Afzelia (doussie) genus

Hardwoods > Fabaceae > Afzelia
Example species (Afzelia sp.)

Common Name(s): Afzelia, doussie, xylay, chanfuta, pod mahogany

Distribution: Tropical regions in Africa and Asia

Genus Size: Approximately 12 species

Mechanical Characteristics: Generally medium-high density and strength characteristics. Most species have very good dimensional stability and, after initial drying, experience little warpage.

Visual Characteristics: Heartwood is golden to reddish brown, superficially resembling mahogany (Swietenia genus). Pieces with burl or highly figured grain are also seen, with the latter sometimes being called xylay pattern.

Identification: Wood is diffuse porous, with few large to very large sized pores. Parenchyma around the large pores tends to be vasicentric, lonzenge, and confluent. Generally narrow rays. Many (but not all) Afzelia species have at least weakly-fluorescing heartwood when viewed under a blacklight.

  Species listing

Comments: A popular hardwood genus that yields commercial species from two different continents. The majority of the species come from Africa, but Asia also utilizes Afzelia species for lumber. However, the IUCN classifies several species in the genera as vulnerable due to exploitation, with the most notable inclusion (listed as endangered) being the Asian species Afzelia xylocarpa.

The Afzelia genus is also very closely related botanically to the Intsia genus (yielding lumber traded as merbau)—with both genera in the tribe Afzelieae. Wood from both genera are similar in anatomy and mechanical characteristics, though merbau tends to be darker in color, and also has occasional yellowish mineral deposits in the pores.