White Oak (Quercus alba)

Oregon White Oak (Q. alba pictured)

View More Images Below

Common Name(s): Oregon White Oak

Scientific Name: Quercus garryana

Distribution: Pacific Northwestern United States

Tree Size: 65-85 ft (20-25 m) tall, 3-4 ft (1-1.2 m) trunk diameter

Average Dried Weight: 52 lbs/ft3 (825 kg/m3)

Basic Specific Gravity: .64

Hardness: 1,660 lbf (7,380 N)

Rupture Strength: 10,300 lbf/in2 (71,030 kPa)

Elastic Strength: 1,100,000 lbf/in2 (7,590 MPa)

Crushing Strength: No data available

Shrinkage: Radial: 4.2%, Tangential: 9.0%, Volumetric: 13.2%, T/R Ratio: 2.1

Color/Appearance: Has a light to medium brown color, though there can be a fair amount of variation in color. Conversely, Red Oak tends to be slightly redder, but is by no means a reliable method of determining the type of oak.

Grain/Pore: Has medium-to-large pores and a fairly coarse grain.

Durability: Good rot resistance: frequently used in boat-building applications.

Workability: Easy to glue, and takes stain and finishes very well.

Scent: Has a tell-tale smell that is common to most oaks. Most find it appealing.

Safety: Although severe reactions are quite uncommon, oak has been reported as a sensitizer. Usually most common reactions simply include eye and skin irritation. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Price/Availability: Slightly more expensive than Red Oak, White Oak is in good/sustainable supply and is moderately priced. Thicker 8/4 planks, or quartersawn boards are slightly more expensive per board foot.

Comments: White Oak, along with its brother Red Oak, are commonly used domestic lumber species. Hard, durable, and moderately priced, White Oak presents an exceptional value to woodworkers—which explains why it is so widely used in cabinet and furniture making.

Related Species:

Scans/Pictures: There are currently no pictures of this exact wood species, but a similar species within the White Oak grouping is being substituted (Q. alba). If you’d like to contribute a wood sample of this specific species to be scanned, (even small pieces of veneer can be sent), please use the contact form.

White Oak (Quercus alba)

White Oak (sanded)

White Oak (sealed)

White Oak (sealed)

Share Your Experience with this Wood Species: