Common Name(s): European Aspen, Common Aspen

Scientific Name: Populus tremula

Distribution: Temperate regions of Europe and Asia

Tree Size: 50-65 ft (15-20 m) tall, 2-3 ft (.6-1.0 m) trunk diameter

Average Dried Weight: 27 lbs/ft3 (430 kg/m3)

Basic Specific Gravity: .35

Hardness: 370 lbf (1,650 N)*

*Estimated hardness based upon specific gravity.

Rupture Strength: No data available

Elastic Strength: 1,406,000 lbf/in2 (9,700 MPa)

Crushing Strength: – lbf/in2 (- MPa)

Shrinkage: No data available

Color/Appearance: No data available.

Grain/Pore: No data available.

Endgrain: No data available.

Durability: No data available.

Workability: No data available.

Scent: There is no characteristic odor associated with this wood species.

Safety: There have been no adverse health effects associated with European Aspen. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Price/Availability: No data available.

Comments: None.

Related Species:

Scans/Pictures: A special thanks to Steve Earis for providing the wood sample of this wood species.

European Aspen (Populus tremula)

European Aspen (sanded)

European Aspen (sealed)

European Aspen (sealed)

Share Your Experience with this Wood Species: