The term “Soft Maple” does not refer to any specific species of maple, but rather, it’s a broad term which includes several different species of maple. The term “Soft Maple” is merely used to differentiate these species from Hard Maple.

Hard Maple, on the other hand, typically refers to one specific type of maple species: Acer saccharum. Hard Maple is also known as Rock Maple or Sugar Maple, (this is the same tree which is tapped to get maple syrup).

Depending on where you live, different species might be sold as Soft Maple. For instance, if you live in Oregon, the Soft Maple that you buy (if it has been harvested locally) will likely be Bigleaf Maple, while those living in the eastern United States may actually be buying Red Maple or Silver Maple.

Some of the most common species of maple that fall under the grouping of Soft Maple are:

Each of these maples have their own characteristics regarding strength, hardness, weight, etc., but overall, they are not as hard nor as strong as Hard Maple.

For more information on Hard and Soft Maple, please see the complete article entitled: Differences Between Hard Maple and Soft Maple.

Share Your Experience with this Wood Species: