Common Name(s): Bastogne Walnut, Paradox Scientific Name: Juglans x paradox (J. hindsii x J. regia) Distribution: California Tree Size: 50-100 ft (15-30 m) tall, 3-5 ft (1-1.5 m) trunk diameter Average Dried Weight: 46 lbs/ft3 (745 kg/m3) Specific Gravity (Basic, 12% MC): .60, .74 Janka Hardness: 1,250 lbf (5,560 N) Modulus of Rupture: No data available* Elastic Modulus: No data available* Crushing Strength: No data available* Shrinkage: No data available* *Values most likely slightly higher than English Walnut |
Color/Appearance: Heartwood colors can vary from lighter golden yellow to reddish brown, sometimes with darker brown to nearly black streaks. Paler sapwood isn’t always sharly demarcated from the heartwood. Curly or rippled grain is also seen on some sections.
Grain/Texture: Grain is usually straight, but can be irregular. Has a medium texture and moderate natural luster.
Endgrain: Semi-ring-porous; large earlywood pores grading to medium latewood pores, few; solitary and radial multiples of 2-3; tyloses occasionally to abundantly present; growth rings distinct; medium rays barely visible without lens, normal spacing; parenchyma diffuse-in-aggregates (sometimes very faint and barely visible even with lens) and banded (marginal).
Rot Resistance: No data available, but most likely at least moderately durable to very durable, matching the durability of the parent species (J. regia and J. hindsii).
Workability: Typically easy to work provided the grain is straight and regular. Planer tearout can sometimes be a problem when surfacing pieces with irregular or figured grain. Glues, stains, and finishes well, (though walnut is rarely stained).
Odor: Bastogne Walnut has a faint, mild odor when being worked.
Allergies/Toxicity: Other species in the Juglans genus (such as Black or English Walnut) have been reported as sensitizers, and Claro Walnut is likely to generate similar allergic reactions. Usually most common reactions simply include eye and skin irritation. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.
Pricing/Availability: Regular lumber is slightly more expensive than the more common Black Walnut. However, as is the case with most walnuts, pricing for figured Bastogne Walnut is heavily tied to its quality of color and figure, with the highest grades being extremely expensive—easily on par with imported exotic timbers.
Sustainability: This wood species is not listed in the CITES Appendices or on the IUCN Red List of Threatened Species.
Common Uses: Gunstocks, veneer, fine furniture, turned objects, musical instruments (guitars), knife handles, and other small specialty items.
Comments: Plant breeder Luther Burbank experimented with hybrid walnuts beginning in the 1890s, and cross pollinated the native Claro Walnut with English Walnut. The resulting hybrid was quite puzzling: the tree grew grew faster than either of the parent species, and also yielded harder and stronger lumber (though unfortunately it didn’t produce very many walnuts). Because of these anomalies, Burbank named the hybrid “Paradox.” The name Bastogne Walnut appears to be a marketing term, and is not commonly used outside of woodworking circles.
- Black Walnut (Juglans nigra)
- Butternut (Juglans cinerea)
- Claro Walnut (Juglans hindsii)
- English Walnut (Juglans regia)
- Peruvian Walnut (Juglans spp.)
None available.
![]() |
![]() |
![]() |
![]() |
![]() |
![]() |







Paradox walnut is often beautiful. Brown heartwood swirling through the white sap wood in a way that seems surreal. Also, curly like I’ve only ever seen in soft maples. Attached is a small piece I turned recently just as a sample.
How do I mitigate or prevent tearout when planing? I have very figured Bastogne Walnut I’m working with but indeed getting tearout when put through the planer
I’ve got an old piece of wood that needs identifying. It’s very unique. Haven’t seen anything like it. Thanks.
This looks like white oak, which could include several species
Looks like a USA west coast white oak