Common Name(s): Grey alder, speckled alder
Scientific Name: Alnus incana
Distribution: Native to Central Europe; various subspecies are also found in temperate regions of North America and Asia
Average Dried Weight: 29.2 lbs/ft3 (465 kg/m3)
Janka Hardness: 770 lbf (3410 N)*
*Estimated hardness based on specific gravity
Comments: Grey alder is closely related to Alnus glutinosa, another alder species native to Europe. However, grey alder tends to occur as smaller, more multi-stemmed trees that are less suited to commercial harvesting for lumber. However, if clear, defect-free pieces can be obtained, the wood from the two species are very comparable.
Note: This is a truncated profile page. If you have any helpful info or experience with this wood species, feel free to leave a comment below and I’ll do my best to integrate any relevant data when I expand the page. ~Eric
Images: Drag the slider up/down to toggle between raw and finished wood.
Identification: See the article on Hardwood Anatomy for definitions of endgrain features. There are currently no pictures of this exact wood species, but a similar species within the Alnus genus is being substituted European alder (A. glutinosa). If you’d like to contribute a wood sample for this webpage, please see the contact form for donating wood samples.
Related Content:
Wood Info & Stats
Mechanical Properties
You can help support the site by buying one of these resources, designed and published by The Wood Database
The specific links on this site are affiliate links (as an Amazon Associate I earn from qualifying purchases) and help support the site at no extra cost to you.
Donating wood samples and pictures of wood items
If you’ve got a new or unusual wood species that isn’t on the site, please consider sharing it with the rest of us! I’m also interested in getting photos of completed wood projects—especially of obscure or lesser known woods. See my page on donating wood samples for more info.
Support me directly through Patreon
If you’ve been helped by the Wood Database, consider saying “thanks” and helping to support the project. There is of course no obligation, but if you’d like to give back and ensure that the project continues to grow, consider supporting me on Patreon.
Hello, I live in Canada (B.C.). We have two types of alder growing here. I would recommend, adding some of the ecological benefits that alders add to ecosystems.