Anjan (Hardwickia binata)

Anjan (Hardwickia binata)

View More Images Below

Common Name(s): Anjan

Scientific Name: Hardwickia binata

Distribution: India

Tree Size: 50-80 ft (15-25 m) tall, 3-5 ft (1-1.5 m) trunk diameter

Average Dried Weight: 46 lbs/ft3 (745 kg/m3)

Basic Specific Gravity: .61

Hardness: 1,460 lbf (6,490 N)*

*Estimated hardness based upon specific gravity

Rupture Strength: No data available

Elastic Strength: 2,177,000 lbf/in2 (15,010 MPa)

Crushing Strength: 8,170 lbf/in2 (56.4 MPa)

Shrinkage: Radial: 3.0%, Tangential: 4.0%, Volumetric: 8.0%, T/R Ratio: 1.3

Color/Appearance: Heartwood dark reddish brown to nearly black. Sapwood thin, whitish in color.

Grain/Pore: Interlocked grain. Close grain.

Endgrain: No data available.

Durability: Very durable.

Workability: High cutting resistance. Good dimensional stability in regards to flatness, though it can split or check.

Scent: There is no characteristic odor associated with this wood species.

Safety: There have been no adverse health effects associated with Anjan. See the articles Wood Allergies and Toxicity and Wood Dust Safety for more information.

Price/Availability: No data available.

Comments: No data available.

Related Species:

None available.

Scans/Pictures: A special thanks to Steve Earis for providing the wood sample and turned photo of this wood species.

Anjan (Hardwickia binata)

Anjan (sanded)

Indian Anjan (sealed)

Anjan (sealed)

Anjan (endgrain)

Anjan (endgrain)

Indian Anjan (endgrain 10x)

Anjan (endgrain 10x)

Anjan (turned)

Anjan (turned)

Share Your Experience with this Wood Species: