Wood Identification Guide

Wood Identification Guide

by Eric Meier

When attempting to identify a wood sample, it’s important to keep in mind the limitations and obstacles that are present in our task. Before starting, please have a look at The Truth Behind Wood Identification to approach the task in a proper mindset; I consider the linked article to be required reading for all those visiting my site with the intent of identifying wood.

1. Confirm it is actually solid wood.

Before proceeding too much farther into the remaining steps, it’s first necessary to confirm that the material in question is actually a solid piece of wood, and not a man-made composite or piece of plastic made to imitate wood.

A solid piece of Cocobolo: note how the grain naturally wraps around the sides and endgrain of the wood.

Can you see the end-grain? 

Manufactured wood such as MDF, OSB, and particleboard all have a distinct look that is—in nearly all cases—easily distinguishable from the endgrain of real wood. Look for growth rings—formed by the yearly growth of a tree—which will be a dead-giveaway that the wood sample in question is a solid, genuine chunk of wood taken from a tree.

Viewing the end of this “board” reveals its true identity: particleboard.

Is it veneered? 

If you see a large panel that has a repeating grain pattern, it may be a veneer. In such cases, a very thin layer of real wood is peeled from a tree and attached to a substrate; sometimes the veneer can be one continuous repeating piece because it is rotary-sliced to shave off the veneer layer as the tree trunk is spun by machines. Assuming it is a real wood veneer with a distinct grain and texture—and not merely a piece of printed plastic—you may still be able to identify the outer veneer wood in question, but you should still realize that is it only a veneer and not a solid piece of wood.

Large repeating patterns suggest a veneer.

Is it painted or printed to look like wood? 

Many times, especially on medium to large-sized flat panels for furniture, a piece of particleboard or MDF is either laminated with a piece of wood-colored plastic, or simply painted to look like wood grain. Many of today’s interior hardwood flooring planks are good examples of these pseudo-wood products: they are essentially a man-made material made of sawdust, glues, resins, and durable plastics.

2. Look at the color.

Some questions to immediately ask yourself:

Is the color of the wood natural, or is it stained?

If there is even a chance that the color isn’t natural, the odds are increased that the entire effort of identifying the wood will be in vain.

The reddish brown stain used on this piece of Jatoba (Hymenaea courbaril) has been planed away on top, exposing the paler color of the raw wood underneath.

Is it weathered or have a patina?

Many woods, when left outside in the elements, tend to turn a bland gray color. Also, even interior wood also takes on a patina as it ages: some woods get darker, or redder, and some even get lighter or lose their color; but for the most part, wood tends to darken with age.

Fresh sanding near the end of this Osage Orange (Maclura pomifera) board has exposed the characteristic yellow coloration of the wood, which has a strong tendency to shift down to a golden brown over time.

Is it possible to sand or plane the board to see the natural raw color of the wood?

The most predictable baseline to use when identifying wood is in a freshly sanded state. This eliminates the chances of a stain or natural aging skewing the color diagnosis of the wood.

3. Observe the wood grain.

If the wood is unfinished, then look at the texture of the grain. Ask yourself these questions:

Does the wood have an open, porous texture?

Most softwoods will be almost perfectly smooth with no grain indentations, while many common hardwoods have an open pore structure, such as oak or mahogany; though there are some hardwoods that are also smooth to the touch, such as maple.

Can you tell if the wood is quartersawn or plainsawn?

By observing the grain patterns, many times you can tell how the board was cut from the tree. Some wood species have dramatically different grain patterns from plainsawn to quartersawn surfaces. For instance, on their quartersawn surfaces, lacewood has large lace patterns, oak has flecks, and maple has the characteristic “butcher block” appearance.

Is there any figure or unusual characteristics, such as sapwood, curly or wild grain, burl/knots, etc.?

Some species of wood have figure that is much more common than in other species: for example, curly figure is fairly common in soft maple, and the curls are usually well-pronounced and close together. Yet when birch or cherry has a curly grain, it is more often much less pronounced, and the curls are spaced farther apart.

Curly Maple (sealed)
The strong, tight curl seen in this wood sample is very characteristic of Maple (Acer spp.).

4. Consider the weight and hardness of the wood.

If it’s possible, pick the piece of wood up and get a sense of its weight, and compare it to other known wood species. Try gouging the edge with your fingernail to get a sense of its hardness. If you have a scale, you can take measurements of the length, width, and thickness of the wood, and combine them to find the density of the wood. This can be helpful to compare to other density readings found in the database. When examining the wood in question, compare it to other known wood species, and ask yourself these questions:

Is the wood dry?

Wood from freshly felled trees, or wood that has been stored in an extremely humid environment will have very high moisture contents. In some freshly sawn pieces, moisture could account for over half of the wood’s total weight! Likewise, wood that has been stored in extremely dry conditions of less than 25% relative humidity will most likely feel lighter than average.

How does the wood’s weight compare to other species?

Taking into account the size of the board, how does its weight compare to other benchmark woods? Is it heavier than oak? Is it lighter than pine? Look at the weight numbers for a few wood species that are close to yours, and get a ballpark estimate of its weight.

A piece of Lignum Vitae is weighed on a small digital scale.

How hard is the wood? 

Obviously softwoods will tend to be softer than hardwoods, but try to get a sense of how it compares to other known woods. Density and hardness are closely related, so if the wood is heavy, it will most likely be hard too. If the wood is a part of a finished item that you can’t adequately weigh, you might be able to test the hardness by gouging it in an inconspicuous area. Also, if it is used in a piece of furniture, such as a tabletop, a general idea of its hardness can be assessed by the number and depth of the gouges/dings in the piece given its age and use. A tabletop made of pine will have much deeper dents than a tabletop made of Oak. Additionally, you can always try the “fingernail test” as a rough hardness indicator:  find a crisp edge of the wood, and with your fingernail try to push in as hard as you can and see if you’re able to make a dent in the wood.

5. Consider its history.

Many times we forget common sense and logic when attempting to identify wood. If you’ve got a piece of Amish furniture from Pennsylvania, chances are more likely that the wood  will be made of something like black walnut or cherry, and not African wenge or jatoba. You might call it “wood profiling,” but sometimes it can pay to be a little prejudiced when it comes to wood identification. Some common-sense questions to ask yourself when trying to identify a piece of wood:

Where did it come from?

Knowing as much as you can about the source of the wood—even the smallest details—can be helpful. If the wood came from a wood pile or a lumber mill where all the pieces were from trees processed locally, then the potential species are immediately limited. If the wood came from a builder of antique furniture, or a boat-builder, or a trim carpenter: each of these occupations will tend to use certain species of woods much more often than others, making a logical guess much simpler.

Despite its discoloration and wear, it’s very likely that this rolling pin is made of hard maple.

How old is it?

As with the wood’s source, its age will also help in identification purposes. Not only will it help to determine if the wood should have developed a natural patina, but it will also suggest certain species which were more prevalent at different times in history. For instance, many acoustic guitars made before the 1990s have featured Brazilian rosewood backs/sides, yet due to CITES restrictions placed upon that species, East Indian rosewood became a much more common species on newer guitars. (And this is a continuing shift as newer replacements are sought for rosewoods altogether.)

How large is the piece of wood?

Some species of trees are typically very small—some are even considered shrubs—while others get quite large. For instance, if you see a large panel or section of wood that’s entirely black, chances are it’s either painted, dyed, or stained: Gaboon ebony and related species are typically very small and very expensive.

What is the wood’s intended use?

Simply knowing what the wood was intended for—when considered in conjunction with where it came from and how old it is—can give you many clues to help identify it. In some applications, certain wood species are used much more frequently than others, so that you can make an educated guess as to the species of the wood based upon the application where it was used. For instance, in the United States: many older houses with solid hardwood floors have commonly used either red oak or hard maple; many antique furniture pieces have featured quartersawn white oak; many violins have spruce tops; many closet items used aromatic red cedar, and so forth. While it’s not a 100% guarantee, “profiling” the wood in question will help reduce the number of possible suspects, and aid in deducing the correct species.

6. Find the X-Factor.

Sometimes, after all the normal characteristics of a sample have been considered, the identity of the wood in question is still not apparent. In these instances—particularly in situations where a sample has been narrowed down to only a few possible remaining choices—it’s sometimes helpful to bring in specialized tests and other narrower means of identification.

The following techniques and recommendations don’t necessarily have a wide application in initially sorting out wood species and eliminating large swaths of wood species, but will most likely be of use only as a final step in special identification circumstances.

Odor

Believe it or not, freshly machined wood can have a very identifiable scent. When your eyes and hands can’t quite get a definitive answer, sometimes your nose can. Assuming there is no stain, finish, or preservative on or in the wood, quickly sand, saw, or otherwise machine a section of the wood in question, and take a whiff of the aroma.

