Yellow Birch (Betula alleghaniensis)

Gray Birch (B. alleghaniensis pictured)

View More Images Below

Common Name(s): Gray Birch

Scientific Name: Betula populifolia

Distribution: Northeastern North America

Tree Size: 20-40 ft (6-12 m) tall, 1 ft (.3 m) trunk diameter

Average Dried Weight: 37 lbs/ft3 (590 kg/m3)

Basic Specific Gravity: .45

Hardness: 760 lbf (3,380 N)

Rupture Strength: 9,800 lbf/in2 (67,590 kPa)

Elastic Strength: 1,150,000 lbf/in2 (7,930 MPa)

Crushing Strength: 4,870 lbf/in2 33.6- MPa)

Shrinkage: Radial: 5.2%, Tangential: 9.5%, Volumetric: 14.7%, T/R Ratio: 1.8

Color/Appearance: Heartwood tends to be a light reddish brown, with nearly white sapwood. Occasionally figured pieces are available with a wide, shallow curl similar to the curl found in Cherry. There is virtually no color distinction between annual growth rings, giving Birch a somewhat dull, uniform appearance.

Grain/Pore: Grain is generally straight or slightly wavy. Pores are closed, with a fine, even texture

Durability: Birch is perishable, and will readily rot and decay if exposed to the elements. The wood is also susceptible to insect attack.

Workability: Generally easy to work with hand and machine tools, though boards with wild grain can cause grain tearout during machining operations. Turns, glues, and finishes well.

Scent: There is no characteristic odor associated with this wood species.

Safety: Birch in the Betula genus has been reported as a sensitizer. Usually most common reactions simply include skin and respiratory irritation. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Price/Availability: Likely to be rather economical in most instances. Figured boards can be more expensive, but normally plain birch lumber is in the same price range as maple or oak.

Comments: Birch is one of the most widely used woods for veneer and plywood worldwide. Besides regular sheets of plywood, Birch veneer is also used for doors, furniture, and paneling.

Some other common uses for Birch include: boxes, crates, turned objects, interior trim, and other small specialty wood items.

Related Species:

Scans/Pictures: There are currently no pictures of this exact wood species, but a similar species within the Betula genus is being substituted (B. alleghaniensis). If you’d like to contribute a wood sample of this specific species to be scanned, (even small pieces of veneer can be sent), please use the contact form.

Yellow Birch (sanded)

Yellow Birch (sanded)

Yellow Birch (sealed)

Yellow Birch (sealed)

Share Your Experience with this Wood Species: