Swietenia (Mahogany) Genus

> Hardwoods > Meliaceae > Swietenia
Swietenia example (S. mahogani)

Common Name(s): Mahogany, caoba

Distribution: Central and South America, including the Carribean; commercial species also grown on plantations worldwide

Genus Size: Three species and one recognized hybrid

Mechanical Characteristics: Medium density and strength; very similar between species. But properties vary depending on growing conditions; plantation-grown trees tend to produce slightly softer, lighter wood with slightly less dimensional stability.[1]Langbour, P., Gérard, J., Roda, J. M., Fauzi, P. A., & Guibal, D. (2011). Comparison of wood properties of planted big-leaf mahogany (Swietenia macrophylla) in Martinique island with naturally … Continue reading

Visual Characteristics: Mahogany heartwood tends to range from a light golden brown to a deeper reddish brown; quartersawn surfaces can have display a ribbon-stripe figure.

Identification: Wood is diffuse porous, with large pores. Annual growth rings can usually be seen from the marginal parenchyma bands (which is a unique characteristic that helps separate it from the very similar-looking African mahogany of the Khaya genus). 

Mahogany: a Name Synonymous with Quality and Beauty: Despite the many dilutive efforts of naming many unrelated woods “mahogany”—the original mahogany of commerce, the species in the Swietenia genus listed here, have been more or less synonymous with everything you’d want in a quality timber for fine woodworking. (See the related article Mahogany Mixups for a discourse on all the related and unrelated woods that have entered the marketplace as mahogany.) Mahogany sits in a sort of Goldilocks zone as being a wood not too heavy (that it becomes extremely difficult to work) and not too light (that it scratches or dents too easily). On top of that, it has very good dimensional stability with changes in humidity, and can have very visually appealing grain patterns and light-refracting properties (known as chatoyance).

The Sustainability Overhang: With all the positives about mahogany, it’s also worth noting that mahogany is an endangered species. Actually, Swietenia mahogani was arguably the original mahogany of commerce, especially lumber coming out of Cuba (hence the common name used today, Cuban mahogany, even though the tree also has natural distribution throughout the Caribbean.) But due to egregious wastage and overexploitation, that tree is all but unknown to woodworkers today, being replaced by the nearly identical (though larger-leafed) S. macrophylla. Presciently, it was predicted in 1919 “There will come a day not very far distant when the waste of this valuable timber will be regretted.”[2]Neville, H. O. (1919, December). Hardwoods in Cuba. The Cuba Review, 18(1), p15. 

But it’s not all bad news for mahogany, the tree is fast grower and a perfect candidate for plantation growth.

Comments: Swietenia is a genus without a lot of variability between species. In fact, some biologists have even thought that Swietenia could be monotypic (that is, the genus only contains one distinct species).[3]Helgason, T., Russell, S. J., Monro, A. K., & Vogel, J. C. (1996). What is mahogany? The importance of a taxonomic framework for conservation. Botanical Journal of the Linnean Society, 122(1), … Continue reading However, further advancements in DNA and gene testing have reinforced the three species as distinct—though perhaps the morphology of the trees are not as well-differentiated as in other genera.[4]Degen, B., Ward, S. E., Lemes, M. R., Navarro, C., Cavers, S., & Sebbenn, A. M. (2013). Verifying the geographic origin of mahogany (Swietenia macrophylla King) with DNA-fingerprints. Forensic … Continue reading

While woodworkers and lumber dealers tend to use commercial names that focus on the most used port or country for that wood historically (e.g., Honduran mahogany, Cuban mahogany, etc.), botanically the trees are usually named or divided based on leaf size. Perhaps the most well known of the three species, S. macrophylla, is commonly known as big-leaf mahogany—the literal meaning of the latin macro (large) phylla (leaf). Conversely, Cuban mahogany is sometimes referred to as small-leaf mahogany.

 

Related Content:

References

References
1 Langbour, P., Gérard, J., Roda, J. M., Fauzi, P. A., & Guibal, D. (2011). Comparison of wood properties of planted big-leaf mahogany (Swietenia macrophylla) in Martinique island with naturally grown mahogany from Brazil, Mexico and Peru. Journal of Tropical Forest Science, 252-259.
2 Neville, H. O. (1919, December). Hardwoods in Cuba. The Cuba Review, 18(1), p15.
3 Helgason, T., Russell, S. J., Monro, A. K., & Vogel, J. C. (1996). What is mahogany? The importance of a taxonomic framework for conservation. Botanical Journal of the Linnean Society122(1), 47-59.
4 Degen, B., Ward, S. E., Lemes, M. R., Navarro, C., Cavers, S., & Sebbenn, A. M. (2013). Verifying the geographic origin of mahogany (Swietenia macrophylla King) with DNA-fingerprints. Forensic Science International: Genetics7(1), 55-62.
Subscribe