Common Name(s): Eastern Cottonwood Scientific Name: Populus deltoides Distribution: Central and eastern United States Tree Size: 100-165 ft (30-50 m) tall, 4-6 ft (1.2-2.0 m) trunk diameter Average Dried Weight: 28 lbs/ft3 (450 kg/m3) Hardness: 430 lbf (1,910 N) Rupture Strength: 8,500 lbf/in2 (58,620 kPa) Elastic Strength: 1,370,000 lbf/in2 (9,450 MPa) Crushing Strength: 4,910 lbf/in2 (33.9 MPa) Shrinkage: Radial:3.9 %, Tangential: 9.2%, Volumetric: 13.9%, T/R Ratio: 2.4 |