Common Name(s): Pericopsis, Nedun

Scientific Name: Pericopsis mooniana

Distribution: Southeast Asia and Oceania

Tree Size: 100-130 ft (30-40 m) tall, 1-2 ft (.3-.7 m) trunk diameter

Average Dried Weight: 48 lbs/ft3 (770 kg/m3)

Basic Specific Gravity: .61

Hardness: 1,460 lbf (6,490 N)

Rupture Strength: 17,640 lbf/in2 (121,660 kPa)

Elastic Strength: 2,166,000 lbf/in2 ( MPa)

Crushing Strength: – lbf/in2 (- MPa)

Shrinkage: Radial: ~4%, Tangential: ~8%, Volumetric: ~11%, T/R Ratio: ~2

Color/Appearance: No data available.

Grain/Pore: No data available.

Durability: No data available.

Workability: No data available.

Scent: There is no characteristic odor associated with this wood species.

Safety: There have been no adverse health effects associated with Pericopsis; however, another wood species in the Pericopsis genus (Afrormosia) has been reported to cause a number of allergic reactions. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Price/Availability: No data available.

Comments: No data available.

Related Species:

Scans/Pictures: There are currently no pictures of this woods species available for viewing. If you’d like to contribute wood samples to be scanned, (even small pieces of veneer can be sent), please use the contact form.


Share Your Experience with this Wood Species: