Dalbergia (rosewood) genus

> Hardwoods > Fabaceae > Dalbergia
Example species (Dalbergia oliveri)

Common Name(s): Rosewood

Distribution: Tropical regions worldwide (most commercial species are from Central and South America, Africa, and southern Asia)

Genus Size: Approximately 270 to 300 species

Mechanical Characteristics: Density of commercial species range from medium-high (D. tucurensis) to very high (D. melanoxylon and D. cearensis).

Visual Characteristics: Heartwood tends to be dark reddish brown colored, sometimes with darker contrasting streaks. With sharply demarcated yellowish sapwood.

Identification: Wood is diffuse porous, typically with large to very large and infrequent pores. Parenchyma tends to be rather extensive in many species, commonly diffuse in aggregates, while sometimes forming bands, as well as vasicentric and aliform patterns.

  Species listing

Comments:  As of the beginning of 2017, all species were included on CITES appendix II as endangered species.

Related Content:

Subscribe
Notify of
guest
3 Comments
Inline Feedbacks
View all comments
Eric S

There is also a Dalbergia granadillo (critically endanged, so I assume not something one normally finds). It does not seem to have an entry in wood database, though two other woods, macacauba and cocuswood are listed as sometimes being called granadillo. I wonder is Dalbergia granadillo the reason these other woods are called that, originally as an attempt to pass them off as this no longer available rosewood?

Ava S.

I don’t really know what “granadillo” has to do with spanish, but if it were for something i think it would be for the fruit “granada” and its red colour