Common Name(s): Oregon Ash Scientific Name: Fraxinus latifolia Distribution: Western North America Tree Size: 65-80 ft (20-25 m) tall, 1-3 ft (.3-1.0 m) trunk diameter Average Dried Weight: 40 lbs/ft3 (645 kg/m3) Hardness: 1,160 lbf (5,160 N) Rupture Strength: 12,700 lbf/in2 (87,600 kPa) Elastic Strength: 1,360,000 lbf/in2 (9,380 MPa) Crushing Strength: 6,040 lbf/in2 (41.7 MPa) Shrinkage: Radial: 4.1%, Tangential: 8.1%, Volumetric: 13.2%, T/R Ratio: 2.0 |
Color/Appearance: The heartwood is a light brown color, though darker shades can also be seen, which is sometimes sold as Olive Ash.
Grain/Pore: Has a medium to coarse texture similar to oak. The grain is almost always straight and regular, though sometimes curly or figured boards can be found.
Durability: Heartwood is rated as perishable, or only slightly durable in regard to decay. Ash is also not resistant to insect attack.
Workability: Easy to work, and takes glues, stains, and finishes well.
Scent: Gives off a distinct, moderately unpleasant smell when being worked.
Safety: Ash in the Fraxinus genus has been reported to occasionally cause a decrease in lung function. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.
Price/Availability: Ash is among the least expensive utility hardwoods available domestically; it should compare similarly to oak in terms of price.
Comments: Oregon Ash is one of a handful of species in the Fraxinus genus that are used as commercial lumber. It’s not quite as strong or dense as the related White Ash (Fraxinus americana).
Some common uses for ash include flooring, millwork, boxes/crates, baseball bats, and other turned objects such as tool handles.
Scans/Pictures: There are currently no pictures of this exact wood species, but a similar species within the Fraxinus genus is being substituted (F. americana). If you’d like to contribute a wood sample of this specific species to be scanned, (even small pieces of veneer can be sent), please use the contact form.





Share Your Experience with this Wood Species: