Common Name(s): Cashew
Scientific Name: Anacardium occidentale
Distribution: Central and South America
Average Dried Weight: 34.9 lbs/ft3 (560 kg/m3)
Janka Hardness: 770 lbf (3,410 N)*
*Estimated hardness based on specific gravity
Comments: Cashew is much more well known for its edible nuts, and not for its wood. Many parts of the tree, such as the bark, fruit, and the shells of the nuts, contain strong skin irritants—similar in effect to poison ivy (both are in the Anacardiaceae family). The wood is a sensitizer, and has been known to cause skin irritation and blisters in some circumstances.
Note: This is a truncated profile page. If you have any helpful info or experience with this wood species, feel free to leave a comment below and I’ll do my best to integrate any relevant data when I expand the page. ~Eric
Images: Drag the slider up/down to toggle between raw and finished wood.
There are currently no pictures of this exact wood species, but a similar species within the Anacardium genus is being substituted espave (A. excelsum). If you’d like to contribute a wood sample for this webpage, please see the contact form for donating wood samples.
Identification: See the article on Hardwood Anatomy for definitions of endgrain features.
Related Content:
Wood Info & Stats
Mechanical Properties
You can help support the site by buying one of these resources, designed and published by The Wood Database
The specific links on this site are affiliate links (as an Amazon Associate I earn from qualifying purchases) and help support the site at no extra cost to you.
Donating wood samples and pictures of wood items
If you’ve got a new or unusual wood species that isn’t on the site, please consider sharing it with the rest of us! I’m also interested in getting photos of completed wood projects—especially of obscure or lesser known woods. See my page on donating wood samples for more info.
Support me directly through Patreon
If you’ve been helped by the Wood Database, consider saying “thanks” and helping to support the project. There is of course no obligation, but if you’d like to give back and ensure that the project continues to grow, consider supporting me on Patreon.
Cashew is native to Asia, not South and Central America
Do you have any references to support this? Everything I’ve seen says that it’s native to Americas and was later introduced to Asia (and Africa). Even the species name itself “occidentale” means western (e.g., occident vs orient).