<?xml version="1.0" encoding="UTF-8"?><rss version="2.0"
	xmlns:content="http://purl.org/rss/1.0/modules/content/"
	xmlns:dc="http://purl.org/dc/elements/1.1/"
	xmlns:atom="http://www.w3.org/2005/Atom"
	xmlns:sy="http://purl.org/rss/1.0/modules/syndication/"
		>
<channel>
	<title>Comments on: Peruvian Walnut</title>
	<atom:link href="http://www.wood-database.com/lumber-identification/hardwoods/peruvian-walnut/feed/" rel="self" type="application/rss+xml" />
	<link>http://www.wood-database.com/lumber-identification/hardwoods/peruvian-walnut/</link>
	<description>By Woodworkers, For Woodworkers.</description>
	<lastBuildDate>Tue, 07 Feb 2012 16:45:18 +0000</lastBuildDate>
	<sy:updatePeriod>hourly</sy:updatePeriod>
	<sy:updateFrequency>1</sy:updateFrequency>
	<generator>http://wordpress.org/?v=3.1.4</generator>
	<item>
		<title>By: Randy Johnson</title>
		<link>http://www.wood-database.com/lumber-identification/hardwoods/peruvian-walnut/comment-page-1/#comment-789</link>
		<dc:creator>Randy Johnson</dc:creator>
		<pubDate>Wed, 02 Nov 2011 17:57:34 +0000</pubDate>
		<guid isPermaLink="false">http://www.wood-database.com/?p=3242#comment-789</guid>
		<description>I have used this lumber and really enjoy it, but your description does not really address the issue that I have come across, which is the gray-greenish streaking (sometimes filling most of a 4/4 board). This is very costly as you don&#039;t see it unless it is planed. I buy mine rough.

I would gladly send hi-res photos if you would like to use them.

Regards,

Randy</description>
		<content:encoded><![CDATA[<p>I have used this lumber and really enjoy it, but your description does not really address the issue that I have come across, which is the gray-greenish streaking (sometimes filling most of a 4/4 board). This is very costly as you don&#8217;t see it unless it is planed. I buy mine rough.</p>
<p>I would gladly send hi-res photos if you would like to use them.</p>
<p>Regards,</p>
<p>Randy</p>
]]></content:encoded>
	</item>
</channel>
</rss>