Although new scents can be very difficult to express in words, many times the scent of an unknown wood may be similar to other known scents. For instance, rosewoods (Dalbergia spp.) are so named for their characteristic odor that is reminiscent of roses. Although difficult to directly communicate, with enough firsthand experience scents can become a memorable and powerful means of wood identification.

Fluorescence

While certain woods can appear basically identical to one another under normal lighting conditions, when exposed to certain wavelengths—such as those found in blacklights—the wood will absorb and emit light in a different (visible) wavelength. This phenomenon is known as fluorescence, and certain woods can be distinguished by the presence or absence of their fluorescent qualities. See the article Fluorescence: A Secret Weapon in Wood Identification for more information.

Black Locust: fluorescence (under blacklight)
Black Locust (Robinia pseudoacacia) glows a bright yellow-green when placed under a blacklight.

Chemical Testing

There are only a small number of chemical tests regularly used on wood, most of which are very specialized and were developed to help distinguish easily confused species with one another. They work by detecting differences in the composition of heartwood extractives. A chemical substance (called a reagent) is usually dissolved in water and applied to the wood surface: the surface is then observed for any type of chemical reaction (and accompanying color change) that may occur. Two of the most useful are the tests that are meant to separate Red and White Oak, and Red and Hard Maple.

Heartwood Extractives Leachability

Sometimes a wood species will have heartwood extractives that will be readily leachable in water and capable of conspicuously tinting a solution of water a specific color. For instance, the heartwood extractives contained in osage orange (Maclura pomifera) contain a yellowish-brown dye that is soluble in water. (This can sometimes be observed anecdotally when the wood is glued with a water-based adhesive: the glue’s squeeze-out is an unusually vibrant yellow.)

In a simple water extract color test, wood shavings are mixed with water in a vial, test tube, or other suitably small container, and the color of the water is observed after a few minutes. If the heartwood extractives are leachable by water, then a corresponding color change should quickly occur.

In addition to osage orange (Maclura pomifera)merbau (Intsia spp.), and rengas (Gluta spp. and Melanorrhoea spp.) are also noted for their readily leachable heartwood extractives. Because this property is quite uncommon, it can serve to quickly differentiate these woods from other lookalikes.

7. Look at the endgrain.

Perhaps no other technique for accurate identification of wood is as helpful and conclusive as the magnified examination of the endgrain. Frequently, it brings the identification process from a mostly intuitive, unscientific process into a predictable, repeatable, and reliable procedure.

Looking at the endgrain with a magnifier shouldn’t be a mystifying or esoteric art. In many cases, it’s nearly as simple as examining small newsprint under a magnifying glass. There are three components necessary to reap the full benefits contained in the endgrain:

I. A prepared surface.

When working with wood in most capacities, it becomes quickly apparent that endgrain surfaces are not nearly as cooperative or as easily worked as face grain surfaces. However, in this case, it is absolutely critical that a clear and refined endgrain surface is obtained.

For a quick glance of a softwood sample, a very sharp knife or razor blade can be used to take a fresh slice from the endgrain. However, in many denser species, especially in tropical hardwoods, one of the best ways to obtain a clear endgrain view is through diligent sanding. It’s usually best to begin with a relatively smooth saw cut (as from a fine-toothed miter saw blade) and proceed through the grits, starting at around 100, and working up to at least 220 or 320 grit, preferably higher for the cleanest view.

II. The right magnifier.

It need not be expensive, but whatever tool is used to view the endgrain should have adequate magnifying power. In most instances, 10x magnification is ideal, however, anything within the range of 8 to 15x magnification should be suitable for endgrain viewing. (Standard magnifying glasses are typically in the range of 2 to 4x magnification.)

These stronger magnifiers, sometimes called loupes, usually have a smaller viewing area than standard magnifying glasses. Fancier models—with built in lights, or larger viewing surfaces—are available at a premium; but the most basic models are usually only a few dollars.

amazon-button
amazon-button

III. A trained eye.

The third element that constitutes a proper endgrain examination is simply knowing what to look for. In analyzing the patterns, colors, shapes, and spacing of the various anatomical features, there is a veritable storehouse of information within the endgrain—all waiting to be unlocked. Yet, if these elements have not been pointed out and learned, the array of features will simply seem like an unintelligible jumble. The discipline of recognizing anatomical endgrain features is not easily summed up in a few sentences or even a few paragraphs, but it is nonetheless critical to the identification process. To this end, an in-depth look should be given to the various categories, divisions, and elements that constitute endgrain wood identification on the macroscopic level. (In this regard, macroscopic denotes what can be seen with a low-powered, 10x hand lens—without the aid of a microscope—rather than simply what can be seen with the naked eye.) Because the anatomy between softwoods and hardwoods is so divergent, each will be considered and examined separately:

Still stumped?

