Common Name(s): Quaking Aspen Scientific Name: Populus tremuloides Distribution: Canada and northern United States Tree Size: 65-100 ft (20-30 m) tall, ft (2-3 m) trunk diameter Average Dried Weight: 26 lbs/ft3 (415 kg/m3) Hardness: 350 lbf (1,560 N) Rupture Strength: 8,400 lbf/in2 (57,930 kPa) Elastic Strength: 1,180,000 lbf/in2 (8,140 MPa) Crushing Strength: – lbf/in2 (- MPa) Shrinkage: Radial: 3.5%, Tangential: 6.7%, Volumetric: 11.5%, T/R Ratio: 1.9 |
Color/Appearance: No data available.
Grain/Pore: No data available.
Endgrain: No data available.
Durability: No data available.
Workability: No data available.
Scent: There is no characteristic odor associated with this wood species.
Safety: There have been no adverse health effects associated with Quaking Aspen. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.
Price/Availability: No data available.