Common Name(s): Tineo Scientific Name: Weinmannia trichosperma Distribution: South America (mainly Chile and Argentina) Tree Size: 65-100 ft (20-30 m) tall, 2-3 ft (.6-1.0 m) trunk diameter Average Dried Weight: 44 lbs/ft3 (710 kg/m3) Hardness: 1,090 lbf (4,850 N) Rupture Strength: 13,050 lbf/in2 (90,000 kPa) Elastic Strength: No data available Crushing Strength: 6,400 lbf/in2 (44.1 MPa) Shrinkage: Radial: 4.0%, Tangential: 8.0%, Volumetric: 13.0%, T/R Ratio: 2.0 |