> Hardwoods > Anacardiaceae > Astronium > graveolens DATA SOURCE(S): 1,2,10,14,28,29 Common Name(s): , Scientific Name: Astronium spp. (primarily A. fraxinifolium and A. graveolens) Distribution: From Mexico southward to Brazil Tree Size: 100-130 ft (30-40 m) tall, 3-5 ft (1-1.5 m) trunk diameter Average Dried Weight: lbs/ft3 ( kg/m3) Specific Gravity (Basic, 12% MC): , … Continue reading Goncalo Alves