Common Name(s): Bulletwood, Massaranduba Scientific Name: Manilkara bidentata Distribution: Carribean, Central and South America Tree Size: 100-150 ft (30-46 m) tall, 2-4 ft (.6-1.2 m) trunk diameter Average Dried Weight: 66 lbs/ft3 (1,060 kg/m3) Basic Specific Gravity: .85 Hardness: 3,190 lbf (14,190 N) Rupture Strength: 29,690 lbf/in2 (204,760 kPa) Elastic Strength: 3,332,000 lbf/in2 (22,980 MPa) [...]

Continue reading about Bulletwood

Aesculus glabra

Continue reading about Ohio Buckeye

Common Name(s): Dogwood, Flowering Dogwood Scientific Name: Cornus florida Distribution: Eastern North America Tree Size: 30-40 ft (9-12 m) tall, 1-1.3 ft (.3-.4 m) trunk diameter Average Dried Weight: 51 lbs/ft3 (820 kg/m3) Basic Specific Gravity: .64 Hardness: 2,150 lbf (9,560 N) Rupture Strength: 14,900 lbf/in2 (102,760 kPa) Elastic Strength: 1,530,000 lbf/in2 (10,550 MPa) Crushing [...]

Continue reading about Dogwood

Tsuga canadensis

Continue reading about Eastern Hemlock

Pinus edulis

Continue reading about Pinyon Pine

Pinus resinosa

Continue reading about Red Pine

Pinus strobus

Continue reading about Eastern White Pine

Pinus monticola

Continue reading about Western White Pine

Cedrelinga catenaeformis

Continue reading about Tornillo

Erythrophleum suaveolens

Continue reading about Tali