If you have a mysterious piece of wood that you’d like identified, you’ve got a few options for next steps:

USDA’s Forest Products Laboratory

You can mail your physical wood samples to the Center for Wood Anatomy Research

Pros:

  • Free
  • Professional wood identification

Cons:

  • Only available to US citizens
  • Slow turnaround times (up to a month or more)
  • Limited to three IDs per year

See their Wood ID Factsheet for more info.

Alden Identification Service

You can mail your physical wood samples (even small sections taken from antiques) to Alden Identification Service.

Pros:

  • Professional wood identification
  • Faster turnaround times (ranging from a few days to a week or two)

Cons:

  • Paid service

See their ordering page for more info. (Note that Harry Alden has written several books while at USDA, including both Hardwoods and Softwoods of North America.)

Ask for help online

If the wood ID is merely a curiosity, or non-critical, you can post pictures of the wood in question.

Pros:

  • Free
  • No need to send physical samples

Cons:

  • Greatly limited by the quality of the pictures provided
  • Extra work usually required to get adequate clarity in photos

See article of Common US Hardwoods to help find the most commonly used woods.

Get the hard copy

wood-book-standupIf you’re interested in getting all that makes The Wood Database unique distilled into a single, real-world resource, there’s the book that’s based on the website—the Amazon.com best-seller, WOOD! Identifying and Using Hundreds of Woods Worldwide. It contains many of the most popular articles found on this website, as well as hundreds of wood profiles—laid out with the same clarity and convenience of the website—packaged in a shop-friendly hardcover book.
Subscribe
Notify of
guest
4.2K Comments
Inline Feedbacks
View all comments
Ana

Hi, I just bought this kitchen table, I am planning to refinish it and I have no idea what type of wood this is. Can you help, thanks!

20200420_083013.jpg
20200420_090425.jpg
Kim

Hi there, am trying to identify the wood that has been used on the cladding of our home. Would very much appreciate your help and thanks!

WhatsApp Image 2020-04-20 at 12.20.15.jpeg
WhatsApp Image 2020-04-20 at 12.20.15 (1).jpeg
WhatsApp Image 2020-04-20 at 12.20.15 (2).jpeg
Paul

Please would you help me out on the following questions. thank you.
Bought this chair awhile ago could you tell me the kind of wood it is and roughly how old is it.
I want to paint or varnish it what do you recommend.
Is it classified as a, Vintage grandfathers armchair.
Thank you

DSCF0911.JPG
DSCF0913.JPG
DSCF0912.JPG
Laura

I planned an old pallet and got this pretty wood but no idea what it is… definitely not pine

Nathan

It might be cherry. Some pallets you can tell are a brighter red and usually a slightly thinner board

Jessica

Hi, can you help determine if this is red oak or white oak? The first pic is how it was, second is after it’s stripped and sanded. Thanks!!

Jessica

0DAAE402-C95F-4D72-996F-3B5109BCC3C5.jpeg
C3D17A9B-98C7-448C-8235-EE9CBA8BDA3C.jpeg
Travis Brown

Found this in my box of offcuts. For the life of me can’t remember what it is or where I got it some 20 years ago.

I thought it might be a cherry heartwood/sapwood cut. About same hardness, weight. Wider grain though. And slightly aromatic. But never have seen anything similar at my local supplier. All the cherry we get around here is pretty uniform red.

Any ideas?

IMG_5956.jpg
IMG_2806.jpg
IMG_8322.jpg
Travis Brown

Huh. I kept thinking possibly it was sort of like aromatic/Tennessee cedar, just seemed not as aromatic, harder, and brighter colours/contrast – more red, less brown than what I’m used to. Maybe it’s just tempered with age sitting in my box. Thank you kindly.

Kyle SODEN

Hi, what kind of wood is this?

Screenshot_20200412-122235_Gallery.jpg
Rob

This website is a wonderful resource of information! However I would like help in identifying some lumber I recently cleaned up and plan to use. I suspect it could be European Beech, as it came from Belgium ( I researched the stamp that was on it before jointing and planing ). Could anyone help identify?

wood.jpg
wood2.jpg
Greg Hart

I found a wood in my wood rack that I couldn’t identify. When working with it, it has a strong tar odour. It is heavier than other woods. Photos are attached. I am based in South Africa so I assume the wood may be an african wood

WhatsApp Image 2020-04-06 at 16.40.10 (2).jpeg
WhatsApp Image 2020-04-06 at 16.40.10 (1).jpeg
WhatsApp Image 2020-04-06 at 16.40.10.jpeg
Greg Hart

Eric, do you need more information to identify the wood?

