Acacia cambagei

Continue reading about Gidgee

Common Name(s): Sumac, Staghorn Sumac Scientific Name: Rhus spp. (Rhus typhina) Distribution: Northeastern United States Tree Size: 30-40 ft (10-12 m) tall, 1 ft (.3 m) trunk diameter Average Dried Weight: 33 lbs/ft3 (530 kg/m3) Basic Specific Gravity: .45 Hardness: 680 lbf (3,030 N) Rupture Strength: 10,200 lbf/in2 (70,350 kPa) Elastic Strength: 1,190,000 lbf/in2 (8,210 [...]

Continue reading about Sumac

Myroxylon peruiferum

Continue reading about Quina

Acacia acuminata (rumored to not only look like raspberry jam, but also smell like it while being worked?)

Continue reading about Raspberry Jam

Aspidosperma tomentosum

Continue reading about Piquia Amarello

Albizia ferruginea

Continue reading about Tanga Tanga

Lonchocarpus spp.

Continue reading about Machiche

Cercis canadensis

Continue reading about Eastern Redbud

Balfourodendron riedelianum

Continue reading about Guatambu

Loxopterigyum sagotii

Continue reading about Hububuli