Utile (Entandrophragma utile)

Utile (Entandrophragma utile)

View More Images Below

Common Name(s): Utile, Sipo, Sipo Mahogany

Scientific Name: Entandrophragma utile

Distribution: West and Central Africa

Tree Size: 150-200 ft (45-60 m) tall, 3-5 ft (1-1.5 m) trunk diameter

Average Dried Weight: 41 lbs/ft3 (655 kg/m3)

Basic Specific Gravity: .52

Hardness: 1,260 lbf (5,610 N)

Rupture Strength: 14,350 lbf/in2 (98,970 kPa)

Elastic Strength: 1,585,000 lbf/in2 (10,930 MPa)

Crushing Strength: 8,330 lbf/in2 (57.4 MPa)

Shrinkage: Radial: 4.6%, Tangential: 6.4%, Volumetric: 11.0%, T/R Ratio: 1.4

Color/Appearance: No data available.

Grain/Pore: No data available.

Endgrain: No data available.

Durability: No data available.

Workability: No data available.

Scent: There is no characteristic odor associated with this wood species.

Safety: Although severe reactions are quite uncommon, Utile has been reported to cause skin irritation. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Price/Availability: No data available.

Comments: No data available.

Related Species:

None available.

Scans/Pictures:

Utile (Entandrophragma utile)

Utile (sanded)

Utile (sealed)

Utile (sealed)

Utile (endgrain)

Utile (endgrain)

Utile (endgrain 10x)

Utile (endgrain 10x)

Share Your Experience with this Wood Species: