Common Name(s): Prosopis juliflora, Mesquite Scientific Name: Prosopis juliflora Distribution: Mexico, Central and South America Tree Size: 50-65 ft (15-20 m) tall, 4 ft (1.2 m) trunk diameter Average Dried Weight: 53 lbs/ft3 (850 kg/m3) Hardness: 2,940 lbf (13,080 N) Rupture Strength: 16,500 lbf/in2 (113,790 kPa) Elastic Strength: 2,060,000 lbf/in2 (14,210 MPa) Crushing Strength: 9,060 lbf/in2 (62.5 MPa) Shrinkage: Radial: 5.1%, Tangential: 8.1%, Volumetric: 13.2%, T/R Ratio: 1.6 |
Color/Appearance: Heartwood tends to be a yellowish brown to dark brown, which darkens with age. Sapwood tends to be narrow and is a pale yellow color.
Grain/Pore: Prosopis juliflora has a medium to coarse texture and a slight natural luster. Grain tends to be straight or wavy.
Endgrain: No data available. Most likely similar to Black Mesquite.
Durability: Prosopis juliflora is considered durable to very durable regarding decay resistance, though it is susceptible to insect attack. Prosopis juliflora has excellent weathering properties.
Workability: Working properties are largely dictated by the quality of the wood itself. Mesquite that is clear and free from defects is easy to work with hand and machine tools, but irregular grain or knots can be challenging. Glues, turns, and finishes well.
Scent: Prosopis juliflora is said to have a fragrant odor while being worked.
Safety: Woods in the Prosopis genus have been reported to cause skin irritation. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.
Price/Availability: Prosopis juliflora is only occasionally available in small sizes, or as large irregular slabs, and is sometimes sold under the generic name of “mesquite.”. Larger boards free from defects are uncommon. Prices for Prosopis juliflora are in the mid range for an imported tropical hardwood.
Comments: Prosopis juliflora is known by a multitude of common names, though not one of them seems to be predominant (or intelligible) in the United States. A very generic term that has been applied to this species is simply “mesquite”—though in the United States, the term usually refers to Honey Mesquite.
Some common uses for Prosopis juliflora include: flooring, firewood, turned objects, cabinetry, and furniture.