advance, Sincerely , Norman

face sanded heavy as oak very hard.jpg
endgrain of sample.jpg
edna Hanson

Please identify if possible. Possibly from India. Thank you

20200905_164158.jpg
Edna Hanson

Ok,ty. It’s a hard wood if that helps. Did the fingernail test.

Arun

Hello,
My previous comment did not attach pic
Need help with identifying all 3 wood and colors
I have refinish them

B2D2E66A-4A56-4963-9853-703576F93E5F.jpeg
DFB8AE29-7A95-41E8-A1DD-CC5BA9F9F741.jpeg
C696841C-FFD5-474B-8352-4C346556344B.jpeg
Arin

Hello,
I have to refinish my furniture but I don’t know why color/types could you help

Rich

Hi Eric. could you identify these for me? I got then in China, Yunnan province

woodB1.JPG
woodB2.JPG
woodC1.JPG
Rich

Ok thanks. how about these pieces?

IMG_7594.JPG
IMG_9591.JPG
IMG_0754.JPG
Nathan Helfman

Wood being orthotropic, could you clarify how Wood Database mechanical properties bare derived? For example, from which set of axes is the modulus of elasticity derived?

NATHAN HELFMAN

Hi Eric,
Thanks for getting back. I’ll explain the source of my question. The book published by the US Department of Agriculture, “Wood Handbook, Wood as an Engineering Material” publishes the value of the Modulus of Elasticity for Black Walnut as 11,600 MPa, which agrees most perfectly with “The Wood Database” value of 11.59 GPa. However, at the bottom of 5-8 (Chapter 5, pg. 8), footnote “c” states, “Modulus of elasticity measured from a simply supported, center-loaded beam, on a span depth ratio of 14/1.” Center loaded, that is to say, a radial load, and not longitudinal. Confusing.

Lee

Ok, my turn! Was given several peices of wood that came from central and south america 20+ years ago. I think the bulk of it is brazilian cherry. There are a couple darker peices as well and at least one snakewood peice. First two pics guessing are the brazilian cherry. Not sure on third pic. Will add end grain in next post.

15991451914873560249310057797344.jpg
15991452470307988326243476024234.jpg
15991453592476158916463933345126.jpg
Lee

Here is an end grain of the second. Almost looks like purple heart… Wondering if they made a mistake on this one’s origin.

15992354238593458761405403084466.jpg
Julia Barling

I was recently given this unit, which I had just presumed was pine but after stripping it off I am not so sure. Could you please tell me what it is?

AA5ED745-1DD3-4353-B3F8-2DCDD031803F.jpeg
Julia Barling

Thanks for your reply Eric, the type of wood it is has totally baffled us! I’ve attached another picture as requested and the piece was purchased from an Eastern European lady in Dubai, so I’m afraid that probably isn’t much help as furniture from every corner of the world here!

96695FF8-9049-405F-91B8-C87AEDBCA6D1.jpeg
B663A7ED-99A5-4F15-933F-84749B85BDD3.jpeg
Julia Barling

Thank you so much!!! ?

Elec

This peice of wood came from my dad. I remember him telling me about it and it was from a tree you could no longer harvest. I cant remember the name and cant be sure this is it but it weighs a ton this peice weighs about 15 pounds. Im afraid to do much to it in case it is a rare find

15990986085341657677076462154821.jpg
15990986297203870070306480489438.jpg
1599098659041704029801590942240.jpg
Elec

Unfortunately i have no way of knowing where it was harvested. I did sand it and there was no real distinctive smell to it. Just smelled like sanded wood.

Dee

Hello Eric, I bought a house that had a few rough sawn boards in the garage. Any idea what kind of wood this might be?

20200829_143032.jpg
20200829_143105.jpg
1 21 22 23 24 25 41