Greg Hart

I hope these photos will help identify the wood

wood-end2.jpg
wood-flat2.jpeg.jpg
wood-side2.jpg
Greg

Thanks Eric. I will try some of the local exotic timber merchants locally

Greg

Eric, I shared the pictures with Cameron from rarewoods.co.za. He thinks it looks like Iroko. A North and West African hardwood

Jay Green

I could be mistaken but that looks to me like iron wood. Especially that you mentioned the tar like odour. I recently made a saloon style swing door from iron wood. It can charachterized by its dense weight, light, dark and reddish colouring, distinctive stinky/tar like smell and being really strenuous to work with yet delivers a great end product. Its one of my favourite woods. Will attach a image for you to refferance to yours. The timber in my image is freshly planed and the centre piece in the middle bottom is not iron wood, it balau which I… Read more »

20200108_123132.jpg
Mike

Thank you for this very helpful website. I am trying to identify the wood used in a couple of benches. I have not been able to identify the wood yet myself, but I am still early in the learning curve. Any clue what it might be from these images? I estimate the density of this wood at about 42-43 lbs/ft^3 (by weighing the wood portion and dividing that by the measured volume). Thank you for any help!

MysteryWood1.jpeg
MysteryWood2.jpeg
MysteryWood2.jpeg
Mike

Thank you for your feedback! I am learning about black walnut now – what I have read so far all seems consistent with this wood.

Deb Giugno

Your site looks like a fabulous source of information and I am trying to verify if this piece is truly teak. I did view the requirements on the site for the Center of Wood Anatomy but due to the age of the piece, I did not want to attempt to get the sample they need. The information that was provided to me on my purchase was that the divider was made in Thailand during the Vietnam war and shipped to the US as a family heirloom. It is very ornate with a few different shades of coloring supposedly due to… Read more »

Jeremy

Century old barnwood board ripped in half and noticed the sawn edge was dark green. Any clue what this wood species is?

20191220_165225.jpg
Richard

White oak or American Chestnut?

Amy Davis

Hey! This is very helpful, although I am completely stumped ( no pun intended) on what type of wood this is. I’m trying to redo our kitchen and I want These exact cabinets. Any clue? Thank you!

920CE5EE-A888-4DC3-B0FD-F99E7E0279E9.jpeg
Richard

Red oak is my guess also

Ted David

Thamk you for your great work in producing this website. It is quite a treasure. I am looking for wood to replace a broken piece from the base of a stairway. It is bent 180°, has a 1/2″ thickness and a bend diameter (OD) of 10″. I believe it is Oak, but am not sure what variety. I am also debating what method to use to bend its replacement. I am leaning toward kerf bending (there is a great guide on exactly how to do so on blocklayer.com) but I have also read about steaming and clamping. Of the thre… Read more »

20200316_130445.jpg
Myla

Hello, Thank you for the great info! We recently picked up an antique table and are in the process of refinishing. A friend thought it might be maple but I don’t recall ever seeing maple with grain this dark…we were leaning towards walnut?? Thanks so much for any insight you can offer!
Best regards, Myla

Table grain.jpg
Myla

Thanks so much, Eric. It’s a little challenging to grab different angels because we started refinishing the top and the underside of the table really gives the best idea of the untouched wood. Here’s a few more photos and the last one is of the top of the table that has been stripped. Not sure what kind of wood it is but we loooove it!! Thanks so much again for your help

44022BA4-2C57-452D-8901-F0971A70C68C.jpeg
Myla

2

1C4E5760-84D7-4633-9C7D-A07D161DA899.jpeg
Myla

3

5BEA2737-DEC9-457E-BC32-A6202DBD36BC.jpeg
Myla

Hi Eric, were you able to identify any additional details from the photos?

