Common Name(s): Rock Elm, Cork Elm Scientific Name: Ulmus thomasii Distribution: Midwestern United States Tree Size: 65-100 ft (20-30 m) tall, 2-4 ft (.6-1.2 m) trunk diameter Average Dried Weight: 47 lbs/ft3 (750 kg/m3) Hardness: 1,320 lbf (5,870 N) Rupture Strength: 14,800 lbf/in2 (102,070 kPa) Elastic Strength: 1,540,000 lbf/in2 (10,620 MPa) Crushing Strength: 7,050 lbf/in2 (48.6 MPa) Shrinkage: Radial: 4.8%, Tangential: 8.1%, Volumetric: 14.9%, T/R Ratio: 1.7 |
Color/Appearance: Heartwood is a light to medium brown, sometimes with a hint of red. Sapwood is a pale white or cream color.
Grain/Pore: Has a medium texture and moderate-sized pores. Grain is sometimes straight, but commonly interlocked.
Durability: Rated as moderately durable to non-durable in regard to heartwood decay, but is susceptible to insect attack, and living trees are very commonly destroyed by Dutch elm disease.
Workability: Can be a challenge to work because of interlocked grain, especially on quartersawn surfaces. Planing can cause tearout and/or fuzzy surfaces. Glues, stains, and finishes well.
Scent: Elm usually has a strong, unpleasant smell when green; though once dried has very little odor.
Safety: Although severe reactions are quite uncommon, Elm in the Ulmus genus has been reported as a sensitizer. Usually most common reactions simply include eye and skin irritation. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.
Price/Availability: Should be moderately priced, though availability from mature trees has been greatly diminished by Dutch elm disease.
Comments: Elm trees are commonly infected with Dutch elm disease, a fungal disease spread by elm bark beetles. D.E.D. has wiped out millions of Elm trees worldwide.
Common uses for elm include: boxes, baskets, furniture, hockey sticks, veneer, wood pulp, and papermaking.
Scans/Pictures: There are currently no pictures of this exact wood species, but a similar species within the Ulmus genus is being substituted (U. americana). If you’d like to contribute a wood sample of this specific species to be scanned, (even small pieces of veneer can be sent), please use the contact form.