Box Elder

>¬†Hardwoods > Sapindaceae > Acer > negundo Common Name(s): Box elder, Manitoba maple, ash-leaved maple Scientific Name: Distribution: North America (most commonly in central and eastern United States) Tree Size: 35-80 ft (10-25 m) tall, 1-2 ft (.3-.6 m) trunk diameter Average Dried Weight: 30.2 lbs/ft3 (485 kg/m3) Specific Gravity (Basic, 12% MC): .42, .49 … Continue reading Box Elder