Claude

a variety of acacia

Myla

Thank you for the help Claude. We were guessing walnut but will definitely look up acacia. Thx again

Mike Battaglia

This is yellow pine (supposedly), but it also has some brown splotches. What are these splotches? It is only on one side of the wood, but it does seem to go beyond the surface. Could this be some kind of “spalting” or…?

guitarwood.jpg
Claude

yellow pine, or a hard pine variety

Emma

Hi can someone help me identify what wood this old church seat is, I have no knowledge at all about different wood types so I apologise now if it is a type that even I myself should no. Thank you

E570A73A-6A93-454B-85F9-7D8A22B83EDC.jpeg
4F52C2EF-4360-49B0-8E6D-4891D989B8D5.jpeg
Claude

looks like douglas fir

John

Can you please identify the species of this turned bowl, I recently bought from a thrift store? It is currently unsanded, unfinished. Looks like a kind of burl to me, but with all of the varieties of knots, curls, and what appears to be sapwood, I don’t have a clue. Please help? Thank-you.

IMG_1694a.jpg
IMG_1696a.jpg
IMG_1697a.jpg
Claude

beech

Apatrida

Olive tree

Mike

I am trying to identify this wood and am leaning towards Ipe or Rhodesian Teak…. Very hard and very dense wood. This is an old decking material that I have salvaged and will be re-purposing. The color keeps throwing me off in my searches. Pictures are through the process of me cleaning it up. Any knowledge or help would be appreciated!

Unknown Wood_Endgrain.jpg
Unknown Wood 1.jpg
Unknown Wood_Cleaned and wet.jpg
Mike

Thank you for your help! Certainly looks like this could be bulletwood

Claude

lacewood but the colour is not right

Mike

I did more research on the Massaranduba wood and think you were correct. Here’s another photo of the very same woof after I repurposed a small chunk of the wood. Thanks again for your help!

Bloodwood mallet 3.jpg
Tim

Can you identify this wood? 1 x 4 v-groove t&g on vaulted ceiling. (actual size 1/2″ x 3 1/2″). Light weight. Surface has clear finish. Very few knots. Probably installed 1990. Also, where could I buy more in Michigan?

wood ceiling 1.jpg
wood ceiling 2.jpg
wood ceiling 3.jpg
Tim

Eric, thanks for your evaluation. I researched further and thought it might be western red cedar. The board is very light, and feels softer than maple. Could this be an option?

Jessica

Can you help identify the wood of this table? It’s very solid and heavy. These are in various lighting.

BC283ADF-FD11-49DA-87D5-6A242EA53B57.jpeg
11B6C9EA-2EB7-4C26-B6EE-61A019B546CE.jpeg
BE33EB55-4CE1-45F4-87BA-8225D075AF01.jpeg
J Burch

Can someone help me identify this floor surface?

3.jpg
Claude

oak flooring

N Lalaian

Can you help me figure out what kind of wood my floors are? I’m guessing they’re pine boards but not sure. Also these custom-built cabinets I have in my home. Thanks!

30284197-B02A-461A-A671-BAF11F8E24CE.jpeg
B1F5E519-1112-4E56-A036-C803ED6A0E8E.jpeg
86D968C1-27F1-4CA7-B4FB-745BC7016890.jpeg
N L

Another photo of the floors:

E4F398A0-0754-47AB-BF08-E12D6FFA9CEC.jpeg
Zac C

Id say Douglas Fir with a shellac over it

Frank

Pine floors for sure. And the chest is oak

Claude

douglas fir

B R STURZL JR

Thanks! For such a comprehensive articl

20200302_191120.jpg
20200302_191115.jpg
Angelique

can you please assist and advise what tye of wood my table is?

woodtable.jpg
Henry

Thank you for the article, it was very helpful, but I am still having trouble. Which wood species would my cabinets fall under? I am in between some sort of oak or maple?

unnamed.jpg
IMG-3891 (1).jpg
unnamed (3).jpg
Claude

maple

Carol

Hi there…great article! Can you help me identify what type of wood my stairs are? I’m trying to match them so I can redo the stairs at the bottom that are currently stone. Thank you!!!

11288B69-9112-460A-9EED-D717ABCA2695.jpeg
Carol

Great! Thanks! Our house is a pine log cabin, so that is what we were thinking! Much appreciated!

Claude

white pine with finish

Chris

Please help. I’m trying to find out what my banister is made of so that I can get a window sill made of the same wood. It has been oiled with clear satin so appears slightly darker that the bare wood underneath. It is a hard wood but I’m unsure what it is. The house is 1930/40 in the southwest of UK.

image.jpg
image.jpg
image.jpg
Heidi Herzog

Very cool and interesting article! Can’t wait to try the fluorescent light trick. So the reason I’m visiting…I recently picked up a coffee table at a yard sale. It seemed obvious to me that whatever the wood, it was painted or manipulated somehow. When I got it home I saw this tag taped to the bottom. I’ve tried searching the ole Google, but I can’t seem to come up with anything. Any advice?

