Zebrawood

Common Name(s): Zebrawood, Zebrano Scientific Name: Microberlinia brazzavillensis Distribution: West Africa Tree Size: 65-130 ft (20-40 m) tall, 4-5 ft (1.2-1.5 m) trunk diameter Average Dried Weight: 50 lbs/ft3 (805 kg/m3) Specific Gravity (Basic, 12% MC): .67, .81 Janka Hardness: 1,830 lbf (8,160 N) Modulus of Rupture: 17,800 lbf/in2 (122.8 MPa) Elastic Modulus: 2,374,000 lbf/in2 (16.37 GPa) Crushing … Continue reading Zebrawood