Common Name(s): Winged Elm, Wahoo

Scientific Name: Ulmus alata

Distribution: Southern and south-central United States

Tree Size: 50-65 ft (15-20 m) tall, 2 ft (.6 m) trunk diameter

Average Dried Weight: 51 lbs/ft3 (815 kg/m3)

Basic Specific Gravity: .60

Hardness: 1,540 lbf (6,850 N)

Rupture Strength: 14,800 lbf/in2 (102,070 kPa)

Elastic Strength: 1,650,000 lbf/in2 (11,380 MPa)

Crushing Strength: 6,780 lbf/in2 (46.8 MPa)

Shrinkage: Radial: 5.3%, Tangential: 11.6%, Volumetric: 17.7%, T/R Ratio: 2.2

Color/Appearance: Heartwood is a light to medium brown, sometimes with a hint of red. Sapwood is a pale white or cream color.

Grain/Pore: Has a medium texture and moderate-sized pores. Grain is sometimes straight, but commonly interlocked.

Durability: Rated as moderately durable to non-durable in regard to heartwood decay, but is susceptible to insect attack, and living trees are very commonly destroyed by Dutch elm disease.

Workability: Can be a challenge to work because of interlocked grain, especially on quartersawn surfaces. Planing can cause tearout and/or fuzzy surfaces. Glues, stains, and finishes well.

Scent: Elm usually has a strong, unpleasant smell when green; though once dried has very little odor.

Safety: Although severe reactions are quite uncommon, Elm in the Ulmus genus has been reported as a sensitizer. Usually most common reactions simply include eye and skin irritation. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Price/Availability: Should be moderately priced, though availability from mature trees has been greatly diminished by Dutch elm disease.

Comments: Elm trees are commonly infected with Dutch elm disease, a fungal disease spread by elm bark beetles. D.E.D. has wiped out millions of Elm trees worldwide.

Common uses for elm include: boxes, baskets, furniture, hockey sticks, veneer, wood pulp, and papermaking.

Related Species:

Scans/Pictures: There are currently no pictures of this exact wood species, but a similar species within the Ulmus genus is being substituted (U. americana). If you’d like to contribute a wood sample of this specific species to be scanned, (even small pieces of veneer can be sent), please use the contact form.


American Elm (Ulmus americana)

American Elm (sanded)



American Elm (sealed)

American Elm (sealed)


Share Your Experience with this Wood Species: