Spalted Maple

Spalted maple (Acer sp.)

Common Name(s): Spalted maple, black line maple

Botanical Designation: Not a distinct species of maple; spalting is a fungal discoloration caused by partially decayed wood.

Distribution: Primarily temperate regions in the Northern Hemisphere

Average Dried Weight: 30.2 to 44.0 lbs/ft3 (485 to 705 kg/m3) depending on species

Janka Hardness: 700 to 1,450 lbf (6,450 N) depending on species

Comments: Spalting is simply a fungal discoloration of wood, and can be found on a wide range of wood species and genera. It is found in wood that has begun initial stages of decay, and is then subsequently dried (preventing further decay). The partial decay, called spalting, can give the wood dark contrasting lines and streaks where fungus has begun to attack the wood. If the wood has been rescued from the spalting at the right time, the lumber should still be sound and usable, with little to no soft spots or rotten wood. 

Maple is a common lumber seen with spalting, as the light colored sapwood provides good contrast for the spalting. Some other temperate species where spalting is commonly seen include sycamore, hackberry, beech, birch, and hickory, as well as tropical species such as tamarind and mango.

Images: Drag the slider up/down to toggle between raw and finished wood. A special thanks to Salem Barker for providing the sculpture photo of this wood species.

 

Watch video of wood finish being applied. (not available)

Spalted maple (sculpture)

Identification: Since spalted maple is not a distinct species, the information below is for red maple (Acer rubrum), though the endgrain images show a sample with ambrosia/fungal staining for reference. See the article on Hardwood Anatomy for definitions of endgrain features.

Ambrosia maple (endgrain 10x)
Ambrosia maple (endgrain 1x)

Porosity: diffuse porous

Arrangement: solitary and radial multiples

Vessels: small to medium; moderately numerous to numerous

Parenchyma: banded (marginal)

Rays: narrow to medium, normal spacing

Lookalikes/Substitutes: Red maple is more or less indistinguishable from other soft maples such as striped maple (Acer pensylvanicum), however, it can usually be separated from hard maple (A. saccharum) according to techniques in this article.

Notes: None.

Related Content:

Subscribe
Notify of
guest
14 Comments
Inline Feedbacks
View all comments
Oleg Plutsis

Very good guitar! Use it musical instrument for 3 years! Sound, of corsrse, not like Gibson, but very goog! (Gibson cost = 2000 $) This Guitar costs 500 $ (now 269 $)! But strings… I have been change it to Elexir Polyveb 10-46. Sorry for my English! I’m from Russia.

Joanne eldred

Can you recommend a few brands of epoxy and tell where you purchased it? I found a spalted maple stump at a local recycling place, had it cut and have made it into a table top. I treated it with wood juice and am letting it dry over the winter. I’d appreciate any suggestions !

Kenny

I have 6/4 spayed maple with 1/64 diameter pin worm holes in face of boards. Are they still worth anything.

Owen O'Neill

Absolutely still worth something. Worm holes aren’t a problem. Just fill them with tabletop epoxy, or something else, and build as normal. They can even be a decorative accent. I recently finished a project using some of my spalted maple and there are regular worm/beetle holes that are 1/8″ or more in diameter.

Erin Ennis

I was lucky enough to have a spalted maple come down in a wind storm in my back yard a few years ago. Since then, I’ve been able to pull a Ukulele (back/sides/top/neck) and Mandolin (back/sides/neck) from the logs we salvaged.

I tried uploading a few pictures, but it seems my login only lets me post text.

Cimmay Rivard

That’s interesting. There’s some acoustic guitars that use spalted Maple for back and sides.

Butcher

Electric, too. Check out this Malinoski Ramrod, which has a spalted maple top:

https://www.petermalinoskiart.com/frames/MAIN_FRAME_2.htm

Cimmay Rivard

Those Malinoski’s are wonderful electrics, never seen before. The acoustic i was looking at that has spalted Maple is the Chinese made Merida DG15SPGACES Grand Auditorium Acoustic Electric Guitar. https://www.americanmusical.com/Item–i-MER-DG15SPGACES-LIST

Curly Pio

The challenge I find is that the longer thewood is allowed to rot before harvesting, the more interesting and beautiful it becomes.
Often the best looking pieces have decayed so far as to need a stabilizer before working.

GrnmtnVT

What would you use/recommend as a stabilizer?

Robert

What I found to work as a stabilizer as good as any other is ordinary wood glue mixed half with water. brush it on the rotten wood, let soak and leave overnight to dry.

Greg

What about using boiled linseed oil as a stabilizer

ORO Woodworks

Linseed oil will not work as a stabilizer — it doesn’t dry solid enough for that sort of purpose. I recently completed four of a set of 8 meditation stools for a custom project and the spalted maple I had was a bit on the soft side in a few places. I used table top epoxy as both stabilizer/void filler, and as the final finish — the good epoxies (as opposed to 5 minute epoxies) get quite runny when they are freshly mixed, so they flow deep into the soft/rotted wood. Judging by the depth of soak when looking at… Read more »

Owen O'Neill

Boiled linseed oil will not make a good stabilizer. It doesn’t dry solid enough. While the wood glue and water will work, it also will potentially cause spots of discoloration when a finish is applied. I recently finished four little meditation stools using pretty heavily spalted maple that had some soft spots of rot. I used table top epoxy to harden those areas and to fill voids left by insects. After soaking the rotted wood, I trimmed the pieces to their final width and was able to check the depth of penetration of the epoxy along the endgrain. The epoxy… Read more »