Heidi Herzog

Sorry, forgot the pics. Thanks!!

2A8B2F42-192F-42C2-8485-55AD5E7EBFDF.jpeg
B3C53758-208C-4EB8-9755-F2FFCA58EFED.jpeg
10FA213B-8EF3-4E54-97CA-F51B879C7DFE.jpeg
Claude

natural black walnut with surface finish

Mark

Hi again
Here are a few more photos of the mystery wood – please advise me if you need specific photos taken. The small piece in the foreground has a freshly planed surface on it, the piece in the round is freshly bandsawed across the end (my poor bandsaw).
Many thanks

20200219_190545.jpg
20200219_190633.jpg
20200219_190901.jpg
Mark

Hi Eric Thanks for this great article and for sharing your expertise so keenly. I’m a wood worker, I make celtic harps for a living and longbows for a hobby. I have recently inherited some old lumps of wood, and I am struggling to find a definitive identification and I was very much hoping you would be able to help me. I’m from the UK so I am not a US citizen, so I can’t use their service. Would you please take a look at the photos and see if you have any key knowledge that would help? I have… Read more »

20200219_190237.jpg
20200219_190423.jpg
20200219_190647.jpg
Martha

Hi there! Can anyone help me find out what kind of wood my coffee table is? Here are some pictures.
Thanks so much for your help!

IMG_3583.jpg
IMG_3576.jpg
john K Jordan

Eric, just a heads up. It looks like the Forest Products Laboratory has changed things up a bit, specifically it looks like they have reduced the number of samples they will process from 5 to 3 per year per household. Maybe someone had his wife and seven kids each send in 5 samples. From their current fact sheet: “The Center for Wood Anatomy Research will identify a maximum of 3 wood specimens per household per calendar year as a free public service to private U.S. citizens.” BTW, I still have that sample of Pink Flame from Iquitos Peru for your… Read more »

Abner Morales

hoping you can help me identify my desk, it used to feel like it had a thick clear coat that felt like glass but now its getting less shine and feels more dry. Im trying to see if i can get it to feel like glass again “thick and shiny” feeling.

WhatsApp Image 2020-02-05 at 7.23.00 AM (1).jpeg
WhatsApp Image 2020-02-05 at 7.23.00 AM.jpeg
WhatsApp Image 2020-02-05 at 7.23.00 AM (2).jpeg
ROBERT KEMP

I bought a couple of solid guitar bodies on ebay. They were listed as “polished maple”, but clearly are neither. `
They’re about as dense as balsa, and soft enough to be easily marked by my thumbnail. Fluorescing with my black light revealed nothing special. The close-up image is roughly 70X. There are many similar listings for “maple” bodies with this grain, although one with a similar grain was listed as “candlewood”.

IMG_20200203_202728 FHD.jpg
IMG_20200203_202814_crop.jpg
SingleShot0005.jpg
ROBERT KEMP

Thanks, Eric. Paulownia is very similar. I can’t believe how many hours I’ve spent on your site since I began this inquiry. (It’s been a delightful time-suck.) I’m gonna post one more photo (because it looks very cool!) that I didn’t even bother to look at yesterday (because I’d accidentally allowed my flash to go off while I was shining a black light on the piece). The light combo really brought out the grain and color in a way that black light alone didn’t.

IMG_20200203_205847 FHD sq.jpg
Sherman

Very informative article. I’m hoping you can help me identify what type of wood my chairs are made from. They are manufactured by Paoli, however I am not sure what type of wood it is. I am hoping to sell them and wanted to ensure I give the correct description.

arm01_edited.jpg
arm03_edited.jpg
arm02_edited.jpg
Matt Cotto

Hoping to identify my wood flooring. Approx 2in width and 1/4 depth, nailed in. Pictures of top side sanded down and a picture of the back side. Oak Maybe?

322BFE60-2AD7-4671-B811-6C82CA57D7EF.jpeg
3B6B339B-4F60-43F2-BA9E-E8DB90F31D40.jpeg
Edward Padget

I’m a pen turner. I recently bought some inventory and though most was marked I had six pieces that were not. I’ve looked through the database and I can’t figure it out. I’d appreciate any input thank you.

D2.jpg
D1A.jpg
Edward Padget

I’m a pen turner. I recently bought some inventory and though most was marked I had six pieces that were not. I’ve looked through the database and I can’t figure it out.

