Redheart (Erythroxylon mexicanum)
Redheart (Erythroxylum spp.)

View More Images Below

Common Name(s): Redheart, Chakte Kok

Scientific Name: Erythroxylum spp. and Simira spp.

Distribution: Southern Mexico to southern Brazil and Paraguay

Tree Size: 50-65 ft (15-20 m) tall, 1-1.5 ft (.3-.5 m) trunk diameter

Average Dried Weight: 40 lbs/ft3 (640 kg/m3)

Specific Gravity (Basic, 12% MC): .52, .64

Janka Hardness: 1,210 lbf (5,380 N)

Modulus of Rupture: 14,320 lbf/in2 (98.7 MPa)

Elastic Modulus: 1,497,000 lbf/in2 (10.32 GPa)

Crushing Strength: 6,690 lbf/in2 (46.2 MPa)

Shrinkage: Radial: 2.8%, Tangential: 8.2%, Volumetric: 10.6%, T/R Ratio: 2.9

Color/Appearance: Aptly named, in some instances freshly surfaced Redheart can be a very bright, watermelon red—though color can vary in intensity and hue from board to board: anywhere from a light orange/pink, (similar to Pink Ivory), to a darker brownish red. In some cases, it can look quite similar to Bloodwood, though usually with a more visible and figured grain pattern. Redheart’s vibrant color quickly fades to a reddish brown in direct sunlight, though this color change can be slowed (but usually not stopped entirely) by using a finish with UV inhibitors, and keeping the wood away from strong lighting.

Grain/Texture: Grain is usually straight or irregular, with a fine, even texture. Low to medium natural luster.

Endgrain: Diffuse-porous; small to very small pores arranged predominantly in radial multiples of 2-5; growth rings indistinct; rays not visible without lens; parenchyma varies by species: sometimes rare or absent, or vasicentric and weakly aliform (winged).

Rot Resistance: Laboratory tests have shown Redheart to be moderately durable to attack by decay fungi.

Workability: Redheart has good working characteristics, and planes, machines, and sands well. Turns, glues, and finishes well, though a brown color shift is to be expected.

Odor: Redheart can have a distinct, rubber-like smell when being worked depending on species.

Allergies/Toxicity: Besides the standard health risks associated with any type of wood dust, no further health reactions have been associated with Redheart. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Pricing/Availability: Sometimes available as narrow boards, but commonly available as turning squares. Tends to be on the medium to high side for an imported hardwood.

Sustainability: This wood species is not listed in the CITES Appendices or on the IUCN Red List of Threatened Species.

Common Uses: Turned objects, inlays, veneer, fine furniture, and small specialty wood items.

Comments: Commonly called Chakte Kok (with a multitude of variant spellings), this species has been previously placed in the Sickingia genus. Another species that’s also in the Rubiaceæ family is Cosmocalyx spectabilis, which is typically sold interchangeably as Chakte Kok. A third, botanically unrelated wood (Erythroxylaceæ family), which bears an uncanny similarity in nearly every respect to the two other species is Erythroxylum havanense, which is most commonly sold as Redheart.

The scans show examples of what is labeled as Redheart (Erythroxylum spp.), while the mechanical data numbers reference the wood referred to as Chakte Kok (Simira genus).

Related Species:

None available.

Related Articles:

Scans/Pictures:

Redheart (sanded)
Redheart (sanded)

Redheart (sealed)
Redheart (sealed)

Redheart (endgrain)
Redheart (endgrain)

Redheart (endgrain 10x)
Redheart (endgrain 10x)

Redheart, Curly Maple, Sapele (turned)
Redheart, Curly Maple, Sapele (turned)
Subscribe
Notify of
guest
15 Comments
Inline Feedbacks
View all comments
Ed Davidson

I like working Redheart on the lathe…holds details well, easy to sand and finish. Does tend to split and crack if not dried carefully.

Sharon

It was raining in Playa del Carmen…behind the salvage yard When I found this pile of spectacular deep red wood! Now I know it’s name. Canadian, so it was new to me.

Alex Smith

lucky find!!! make a table out of that wood if you took some

Marco

With this wood are also made wristwatches such as this photo, the Italian brand Woodstar Milanocomment image . https://woodstar.itcomment image

Alex Smith

I love the watch

Stacy Graham

I have attached a picture of
some Celtic Lovespoons I carved from Redheart, for my 2 daughters. In
your wood type information brake down, you noted in the ODOR category,

(…a distinct, rubber-like smell when being worked…)

If you think that smell would be unpleasant, you should smell how bad
it is when using a wood burning tool. My wife said the smell lingered
in the house for about 2 days.

Duane Keck

There are 3 species of trees where the wood looks almost the same.

Chakte-kok Simira salvadorensis
Chakte-kok Cosmocalyx spectabilis
Red Heart Erythroxylon havanense

With a hand lens or a good microscope, do you know how to separate these three.

I call these three (3) the “The 3 Red Look-a-Likes”

Duane Keck IWCS # 9086

Curly Pio

I have used Redheart in a project with silver wire inlaid in the wood.
It was easy to work with, no splitting issues even when I used downward force to split the grain for the silver wire.
The color has been the same months after being finish sanded.

Trevor

Well today in wood shop my buddy buddy Alex was drilling a red heart pen blank for me when he brought it back to me the cracked unexpectedly during the drilling process, Eric do you have any advice?
~Trevor

Trevor

I just purchased a Redheart pen blank it is redish-brown in color, will the color change once I turn it, how long will the color stay?

Stacy Graham

I have attached a picture of some Celtic Lovespoons I carved from Redheart, for my 2 daughters. In your wood type information brake down, you noted in the ODOR category,

(…a distinct, rubber-like smell when being worked…)

If you think that smell would be unpleasant, you should smell how bad it is when using a wood burning tool. My wife said the smell lingered in the house for about 2 days.

Duane Keck

There are 3 species of trees where the wood looks almost the same.

Chakte-kok Simira salvadorensis
Chakte-kok Cosmocalyx spectabilis
Red Heart Erythroxylon havanense

With a hand lens or a good microscope, do you know how to separate these three.

I call these three (3) the “The 3 Red Look-a-Likes”

Duane Keck IWCS # 9086