B2.jpg
C1.jpg
C2.jpg
Justin

Any chance the one in the middle maybe mesquite? Just asking because of the purple reddish color. Looks like some blanks I have milled from logs here in South Texas that I know where mesquite.

Edward Padget

I’m a pen turner. I recently bought some inventory and though most was marked I had six pieces that were not. I’ve looked through the database and I can’t figure it out.

A1.jpg
A2.jpg
B1.jpg
Holly

Hi Eric! Just wondered if you had any idea what this wood might be?

Screenshot_20200127-233642.jpg
Holly

Thanks Eric! Really very much appreciated. I’m getting good at this, it was my guess too :) thanks again for your help.

Joyce L Nevels

I just purchased this 100 year old handmade Irish table and before I try to do anything to it, would like to know what your opinion of this wood is. It is definitely handmade as the joints are obviously handmade. The wood is a yellowish wood, and resembles Oak, but it may be pine. Since pine takes stain differently than oak, I really need to find out exactly what it is. Thank you..

MYtable6.jpg
Mytable7.jpg
mytable9.jpg
shedfaerie

…… hi, is there any chance you could identify this wood for me……. it is very “hard”, marble like even!

100_4824.jpg
Alison

Hi… What type of wood is this? Yes, it’s stained. House is in eastern Long Island and was built in 1978. Looking to sand & refinish. Thanks in advance!

20171113_Couch copy.JPG
20171117_KitchenStools copy.JPG
Alison Amsterdam

Thank you Eric! I’m surprised and pleased as oak is strong!!!

kathleen tulevski

this is (poorly) sanded wood (probably varnished)….but really rough….the insides of the doors are unfinished. could you tell me what wood it is?

bookcase.jpeg
unfinished wood.jpeg
Sophie

Hi – I have gotten at least three different answers as to what kind of wood this cabinet is made of (pine, hickory, white oak), do you have any suggestions for how I can determine what this cabinet is made of? Thank you!

what kind of wood is this.jpg
wood close up.png
Doug

It is Hickory.

Sophie

Hi here are some more pictures of the grain, thank you.

IMG_0433.jpg
IMG_0428.jpg
IMG_0427.jpg
Sophie

One more…

IMG_0425.jpg
Payton Abernathy

Hi,

I have been searching online trying to determine what this is on the walls.

Thanks so much,
Payton

walls.JPG
Tina K.

Oak? Whatever it is it’s beautiful. Please don’t say that you are removing it!

Javi

Hello everyone,

I’m trying to have a local carpenter make a few boxes for me and would like a nautical theme. Could anyone tell me what type of would this is?

Thanks,

Javi

James

So that’s a traditional Carolina flare – probably a Jarret bay or similar. The sterns on a boat like that are traditionally teak or mahogany. They could even be mahogany plywood or a veneer over a marine plywood. In reality you could get any wood to look like this with stain, and with enough epoxy, sanding, and finishing, you could make it look like that. I’m a professional boat captain, and I’ve worked on a many many wood boats (YES, that boat above is WOOD. it’s epoxy over wood- but those boats are stick build, traditional frames and marine plywood,… Read more »

Andrew

Helleo again, I just realized this photo may have the clearest view of the grain, and the edge (above the clock dial) looks so different from the face of the same piece, that I’m concerned it’s a hint of inferior wood, even veneer as opposed to solid. But the grain around the clock dial seems pretty rich looking. Should I take that as good sign of mahogany? Tried reading your great article on African & S. American, but still perplexed. These photos only evidence I have. Any insights (even if unsure) so deeply appreciated! Thanks again, and sorry pushing so… Read more »

Andrew

Eric, you are amazing!!! Thank you!!! I can’t believe it! But I must, because, well, your passion and expertise as to wood being the extraordinary phenomenon they are, I have to accept this unbelievably amazing surprise! To say you made my day, an understatement! (Esp. after last time what I was hoping was mahogany you informed me was poplar!). It’s sinking in I managed to get a solid walnut clock, just unbelievable, as “poplar” is how these things often turn out. As to the trim on top, I must say I’m surprised that they’d use a lesser wood in that… Read more »

Andrew

Well, apologizing if I’m being a nuisance (I saw on some other comments you asked for another photo) — Just this last picture! Thank you a million if you can help!! Obviously I’m a bit curious about the burl also (is it from random tree or identifiable?). Can’t thank you enough, not just on this but all the other info/responses on your site! Amazing!

1 17 18 19 20 21 41